| INFLUENCES OF ADDITIONS OF Nb, Ti AND Cu ON DAMPING CAPACITY AND CORROSION RESISTANCE OF Fe--13Cr--2.5Mo ALLOY |
| HU Xiaofeng; LI Xiuyan; ZHANG Bo; RONG Lijian; LI Yiyi |
| Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110016 |
|
Cite this article:
HU Xiaofeng LI Xiuyan ZHANG Bo RONG Lijian LI Yiyi. INFLUENCES OF ADDITIONS OF Nb, Ti AND Cu ON DAMPING CAPACITY AND CORROSION RESISTANCE OF Fe--13Cr--2.5Mo ALLOY. Acta Metall Sin, 2009, 45(6): 717-722.
|
|
|
Abstract Fe--Cr base high damping alloys (HDA), as the typical ferromagnetic type HDA, have been well investigated in a long history due to their merits in
low cost and superior workability like steels, and are widely applied for suppression of noise or vibration in many industrial fields. The agnetoelastic
coupling in ferromagnetic materials is well known to be an important source of internal friction, which could produce a high damping capacity. The
damping mechanism has been mainly attributed to the stress--induced irreversible movements of magnetic domain walls. Fe--(12%---16%)Cr--(2%---4%)Mo (mass fraction) base alloys were found to possess higher damping capacity and better corrosion resistance. As well known Nb, Ti and Cu can improve corrosion resistance of stainless steel. In the present work, dynamic mechanical analyzer (DMA) and field--emission scanning electron microscope (FESEM) were used to investigate the influences of additions of 1.0%Nb, 1.0%Ti and 0.5%Cu on the damping capacity and corrosion resistance of Fe--13Cr--2.5Mo alloy. The results show that addition of 1.0%Nb causes abundant precipitations of (Nb, Mo)C, which
can obstruct the movement of domain walls, and significantly deteriorate the damping capacity at low strain amplitude. At strain amplitudes higher than 3.5×10-5, the amplitude--dependent dislocation damping Qdis-1 is generated due to dislocations interaction with (Nb, Mo)C, so the damping
capacity of Nb--containing alloy becomes higher than other alloys. Addition of Ti or Cu inhibits the precipitation of grain--boundary carbides,
while promotes the intragranular precipitations in the alloy distinctly. As a result, the damping capacity of the alloy with Ti or Cu is slightly lower than that of Fe--13Cr--2.5Mo alloy. Pitting corrosion test indicates that the three alloying elements can all improve the corrosion resistance of Fe--13Cr--2.5Mo damping alloy. The 1.0%Ti--containing alloy possesses not only high damping capacity but also good corrosion resistance.
|
|
Received: 04 December 2008
|
|
|
| Fund: Supported by National Natural Science Foundation of China (No.50871110) |
| [1] Golovin I S. J Alloy Compd, 1994; 212: 147
[2] Golovin I S. Metall Mater Trans, 1994; 25A: 111
[3] Ritchie I G, Pan Z L. Metall Trans, 1991; 22A: 607
[4] Igata N, Nishiyama K, Ota K, Yin Y, Wuttig W, Golovin I S, Humbeeck J V, San Juan J. J Alloy Compd, 2003; 355: 230
[5] Azcoitia Ch, Karimi A. J Alloy Compd, 2000; 310: 160
[6] Pulino–Sagradi D, Sagradi M, Karimi A, Martin J L. Scr Mater, 1998; 39: 131
[7] Karimi A, Giauque P H, Martin J L. J Appl Phys, 1996; 79: 1670
[8] Chen S Y, Zhang T K, Kang X F, Yang C Q, Wang X. Stainless Steel. Beijing: Atomic Energy Press, 1995: 77
(陈世英, 张廷凯, 康喜范, 杨长强, 王 熙. 不锈钢. 北京: 原子能出版社, 1995: 77)
[9] Wang W G, Zhou B X. Mater Sci Eng, 2004; A366: 45
[10] Wang W G, Zhou B X, Zheng Z M. Acta Metall Sin, 1998; 34 : 1039
(王卫国, 周邦新, 郑忠民. 金属学报, 1998; 34: 1039)
[11] Lin R R, Cao M Z, Yang R. Mater Sci Forum, 2005; 475–479: 261
[12] Lin R R, Liu F, Cao M Z, Yang R. Acta Metall Sin, 2005; 41: 958
(林仁荣, 刘 芳, 曹名洲, 杨 锐. 金属学报, 2005; 41: 958)
[13] Aksoy M, Yilmaz O, Korkut M H. Wear, 2001; 249: 639
[14] Kuzucu V, Aksoy M, Korkut M H. J Mater Process Technol, 1998; 82: 165
[15] Cao J C, Yong Q L, Liu Q Y, Sun X J. Trans Mater Heat Treat, 2006; 27(5): 51
(曹建春, 雍岐龙, 刘清友, 孙新军. 材料热处理学报, 2006; 27(5): 51)
[16] Misra R D K, Weatherly G C, Hartmann J E, Boucek A J. Mater Sci Technol, 2001; 17: 1119
[17] Cao J C, Yong Q L, Liu Q Y, Sun X J. J Mater Sci, 2007; 42: 10080
[18] Hong I T, Koo C H. Mater Sci Eng, 2005; A393: 213
[19] Smith G W, Birchak J R. J Appl Phys, 1968; 39: 2311
[20] Smith G W, Birchak J R. J Appl Phys, 1969; 40: 5174
[21] Zhou Z C, Wei J N, Han F S. Phys Status Solidi, 2002; 191A: 89
[22] Coronel V F, Beshers D N. J Appl Phys, 1988; 64: 2006
[23] Nowick A S, Berry B S. Anelastic Relaxation in Crystalline Solids. New York: Academic Press, 1972: 411
[24] Feng D. Metal Physics (Vol.III)—Metallic Mechanical Properties. Beijing: Science Press, 1999: 157
(冯 端. 金属物理学(第3卷)------金属力学性质. 北京: 科学出版社, 1999: 157) |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|