Chun-guang Kuai; Zhifang Peng. ELEMENTAL PARTITIONING CHARACTERISTICS AND STABILITY OF EQUILIBRIUM PHASES DURING 450-1200℃ IN T/P91 HEAT-RESISTANT STEEL. Acta Metall Sin, 2008, 44(8): 897-900 .
|
|
|
Abstract Chemical compositions and amounts of equilibrium phases in T/P91 heat resistant steel in the temperature range of 450℃ ~ 1200℃ have been calculated by using thermodynamic software ‘Thermo-Calc’. Concept of elemental partitioning fraction is introduced to study the elemental partitioning characteristics of such main alloying elements as Cr, Mo, Fe, V, Nb, C and N, the stability, the constituents and the evolutional rule of the equilibrium phases at elevated temperatures. The results show that using the elemental partitioning characteristics with the change of temperatures the stability of the equilibrium phases can be easily revealed, and the sub-types of MX and the formation of M and X in MX, and the elemental evolution rule in MX type phases can be reasonably determined, and as well as the effect of carbon content in the matrix phase on the formation of MX phases can be helpfully understood, respectively.
|
|
Received: 10 October 2007
|
|
|
[1]Race J M,Bhadeshia H K D H.Mater Sci Technol,1992; 8:875 [2]Furtado H C,de Almeida L H,Le M I.Mater Charact, 2007;58:72 [3]Kropa A,V■rostkováA,Svoboda M,Janovec J.Acta Mater,1998;46:39 [4]Taneike M,Sawada K,Abe F.Metall Mater Trans,2004; 35A:1255 [5]Yamada K,Igarashi M,Muneki S,Abe F.ISIJ Int,2002; 42:779 [6]Sawada K,Ohba T,Kushima H,Kimura K.Mater Sci Eng,2005;A394:36 [7]Marinkovic B A,de Avillez R R.Mater Res,2002;5:491 [8]HomolováV,Janovec J,Záhumensk■P,V■rostková A. Mater Sci Eng,2003;A349:306 [9]Abe F.Metall Mater Trans,2005;36A:321 [10]Peng Z F,Ren Y Y.Acta Metall Sin,2001;37:472 (彭志方,任遥遥.金属学报,2001;37:472) [11]Peng Z F,Ren Y Y.Metall Mater Trans,2002;33A:3065 [12]Cheng S G,Peng Z F,Cheng F Y,Ren Y Y.Rare Met Mater Eng,2006;35:1765 (陈盛广,彭志方,陈方玉,任遥遥.稀有金属材料与工程,2006;35:1765) [13]Andersson J O,Helander T,Hdghmd L,Shi P F,Sundman B.Calphad,2002;26:273 [14]Sawada K,Kubo K,Abe F.Mater Sci Eng,2001;A319- 321:784 [15]Maruyama K,Sawada K,Koike J.ISIJ Int,2001;41:641 [16]Abe F,Horiuchi T,Taneike M,Sawada K.Mater Sci Eng, 2004;A378:299 [17]Taneike M,Abe F,Sawada K.Nature,2003;424:17 [18]Abe F,Taneike M,Sawada K.Int J Pressure Vessels Pip- ing,2007;84:3 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|