| Study on Microstructure Evaluation of hot rolled C-Mn-Si-Al TRIP steel based on dynamic transformation of undercooled austentie |
| ;;;; |
| 北京科技大学 |
|
Cite this article:
. Study on Microstructure Evaluation of hot rolled C-Mn-Si-Al TRIP steel based on dynamic transformation of undercooled austentie. Acta Metall Sin, 2008, 44(6): 686-692 .
|
|
|
Abstract Abstract: The microstructure evolution of hot rolled C-Mn-Al-Si TRIP steel based on dynamic transformation of undercooled austenite was investigated by uniaxial hot compression tests on a Gleeble1500 simulation test machine. The results showed that the volume fraction of ferrite transformed during dynamic transformation of undercooled austenite was determined by applied strain,at the meantime, the formation of ferrite was significantly accelerated and the remained austenite was much dispersed. When the isothermal bainitic treatment was implemented after the dynamic transformation of undercooled austenite, the remained austenite which had relatively larger size transformed quickly to bainite with fine structure and chaotic orientation, the small austenite islands with grain size between 0.5~1.5µm located among ferrite had higher stability and rather difficult transformed to bainite. By dynamic transformation of undercooled austenite and the subsequent isothermal bainitic transformation, a desired microstructure of hot rolled TRIP Steel was obtained, which characterized by fine grain size of ferrite, high volume fraction of retained austenite and the uniform distribution of bainite and retained austenite.
|
|
Received: 05 November 2007
|
|
|
[1]Ushilda K.Scand J Metall,1999,28:33 [2]Tosal Martinez L,Vanderschueren D,Jacobs S,Van dcputte S.Steel Res,2001;72:412 [3]Bcllhouse E M,Mertens A I M,McDermid J R.Mater Sc Eng,2007;A463:147 [4]Pichlcr A,Stiaszny P.Steel Res,1999;70:457 [5]Girault E,Mcrtens A,Jacques P,Houbaert Y,Verlinden B,Van Humbeeck J.Scr Mater,2001;44:885 [6]Barbe L,Verbeken K,Wettinck E.ISIJ lnt,2006;46:1251 [7]Meyer D,Vanderschueren D,De Cooman B C.ISIJ lnt 1999;39:813 [8]Jacques P J,Girault E,Mertens A,Verlinder B,Van Hum beeck J,Delannay F.ISIJ lnt,2001;41:1068 [9]Basuki A,Aernoudt E.Scr Mater,1999;40:1003 [10]Timokhina I B,Hodgson P D,Pereloma E V.Metall Mate Trans,2003;34A:1599 [11]Ryu H B,Speer J G,Wise J P.Metall Mater Trans,2002 33A:2811 [12]Yang W Y,Qi J J,Sun Z Q,Yang P.Acta Metall Sin 2004;40:135 (杨王玥,齐俊杰,孙祖庆,杨平.金属学报,2004:40:135) [13]Yang P,Fu Y Y,Cui F E,Sun Z Q.Acta Mctall Sin,2001; 37:592 (杨平,傅云义,崔凤娥,孙祖庆.金属学报.2001:37:592) [14]Mahieu J,Maki J,De Cooman B C,Claessens S.Metall Mater Trans,2002;33A:2573 [15]Mintz B.lnt Mater Rev,2001;46:169 [16]Miller R L,Trans ASM,1964;57:892 [17]Sung-Joon K,Chang G L,Ildong C,Sunghak L.Metall Mater Trans,2001;32A:505 [18]Qi J J,Yang W Y,Sun Z Q,Zhang X Z,Dong Z F.Acta Metall Sin,2005;41:605 (齐俊杰,杨王玥,孙祖庆,章晓中,董志峰.金属学报,2005;41:605) [19]De Meyer M,Mahicu J,De Cooman B C.Mater Sci Tech- nol,2002;18:1121 [20]Sakuma Y,Matsumura O,Takechi tl.Metall Trans,1991; 22A:489 [21]Lee Y K,Shin tt C,Jang Y C,Kim S H,Choi C S.Set Mater,2002;47:805 [22]Bhadeshia H K D H,Waugh A R.Aeta Metall,1982;30: 775 [23]ttanzaki A Z,Hodgson P D,Yue S.Metall Mater Trans, 1997;28A:2405 [24]Timokhina I B,Hodgson P D,Pcreloma E V.In:De Cooman B C ed.,Proc of Int Conf on TRIP Aided High Strength Ferrous Alloys,Wisscnschafts Vcrlag Mainz GmbH,Aachen,2002:181 [25]Tsuzaki K,Fukasaku S,Tomota Y,Maki T.Mater Trans, JIM,1991;32:222 [26]Singh S B,Bhadeshia H K D H.Mater Sci Technol,1996; 12:610 [27]Shipway P H,Bhadeshia H K D H.Mater Sei Technol, 1995;11:1116 [28]Luo H W,Zhao L,Kruijver S O,Sictsma J,Van der Zwaag S.ISIJ Int,2003;43:1219 [29]Jacques P,Cornet X,Harlot Ph,Ladricre J,Delannay F. Metall Mater Trans.1998;29A:2383 [30]Kawano O,Wakita.J,Esaka K,Abe It.Iron Steel Inst Jpn Int,1996;82:232 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|