Abstract The formation of a double-recirculation flow pattern(DRFP) in continuous casting mold will be helpful for the improvement of slab quality. In the present study, the condition for the formation of the DRFP in a slab continuous casting mold with blowing argon gas was quantitively described using the Lagrange multi-phase flow model, and the prediction was validated by the water model. The influences of argon gas volume flowrate, fluid steel mass flowrate, mold width, submergence depth of SEN (Submerged Entry Nozzle) and port downward angle on the DRFP were numerically investigated. The results show that it is important for ensuring the DRFP that the argon gas flowrate matchs the other casting conditions. The critical argon gas flowrate increases with the increasing fluid steel mass flowrate, and the range of argon gas flowrate for keeping the DRFP will be enlarged by decreasing the mold width and increasing the submergence depth of SEN as the fluid steel mass flowrate is more than 2.486 ton/min, nevertheless, the port downward angle of SEN has little effect on it. However, the operation parameters have no significant influence on it as the fluid steel mass flowrate is below 2.486 ton/min.
|
|
Received: 15 October 2007
|
|
|
[1]Herbertson J,He Q L,Flint P J,Mahapatra R.74th Steel- making Conference Proceedings,Warrendale,PA:Iron and Steel Society,1991:171 [2]Thomas B G,Jenkins M S,Mahapatra R B.Ironmaking Steelmaking,2004;31:485 [3]Thomas B G.Iron Steel Technol,2006;3(7):128 [4]Zhang L F,Yang S B,Cai K K,Li J Y,Wan X G,Thomas B G.Metall Mater Trans,2007;38B:63 [5]Thomas B G,Huang X,Sussman R C.Metall Mater Trans,1994;25B:527 [6]Kasai N,Iguchi M.Tetsu Hagané,2005;91:546 (笠井宣文,井口学.铁钢,2005;91:546) [7]Kasai N,Iguchi M.Tetsu Hagané,2005;91:847 (笠井宣文,井口学.铁钢,2005;91:847) [8]Ma F J,Wen G H,Li G.Steelmaking,2000;16(3):42 (马范军,文光华,李刚.炼钢,2000;16(3):42) [9]Zhang J M,He J C,Li B K.Acta Metall Sin,1995;31: 269 (张炯明,赫冀成,李宝宽.金属学报,1995;31:269) [10]Yu H X,Zhu G S,Wang X H,Zhang J M,Wang W J.J Univ Sci Technol Beijing,2003;25:215 (于会香,朱国森,王新华,张炯明,王万军.北京科技大学学报,2003;25:215) [11]Lu Q T,Yang R G,Wang X H,Zhang J M,Wang W J. Iron Steel,2006;41(7):29 (陆巧彤,杨荣光,王新华,张炯明,王万军.钢铁,2006;41(7):29) [12]Zhang S J,Zhu M Y,Zhang Y L,Zheng S G,Cheng N L, Song J X.Acta Metall Sin,2006;42:1087 (张胜军,朱苗勇,张永亮,郑淑国,程乃良,宋景欣.金属学报,2006;42:1087) [13]Cao N,Zhu M Y.Acta Metall Sin,2008;44:79 (曹娜,朱苗勇.金属学报,2008;44:79) [14]Andrzejewski P,Gotthelf D,Julius E,Haubrich H.80th Steelmaking Conference,Warrendale,PA:Iron and Steel Society/AIME,1997:153 [15]Dauby P H,Kuustreich S.Iron Steelmaker,2003;30(11): 21 [16]Kunstreich S,Dauby P H.Ironmaking Steelmaking,2005; 32:80 [17]Assar M B,Dauby P H,Lawson G D.83rd Steelmak- ing Conference,Warrendale,PA:Iron and Steel Soci- ety/AIME,2000:397 [18]Cao N,Zhu M Y.Acta Metall Sin,2007;43:834 (曹娜,朱苗勇.金属学报,2007;43:834) [19]Bai H,Thomas B G.Metall Mater Trans,2001;32B:253 [20]Bai H,Thomas B G.Metall Mater Trans,2001;32B:1143 [21]Toh T.Hasegawa H,Harada H.ISIJ Int,2001;41:1245 [22]Bessho N,Yoda R,Yamasaki H,Fujii T,Nozaki T,Taka- tori S.ISIJ Int,1991;31:40 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|