| DEGASSING EFFECT AND GRAIN REFINEMENT OF Al-Si ALLOY WITH POWER ULTRASOUND |
| ;TingJu Li;;; |
| 大连理工大学铸造工程研究中心 |
|
Cite this article:
TingJu Li. DEGASSING EFFECT AND GRAIN REFINEMENT OF Al-Si ALLOY WITH POWER ULTRASOUND. Acta Metall Sin, 2008, 44(4): 414-418 .
|
|
|
Abstract The degassing effect and the grain refinement of Al-Si alloy with power ultrasound were studied. The value of porosity volume of Al-Si alloy decreases obviously when the treated time is 60s. The grains are fine and globular when the solidification of Al-Si alloy was treated by power ultrasound and the grains are fine but not globular at isothermal temperature in the mushy zone with ultrasonic vibrations. The results imply that the expansion and collapse of cavities which results in the formation of nuclei plays the dominant important role in the formation of fine and globular grains.
|
|
Received: 21 September 2007
|
|
|
[1]Bai X Q,Li D H,Zhang L,He J C.Acta Metall Sin,2002; 38:483 (白晓清,李东辉,张林,赫冀成.金属学报,2002;38:483) [2]Abramov V,Abramov O,Bulgakov V,Sommer F.Mater Lett,1998;37:27 [3]Eskin G I.Ultrason Sonochem,2001;8:319 [4]Seifert J,Fischer F.Ultrasonics,1977;15:154 [5]Zhang H B,Zhai Q J,Qi F P,Gong Y Y.Trans Nonfer- rous Met Soc Chin,2004;14:302 [6]Li X T,Li T J,Li X M,Jin J Z.Ultrason Sonochem,2006; 13:121 [7]Gao X P,Li X T,Qie X W,Wu Y P,Li X M,Li T J.Acta Metall Sin,2007;43:17 (高学鹏,李新涛,郄喜望,吴亚萍,李喜孟,李廷举.金属学报,2007;43:17) [8]Slvamov O V.Hutink,1970;37:276 [9]Ying C F.Ultrasound.Beijing:Science Press,1990:10 (应崇福.超声学.北京:科学出版社,1990:10) [10]Campbell J.Int Met Rev,1981;26:71 [11]Schaefer R J,Glicksman M B.Trans AIME,1967;239: 257 [12]Southin R T.Trans AIME,1967;239:220 [13]Hu H Q.Metal Solidification Principle.Beijing:China Machine Press,2000:59 (胡汉起.金属凝固原理.北京:机械工业出版社,2000:59)q |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|