EFFECTS OF N CONTENT ON MICROSTRUCTURE AND PROPERTIES OF 29Cr CASTING SUPER DUPLEX STAINLESS STEEL
XIANG Hongliang; HUANG Weilin; LIU Dong; HE Fushan
School of Mechanical Engineering and Automation; Fuzhou University; Fuzhou 350108
Cite this article: 

XIANG Hongliang HUANG Weilin LIU Dong HE Fushan. EFFECTS OF N CONTENT ON MICROSTRUCTURE AND PROPERTIES OF 29Cr CASTING SUPER DUPLEX STAINLESS STEEL. Acta Metall Sin, 2010, 46(3): 304-310.

Download:  PDF(1124KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  

Microstructures, mechanical properties and corrosion resistances of 29Cr super duplex stainless steel (SDSS) with N contents of 0.11%, 0.26% and 0.42% have been investigated by XRD, SEM, EDS, electrochemical workstation and XPS. The results show that with increasing N content the distribution of Cr becomes homogeneous, the amount of $\gamma$ phase increases according to a linear relationship of Φ(γ)=60×w(N)+21.97, and the tensile strength and elongation of the steel are improved according to the relationships of σb=318.33×(w(N))1/2+626.3 and δ=60×w(N)+10.83, respectively, due to the roles of solution strengthening and reducing (Mn, Cr)S precipitation. In the process of seawater corrosion, α phase in the steel would be corroded first, N can form NH4+ and NO3- to promote the re-passivation effect of passive film; and Mo can form MoO42- to improve the stability of passivated layer and strengthen the corrosion resistance of the steel. The higher the N content, the lower the corrosion current density and the better the corrosion resistance for the steel.

Key words:  29Cr super duplex stainless steel      N content      tensile strength      elongation      polarization curve      passive film     
Received:  23 September 2009     
Fund: 

Supported by Program for Service of Enterprise by Technical Personnel, the Ministry of Science and Technology of China (No.2009GJC40018), Innovation Foundation for Young Talent of Fujian Province (No.2008F3061) and Technological Development Foundation of Fuzhou University (No.2008-XQ-16)

URL: 

https://www.ams.org.cn/EN/10.3724/SP.J.1037.2009.00641     OR     https://www.ams.org.cn/EN/Y2010/V46/I3/304

[1] Campos M, Bautista A, Caceres D, Abenojar J, Torralba J M. J Eur Ceram Soc, 2003; 23: 2813
[2] Tan H, Jiang Y, Deng B, Sun T, Xu J, Li J. Mater Charact, 2009; 60: 1049
[3] Kangas P, Nilsson J O. 2nd Beijing International Duplex Stainless Steel Conference 2006, Beijing: Stainless Steel Council China Special Steel Enterprises Association, 2006: 1
[4] Delong W B. Met Process, 1960; 11: 98
[5] Wu J. Duplex Stainless Steel. Beijing: Metallurgy Industry Press, 1999: 8
(吴玖. 双相不锈钢. 北京: 冶金工业出版社, 1999: 8)
[6] Cui D W, Qu X H, Li K. Mater Rev, 2005; 19: 64
(崔大伟, 曲选辉, 李 科. 材料导报, 2005; 19: 64)
[7] Kamachi U M, Raj B, Translated by Li J, Huang Y H. High Nitrogen Steels and Stainless Steels. Beijing: Chemical Industry Press, 2006: 184
(Kamachi U M, Raj B, 李晶, 黄运华~译. 高N钢和不锈钢. 北京: 化学工业出版社, 2006: 184)

[8] Speidel H J C, Markus O S. Mater Manuf Processes, 2004; 19: 95
[9] Rashev T. High Nitrogen Steels—Metallurgy under Pressure. Sofia: House of the Bulgarian Academy of Sciences, 1995: 253
[10] Ren Y B, Yang K, Zhang B C, Yang H B. J Biomed Eng, 2006; 23: 1101
(任伊宾, 杨柯, 张炳春, 杨慧宾. 生物医学工程学杂志, 2006; 23: 1101)

[11] Young H P, Zin H L. Mater Sci Eng, 2001; A297: 78
[12] Wang S T. PhD Thesis, Technical Institute of Physics and Chemistry, Chinese Academy of Sciences, Beijing, 2008
(王松涛. 中国科学院理化技术研究所博士学位论文, 北京, 2008)

[13] Lothongkum G, Wongpanya P, Morito S, Furuhara T, Maki T. Corros Sci, 2006; 48: 137
[14] Zhang W, Lai Z J, Jin C H, Hong M S. Mater Sci Eng, 2008; A497: 501
[15] Xiao X S, Li J, Jiang L Z, Zhao J L. J Shanghai Univ, 2008; 14: 472
(肖学山, 李 钧, 江来珠, 赵钧良. 上海大学学报, 2008; 14: 472)

[16] Li G Q, Dong T L. China Metall, 2007; 17: 5
(李光强, 董廷亮. 中国冶金, 2007; 17: 5)
[17] Tong J. Master Dissertation, Yanshan University, Qinhuangdao, 2006
(童骏. 燕山大学硕士学位论文, 秦皇岛, 2006)
[18] Fu Y, Lin C J, Cai W D. Acta Metall Sin, 2005; 41: 302
(付 燕, 林昌健, 蔡文达. 金属学报, 2005; 41: 302)
[19] Cvijovic Z, Radenkovic G. Corro Sci, 2006; 48: 3887
[20] Yuan Z Z, Dai Q X, Cheng X N, Zhang C H. J Jiangsu Univ Sci Technol, 2002; 23: 72
(袁志钟, 戴起勋, 程晓农, 张成华. 江苏大学学报, 2002; 23: 72)

[21] Byrnes M L G, Grujicic M, Owen W S. Acta Metall, 1987; 35: 1853
[22] Zhong Q P, Zhao Z H. Fractography. Beijing: High Education Press, 2006: 138
(钟群鹏, 赵子华. 断口学. 北京: 高等教育出版社, 2006: 138)
[23] Brooks C R, Choudhury A, Translated by Xie F J, Sun J X. Failure Analysis of Engineering Materials. Beijing: Machinery Industry Press, 2003: 124
(Brooks C R, Choudhury A, 谢斐娟, 孙家骧~译. 工程材料的失效分析. 北京: 机械工业出版社, 2003: 124)

[24] Huang C S, Shih C C. Mater Sci Eng, 2005; A402: 66
[25] Bastidas J M, Lopez M F, Gutierrez A, Torres C L. Corro Sci, 1998; 40: 431
[26] Lothongkum G, Wongpanya P, Morito S, Furuhara T, Maki T. Corro Sci, 2006; 48: 137 [27] Clayton C R, Halada G P, Kearns J R. Mater Sci Eng, 1995; A198: 135
[28] Montemor M F, Sim?es A M P, Ferreira M G S, Belo M D C. Corro Sci, 1999; 41: 17

[1] ZHENG Liang, ZHANG Qiang, LI Zhou, ZHANG Guoqing. Effects of Oxygen Increasing/Decreasing Processes on Surface Characteristics of Superalloy Powders and Properties of Their Bulk Alloy Counterparts: Powders Storage and Degassing[J]. 金属学报, 2023, 59(9): 1265-1278.
[2] ZHAO Pingping, SONG Yingwei, DONG Kaihui, HAN En-Hou. Synergistic Effect Mechanism of Different Ions on the Electrochemical Corrosion Behavior of TC4 Titanium Alloy[J]. 金属学报, 2023, 59(7): 939-946.
[3] CHENG Yuanyao, ZHAO Gang, XU Deming, MAO Xinping, LI Guangqiang. Effect of Austenitizing Temperature on Microstructures and Mechanical Properties of Si-Mn Hot-Rolled Plate After Quenching and Partitioning Treatment[J]. 金属学报, 2023, 59(3): 413-423.
[4] TANG Yanbing, SHEN Xinwang, LIU Zhihong, QIAO Yanxin, YANG Lanlan, LU Daohua, ZOU Jiasheng, XU Jing. Corrosion Behaviors of Selective Laser Melted Inconel 718 Alloy in NaOH Solution[J]. 金属学报, 2022, 58(3): 324-333.
[5] LV Chenxi, SUN Yangting, CHEN Bin, JIANG Yiming, LI Jin. Influence of Potentionstatic Pulse Technique on Pitting Behavior and Pitting Resistance of 317L Stainless Steel[J]. 金属学报, 2021, 57(12): 1607-1613.
[6] ZHANG Lin, GUO Xiao, GAO Jianwen, DENG Anyuan, WANG Engang. Effect of Electromagnetic Stirring on Microstructure and Mechanical Properties of TiB2 Particle-Reinforced Steel[J]. 金属学报, 2020, 56(9): 1239-1246.
[7] SUN Heng,LIN Xiaoping,ZHOU Bing,ZHAO Shengshi,TANG Qin,DONG Yun. Microstructures and Tensile Deformation Behavior of Directionally Solidified Mg-xGd-0.5Y Alloys[J]. 金属学报, 2020, 56(3): 340-350.
[8] Hanchen FENG,Xuegang MIN,Dasheng WEI,Lichu ZHOU,Shiyun CUI,Feng FANG. Effect of Low Temperature Annealing on Microstructure and Mechanical Properties of Ultra-Heavy Cold-DrawnPearlitic Steel Wires[J]. 金属学报, 2019, 55(5): 585-592.
[9] Kaiqiang LI, Lujia YANG, Yunze XU, Xiaona WANG, Yi HUANG. Influence of SO42- on the Corrosion Behavior of Q235B Steel Bar in Simulated Pore Solution[J]. 金属学报, 2019, 55(4): 457-468.
[10] Ran TAO, Yutao ZHAO, Gang CHEN, Xizhou KAI. Microstructure and Properties of In-Situ ZrB2 np/AA6111 Composites Synthesized Under an Electromagnetic Field[J]. 金属学报, 2019, 55(1): 160-170.
[11] Xiaohua MIN, Li XIANG, Mingjia LI, Kai YAO, Satoshi EMURA, Congqian CHENG, Koichi TSUCHIYA. Effect of {332}<113> Twins Combined with Isothermal ω-Phase on Mechanical Properties in Ti-15Mo Alloy with Different Oxygen Contents[J]. 金属学报, 2018, 54(9): 1262-1272.
[12] Peibei JI, Lichu ZHOU, Xuefeng ZHOU, Feng FANG, Jianqing JIANG. Study on Anisotropic Mechanical Properties of Cold Drawn Pearlitic Steel Wire[J]. 金属学报, 2018, 54(4): 494-500.
[13] Jiang XU, Xike BAO, Shuyun JIANG. In Vitro Corrosion Resistance of Ta2N Nanocrystalline Coating in Simulated Body Fluids[J]. 金属学报, 2018, 54(3): 443-456.
[14] Dahai XIA, Shizhe SONG, Jianqiu WANG, Jingli LUO. Research Progress on Sulfur-Induced Corrosion of Alloys 690 and 800 in High Temperature and High Pressure Water[J]. 金属学报, 2017, 53(12): 1541-1554.
[15] Yonghua RONG,Nailu CHEN. The Principle and Mechanism of Enhancement of Both Strength and Ductility of Martensitic Steels by Carbon[J]. 金属学报, 2017, 53(1): 1-9.
No Suggested Reading articles found!