| [1] Miettinen J. Calphad, 1998; 22: 231
[2] Zhu H T. Report of Postdoctoral Research, Shanghai JiaoTong University, 2002
(朱洪涛. 上海交通大学博士后报告. 2002)
[3] Chou K C, Chang Y A. Ber Bunsen–Ges Phys Chem, 1989; 93: 741
[4] Bichara C, Bergman C, Mathieu J C. Acta Metall, 1985; 33: 91
[5] Hashiguchi K, Kirkaldy J S, Fukuzumi P, Pavaskar V. Calphad, 1984; 8: 173
[6] Chang H B, Hsu T Y (Xu Z Y). Acta Metall, 1986; 34: 333
[7] Qu J B, Liu Z Y, Liu X H,Wang G D. Mater Sci Technol, 1998; 14: 380.
[8] Bhadeshia H K. Met Sci, 1981; 15: 178
[9] Zhang B, Zhang H B, Ruan X Y. J Shanghai JiaoTong Univ, 2003; 37: 10
(张斌, 张鸿冰, 阮雪榆. 上海交通大学学报, 2003; 37: 10)
[10] Liu Z Y, Xu Y B, Wang G D. Simulation and Prediction of the Evolution of Microstructure and Properties of Hot Rolled Steels. Shenyang: Northeastem University, 2004: 34
(刘振宇, 许云波, 王国栋. 热轧钢材组织-性能演变的模拟和预测. 沈阳: 东北大学出版社, 2004: 34)
[11] Aaronson H I, Domain H A, Pound G M. Trans Metall Soc AIME, 1966; 236: 768
[12] Zener C. Trans AIME, 1955; 203: 619
[13] Kaufman L, Clougherty E X,Weiss R J. Acta Metall, 1963; 11: 323
[14] Orr R L, Chipman J. Trans Metall Soc AIME, 1967; 239: 630
[15] Mogumov B M, Tomilin I A, ShvarsmanL A. Thermodynamics of Fe–C Alloys. Moscow: Metallurgy Press, 1972: 110
[16] Hsu T Y (Xu Z Y), Zhang H B, Luo S F. Acta Metall Sin, 1984; 32: 343
(徐祖耀, 张鸿冰, 罗守福. 金属学报, 1984; 32: 343)
[17] Hsu T Y. Materials Thermodynamics. Beijing: Science Press, 2005: 204
(徐祖耀. 材料热力学. 北京: 科学出版社, 2005: 204)
[18] Mou Y W, Hsu T Y(Xu Z Y). Acta Metall, 1986; 34: 325
[19] Mou Y W, Hsu T Y(Xu Z Y). Acta Metall Sin, 1987; 23: 329
(牟翊文, 徐祖耀. 金属学报. 1987; 23: 329 )
[20] Hsu T Y. Martensite Transformation and Martensite. Beijing: Science Press, 1980: 53
(徐祖耀. 马氏体和马氏体相变. 北京: 科学出版社, 1980: 53)
[21] Wray P J. Metall Trans, 1982; 13A: 125
[22] Dai Q X, Cheng X N, Yang Z Z. Mater Charact, 2004; 52: 349
[23] Byun T S. Acta Mater, 2003; 51: 3063
[24] Cheng X N, Dai Q X. Design and Control for Austenitic Steels. Beijing: Defense Industry Press, 2005: 37
(程晓农, 戴起勋. 奥氏体钢设计与控制. 北京: 国防工业出版社, 2005: 37)
[25] Xie J P, Li Q C, He Z M, Chen Q D. J Luoyang Inst Technol, 1997; 18(2): 6
(谢敬佩, 李庆春, 何镇明, 陈全德. 洛阳工学院学报, 1997; 18(2): 6)
[26] Central Iron and Steel Research Institute of Ministry of Metallurgical Industry. The Atlas of Super–Cooling Austenite Transformation Diagrams. Beijing: Metallurgical
Industry Press, 1979: 1
(冶金工业部钢铁研究总院. 钢的过冷奥氏体转变曲线图集. 北京: 冶金工业出版社, 1979: 1)
[27] Li M Y, Sun B R. Steel Technical Manual on Rolling Control and Control of Cooling. Beijing: Metallurgical Industry Press, 1989: 124
(李曼云, 孙本荣. 钢的控制轧制和控制冷却技术手册. 北京: 冶金工业出版社, 1989: 124)
[28] The No.1 Iron Factory, Benxi Iron and Steel Corporation, Tsinghua University. The Atlas of Super–Cooling Austenite Transformation Diagrams. Benxi: The No.1 Iron Factory Press, Benxi Iron and Steel Corporation, 1978: 1
(本溪钢铁公司第一炼钢厂, 清华大学机械系金属材料教研组. 钢的过冷奥氏体转变曲线. 本溪: 本溪钢铁公司
第一炼钢厂, 1978: 1)
[29] Zhang S Z. Atlas of Super–Cooling Austenite Transformation Diagrams. Beijing: Metallurgical Industry Press, 1993: 22
(张世中. 钢的过冷奥氏体转变曲线图集. 北京: 冶金工业出版社, 1993: 22)
[30] Harbin Research Institute of Welding of Ministry of Machine Building and Electronics Industry. CCT Atlas of Welding of Low Alloy Steels. Beijing: China Machine Press, 1990: 3
(机械电子工业部哈尔滨焊接研究所. 国产低合金钢焊接CCT图册. 北京: 机械工业出版社, 1990: 3)
[31] Japan Society for Irons & Steels. Atlas of Continuous Cooling Transformation Diagrams of Low Carbon Steels. Tokyo: Japan Society for Irons and Steels Press, 1992: 32
(日本钢铁学会. 低碳钢连续冷却转变图集. 东京: 日本钢铁学会出版社, 1992: 32)
[32] American Society for Metals. Atlas of Isothermal Transformation and Cooling Transformation Diagrams. Metals Park, Ohio: American Society for Metals Press, 1977: 1
[33] Breedies J F. Trans Metall Soc AIME, 1964; 230: 1583
[34] Aaronson H I, Domain H A. Trans Metall Soc AIME, 1966, 236: 781
[35] Walters F M, Wells C. Trans Metall Soc AIME, 1936; 24: 359
[36] Hansen M. Constitution of Binary Alloys. New York: McGraw–Hill, 1958: 960
[37] Kriz A, Poboril F. Int Iron Steel Inst, 1932; 126: 323
[38] You W, Bai B Z, Fang H S, Xie X S. Acta Metall Sin, 2004; 40: 1133
(由伟, 白秉哲, 方鸿生, 谢锡善. 金属学报, 2004; 40: 1133) |