MODELING AND SIMULATION OF MICROSTRUCTURE EVOLUTION OF CAST MAGNESIUM ALLOYS USING CA METHOD BASED ON TWO SETS OF MESH
HUO Liang; HAN Zhiqiang; LIU Baicheng
Key Laboratory for Advanced Materials Processing Technology; Ministry of Education; Department of Mechanical Engineering; Tsinghua University; Beijing 100084
Cite this article: 

HUO Liang HAN Zhiqiang LIU Baicheng. MODELING AND SIMULATION OF MICROSTRUCTURE EVOLUTION OF CAST MAGNESIUM ALLOYS USING CA METHOD BASED ON TWO SETS OF MESH. Acta Metall Sin, 2009, 45(12): 1414-1420.

Download:  PDF(2848KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  

The texture of Mg alloy dendrites is quite different from that of fcc or bcc metals because of the influence of hcp crystal lattice on the dendrite morphology evolutions during solidification. Although the simulations of dendrite morphologies for fcc or bcc metals by cellular automaton (CA) methods have been widely reported, CA simulations of magnesium alloys with hcp crystal lattice have just appeared in recent years. When performing the simulation of Mg alloy dendrites with a CA method on a square mesh, the artificial anisotropy of growth kinetics introduced by the square mesh makes it hard to reflect the texture of Mg alloy dendrites, which shows the six–fold symmetry instead of four–fold symmetry of bcc or fcc metal dendrites.

In the present paper, a two dimensional CA model has been developed for simulating the dendrite morphology evolution of castMg alloys. The model employs two sets of meshes to perform the numerical simulation, where a hexagonal mesh is used to perform CA calculation to reflect the texture of Mg alloy dendrites, and an orthogonal mesh is used to solve the mass transportation equation. The two sets of meshes are coupled by an interpolation method. By employing the two–set mesh method, the texture of Mg alloy dendrites is well reflected and the undesired artificial growth kinetics introduced by square mesh is avoided. In the model, the growth kinetics of dendrite tips was determined by the difference between local equilibrium and local actual compositions obtained by solving the solute transport equation. With this calculation method for growth kinetics, the solid fraction of interface CA cell can be obtained directly from the solute field, which decreases the computational cost greatly. The model was applied to simulate the single dendrite evolution and columnar dendrite growth of AZ91D Mg alloy, as well as multi–dendrite growth and grain size of Mg–10Gd–2Y–0.5Zr (mass fraction, %) alloy step–shaped castings. To validate the current model, permanent mold sample castings of AZ91D Mg alloy and step–shaped castings of Mg–10Gd–2Y–0.5Zr alloy were produced. Optical metallographic examinations were performed on specimens of these two Mg alloys, and grain sizes were measured on solution treated specimens of Mg–10Gd–2Y–0.5Zr alloy. The simulated and experimental results were compared.

Key words:  magnesium alloy      dendrite morphology      numerical simulation      cellular automaton method      hexagonal mesh     
Received:  06 May 2009     
ZTFLH: 

111.4

 
Fund: 

Supported by National Basic Research Program of China (Nos.2005CB724105 and 2006CB605208) and National Natural Science Foundation of China (No.50875143)

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2009/V45/I12/1414

[1] Mordike B L, Eert T. Mater Sci Eng, 2001; A302: 37
[2] Gandin C A, Rappaz M. Acta Mater, 1994; 42: 2233
[3] Zhu M F, Hong C P. ISIJ Int, 2001; 41: 436
[4] Wang W, Lee P D, Mclean M. Acta Mater, 2003; 51: 2971
[5] Dahle A K, Lee Y C, Nave M D, Schaffer P L, StJohn D H. J Light Met, 2001; 1: 61
[6] Bottger B, Eiken J, Ohno M, Klaus G, Fehlbier M, Schmid–Fetzer R, Steinbach I, B¨uhrig–Polaczek A. Adv Eng Mater, 2006; 8: 241
[7] Beltran–Sanchez L, Stefanescu D M. Metall Mater Trans, 2003; 34A: 367
[8] Shan B W. PhD thesis, Northwestern Polytechnical University, xi’an, 2009
(单博炜. 西北工业大学博士论文, 西安, 2009)
[9] Dong H B, Lee P D. Acta Mater, 2005; 53: 659
[10] Nastac L. Acta Mater, 1999; 47: 4253
[11] Huo L, Han Z Q, Liu Z Y, Liu B C. Mater Sci Forum,2007; 561–565: 1797
[12] Fu Z N, Xu Q Y, Xiong S M. Chin J Nonferrous Met,2007; 17: 1567
(付振南, 许庆彦, 熊守美. 中国有色金属学报, 2007; 17: 1567)
[13] Zhu M F, Stefanescu D M. Acta Mater, 2007; 55: 1741
[14] Stefanescu D M. Science and Engineering of Casting Solidification. London: Kluwer Academic/Plenum Publishers,2002: 149
[15] Sasikumar R, Sreenivasan R. Acta Metall Mater, 1994; 42:2381
[16] Beltran–Sanchez L, Stefanescu D M. Int J Cast Met Res, 2002; 15: 251
[17] Th´evoz P, Desbiolles J L, Rappaz M. Metall Trans, 1989; 20A: 311
[18] Liu Z Y. PhD thesis, Tsinghua University, Beijing, 2006
(刘志勇. 清华大学博士学位论文, 北京, 2006)
[19] Guo Y C, Li J P, Li J S, Yang Z, Zhao J, Xia F, Liang M X. J Alloys Compd, 2008; 450: 446
[20] Huo L, Han Z Q, Liu B C. The 2nd Int Conf on Advances in Solidification Processes. Leoben, Austria, 2008 (in press)

[1] BI Zhongnan, QIN Hailong, LIU Pei, SHI Songyi, XIE Jinli, ZHANG Ji. Research Progress Regarding Quantitative Characterization and Control Technology of Residual Stress in Superalloy Forgings[J]. 金属学报, 2023, 59(9): 1144-1158.
[2] SHAO Xiaohong, PENG Zhenzhen, JIN Qianqian, MA Xiuliang. Unravelling the {101¯2} Twin Intersection Between LPSO Structure/SFs in Magnesium Alloy[J]. 金属学报, 2023, 59(4): 556-566.
[3] ZHU Yunpeng, QIN Jiayu, WANG Jinhui, MA Hongbin, JIN Peipeng, LI Peijie. Microstructure and Properties of AZ61 Ultra-Fine Grained Magnesium Alloy Prepared by Mechanical Milling and Powder Metallurgy Processing[J]. 金属学报, 2023, 59(2): 257-266.
[4] TANG Weineng, MO Ning, HOU Juan. Research Progress of Additively Manufactured Magnesium Alloys: A Review[J]. 金属学报, 2023, 59(2): 205-225.
[5] ZHANG Kaiyuan, DONG Wenchao, ZHAO Dong, LI Shijian, LU Shanping. Effect of Solid-State Phase Transformation on Stress and Distortion for Fe-Co-Ni Ultra-High Strength Steel Components During Welding and Vacuum Gas Quenching Processes[J]. 金属学报, 2023, 59(12): 1633-1643.
[6] WANG Chongyang, HAN Shiwei, XIE Feng, HU Long, DENG Dean. Influence of Solid-State Phase Transformation and Softening Effect on Welding Residual Stress of Ultra-High Strength Steel[J]. 金属学报, 2023, 59(12): 1613-1623.
[7] XIA Dahai, DENG Chengman, CHEN Ziguang, LI Tianshu, HU Wenbin. Modeling Localized Corrosion Propagation of Metallic Materials by Peridynamics: Progresses and Challenges[J]. 金属学报, 2022, 58(9): 1093-1107.
[8] CHEN Yang, MAO Pingli, LIU Zheng, WANG Zhi, CAO Gengsheng. Detwinning Behaviors and Dynamic Mechanical Properties of Precompressed AZ31 Magnesium Alloy Subjected to High Strain Rates Impact[J]. 金属学报, 2022, 58(5): 660-672.
[9] ZENG Xiaoqin, WANG Jie, YING Tao, DING Wenjiang. Recent Progress on Thermal Conductivity of Magnesium and Its Alloys[J]. 金属学报, 2022, 58(4): 400-411.
[10] LI Shaojie, JIN Jianfeng, SONG Yuhao, WANG Mingtao, TANG Shuai, ZONG Yaping, QIN Gaowu. Multimodal Microstructure of Mg-Gd-Y Alloy Through an Integrated Simulation of “Process-Structure-Property”[J]. 金属学报, 2022, 58(1): 114-128.
[11] HU Long, WANG Yifeng, LI Suo, ZHANG Chaohua, DENG Dean. Study on Computational Prediction About Microstructure and Hardness of Q345 Steel Welded Joint Based on SH-CCT Diagram[J]. 金属学报, 2021, 57(8): 1073-1086.
[12] LI Zihan, XIN Jianwen, XIAO Xiao, WANG Huan, HUA Xueming, WU Dongsheng. The Arc Physical Characteristics and Molten Pool Dynamic Behaviors in Conduction Plasma Arc Welding[J]. 金属学报, 2021, 57(5): 693-702.
[13] WANG Huiyuan, XIA Nan, BU Ruyu, WANG Cheng, ZHA Min, YANG Zhizheng. Current Research and Future Prospect on Low-Alloyed High-Performance Wrought Magnesium Alloys[J]. 金属学报, 2021, 57(11): 1429-1437.
[14] PAN Fusheng, JIANG Bin. Development and Application of Plastic Processing Technologies of Magnesium Alloys[J]. 金属学报, 2021, 57(11): 1362-1379.
[15] WANG Xuemei, YIN Zhengzheng, YU Xiaotong, ZOU Yuhong, ZENG Rongchang. Comparison of Corrosion Resistance of Phenylalanine, Methionine, and Asparagine-Induced Ca-P Coatings on AZ31 Magnesium Alloys[J]. 金属学报, 2021, 57(10): 1258-1271.
No Suggested Reading articles found!