| LOW CYCLE FATIGUE BEHAVIORS AND MICROSTRUCTURES OF Ti–2Al–2.5Zr WITH FINE GRAIN AT RT AND 77 K |
| WANG Hang; XU Yanling; SUN Qiaoyan; XIAO Lin; SUN Jun |
| State Key Laboratory for Mechanical Behavior of Materials; Xi’an Jiaotong University; Xi’an 710049 |
|
Cite this article:
WANG Hang XU Yanling SUN Qiaoyan XIAO Lin SUN Jun. LOW CYCLE FATIGUE BEHAVIORS AND MICROSTRUCTURES OF Ti–2Al–2.5Zr WITH FINE GRAIN AT RT AND 77 K. Acta Metall Sin, 2009, 45(4): 434-441.
|
|
|
Abstract Ti–2Al–2.5Zr alloy with hcp structure is a kind of structural materials used under low temperature condition, e.g. pipeline system of liquid hydrogen and liquid oxygen in missile engine. It is usually serviced in condition of severe low temperature and dynamic loading. Deformation twinning is a common and important plastic deformation mode in the hexagonal close–packed alloy, but will be severely restricted as the grain is refined from tens of microns to a few microns. On the other hand, twinning has a low sensitivity to temperature, consequently becomes a favorable deformation mode at low temperature in comparison with dislocation slip. The objective of this work is to study the coupling effect of grain refinement and testing temperature on twinning behavior and the low–cycle fatigue behavior of Ti–2Al–2.5Zr. Symmetrical push–pull low–cycle fatigue (LCF) tests were performed on Ti–2Al–2.5Zr with grain size of about 5 μm at room temperature (RT) and low temperature (77 K). The results show that the alloy exhibits the higher ductility and the longer low–cycle fatigue life at 77 K than those at RT. The cyclic stress response curves show that the cyclic softening occurs at the low strain amplitudes of 0.5% and 1.0%. However, as strain amplitude increased to 1.5% and 2.0%, cyclic stress saturation appeared. When testing temperature declined to 77 K, the cyclic hardening was observed at all four strain amplitudes. The degree of cyclic ardening increases as the strain amplitude rises. The fractography analyses suggest that transgranular fracture with well–developed fatigue striations is the predominant failure mode. The amount of secondary cracks is much higher in the alloys deformed at RT than that at 77 K. TEM examination reveals that deformation twins become more active. The primary types of twinning are {1011} and {1121}. The typical deformation microstructures consist of individual dislocation lines together with the tangled dislocation at the low strain amplitudes of 0.5% and 1.0%. As the strain amplitude increased to 1.5% and 2.0%, {1010}prismatic slip and {1121} pyramidal slip were simultaneously activated, the subgrain and dislocation cells were formed. At 77 K and strain amplitude of 2.0%, the parallel dislocation bands distribute along prismatic plane. As the strain amplitude increased to 0.5%, utual perpendicular dislocation lines appeared. The improvement of fatigue life of Ti–2Al–2.5Zr at 77 K is attributed to the constraint of inhomogeneous slip and the activation of deformation twinning.
|
|
Received: 10 October 2008
|
|
|
| Fund: Supported by National Basic Research Program of China (Nos.2007CB386104 and 2004CB619303) and National Natural Science Foundation of China ( Nos.50671077 and 50771080) |
| [1] Yu Z T, Zhou L, Deng J, Gu H C. Rare Met Mater Eng, 1999; 28: 340
(于振涛, 周 廉, 邓 炬, 顾海澄. 稀有金属材料与工程, 1999; 28: 340)
[2] Yu Z T. Nonferrous Smelting, 2002; 31(6): 182
(于振涛. 有色冶炼, 2006; 31(6): 182)
[3] Yu Z T, Zhou L, Deng J, Gu H C. Rare Met Mater Eng, 2000; 29: 86
(于振涛, 周 廉, 邓炬, 顾海澄. 稀有金属材料与工程, 2000; 29: 86)
[4] Venables J A. In: Reed–Hill R E, Hirth J P, Rogers H C, eds. Deformation Twinning. New York: Gordon and Breach, 1964: 7
[5] Meyers M A, V¯ohringer O, Lubarda V A. Acta Mater, 2001; 49: 4025
[6] Harding J. Proc R Soc London, 1967; 299A: 464
[7] Bolling G F, Richman R H. Acta Metall, 1965; 13: 709
[8] Chen M, Ma E, Hemker K J, Sheng H W, Wang Y M, Cheng X M. Science, 2003; 300: 1275
[9] Huang C X, Wang K, Wu S D, Zhang Z F, Li G Y, Li S X. Acta Mater, 2006; 54: 655
[10] Wu X L, Ma E. Appl Phys Lett, 2006; 88: 195
[11] Ueji R, Tsuchida N, Terada D, Tsuji N, Tanaka Y, Takemura A, Kunishige K. Scr Mater, 2008; 59: 963
[12] Meyers M A, Andrade U R, Chokshi A H. Metall Mater Trans, 1995; 26A: 2881
[13] Levine E D. Trans Met Soc AIME, 1996; 236: 1558
[14] Song S G, GrayIII G T. Acta Metall Mater, 1995; 43: 2325
[15] Christan J W, Mahajan S. Prog Mater Sci, 1995; 39: 84
[16] Tsuji N, Ito Y, Saito Y, Minamino Y. Scr Mater, 2002; 47: 893
[17] Hirth J P, Lothe J. Theory of Dislocations. 2nd ed, Malabar, UK: Krieger Publishing, 1992: 650
[18] Laird C, Stanzl S, de La Veaux R, Buchinger L. Mater Sci Eng, 1986; 80: 143
[19] Xiao L, Kuang Z B. Acta Mater, 1996; 44: 3059
[20] Bacon D J, Martin J W. Philos Mag, 1981; 43: 883
[21] Lagerlf K P D, Castaing J, Pirouz P, Heuer A H. Philos Mag, 2002; 82: 2841
[22] Xiao L, Umakoshi Y, Sun J. Metall Mater Trans, 2001; 32A: 2841
[23] Nilsson J O. Scr Metall, 1983; 17: 593
[24] Li X W, Wu X M, Wang Z G, Umakoshi Y. Metall Mater Trans, 2003; 34A: 307
[25] Starke E A, Lutjering G Jr. Fatigue and Microstructure, Metals Park, OH: ASM, 1978: 14
[26] Jouiad M, Clement N, Coujou A. Philos Mag, 1998; 77A:689
[27] Heino S, Karlsson B. Acta Mater, 2001; 49: 353
[28] Steffens Th, Schwink Ch, Korner A, Karnthaler H P. Philos Mag, 1987; 56: 161
[29] Partridge P G. Metall Rev, 1967; 118: 175
[30] Christian J W, Mahajan S. Prog Mater Sci, 1995; 39: 1
[31] Yoo M H, Wei C T. Philos Mag, 1966; 14: 573
[32] Tomsett D I, Bevis A. Philos Mag, 1969; 19: 533
[33] Yoo M H. Metall Trans, 1981; A12: 409
[34] Ehab E D, Surya R K, Roger D D. Metall Mater Trans, 1999; 30A: 1223
[35] Ayman A S, Surya R K, Roger D D. Scr Mater, 2002; 46: 419
[36] Ayman A S, Surya R K, Roger D D. Acta Mater, 2003; 51: 4225
[37] Mullins S, Mpatchett B. Metall Trans, 1981; 12A: 74
[38] Akhtar A. Metall Trans, 1975; 6A: 1105
[39] Beevers C J, Halliday M D. J Met Sci, 1969; 3: 74
[40] Byrne J G. Deformation Twinning. Gainsville: AIME Conf, 1963: 397 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|