Magnetocaloric effect of LaFe11.9-xCoxSi1.1B0.2( x=0.7, 0.8, 0.9)
Cite this article: 

. Magnetocaloric effect of LaFe11.9-xCoxSi1.1B0.2( x=0.7, 0.8, 0.9). Acta Metall Sin, 2008, 44(3): 371-374 .

Download:  PDF(629KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The LaFe11.9-xCoxSi1.1B0.2 (x=0.7, 0.8, 0.9) compounds were prepared by arc melting. X-ray diffraction analysis shows that the phases of LaFe11.9-xCoxSi1.1B0.2 (x=0.7, 0.8, 0.9) compounds mainly consist of the NaZn13-type cubic structure phase and a small amount of the a-Fe phase. The space group is Fm-3c. It is found that the lattice parameters and the lattice volumes have slightly increase with increasing x. the lattice parameters are found to be 11.487,11.496 and 11.498 Å and the lattice volume is found to be 1515.9,1519.4 and 1519.9 Å3 for x=0.7, 0.8 and 0.9. The magnetic measurement shows that the Curie temperature of the compounds have slightly increased with increasing Co and near the room temperature, 270, 290 and 300 K for x=0.7, 0.8 and 0.9. The maximum values of the magnetic entropy change of LaFe11.9-xCoxSi1.1B0.2 compounds are 7.47, 5.93 and 5.90 Jkg-1K-1 for x=0.7, 0.8 and 0.9 for a field change from 0 to 1.5 T. It markedly exceeds that of pure Gd at the corresponding applied field. The relative cooling power (RCP) based on the magnetic entropy change is as large as that of pure Gd at the corresponding applied field.
Key words:  Magnetic entropy change      Intermetallic compound      Relative cooling power      
Received:  03 July 2007     
ZTFLH:  TM271.4  
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2008/V44/I3/371

[1]Zimm C B,Jastrab A,Pecharsky V K,Gschneidner K A Jr,Osborne M,Anderson I.Adv Cryog Eng,1998;43: 1759
[2]Fujita A,Fujieda S,Fukamiehi K.Phys Rev,2001;65 B: 014410
[3]Hu F X,Shen B G,Sun J R,Cheng Z H,Rao G H,Zhang X X.Appl Phys Lett,2001;78:3675
[4]Tegus O,Brück E,Buschow K H J,de Boer F R.Nature, 2002;415:150
[5]Pecharsky V K,Gschneidner K A.Appl Phys Lett,1997; 70:3299
[6]Fujita A,Fujieda S,Hasegawa Y,Fukamichi K.Phys Rev, 2003;67B:104416
[7]Hu F X,Shen B G,Sun J R,Wang G J,Cheng Z H.Appl Phys Lett,2002;80:826
[8]Huang J H,Song L,Jin P Y,Wang G F,Liu J R,Yan H W,Zhang J X.Funct Mater,2006;37:1888 (黄焦宏,松林,金培育,王高峰,刘金荣,闫宏伟,张久兴功能材料,2006;37:1888)
[9]Xie S H,Li J Q,Zhuang Y H.J Magn Magn Mater,2007; 311:589
[10]Entel P,Shr(?)ter M.Physics,1989;161B:160
[11]Sinnema S,Franse J J M,Radwanski R J,Menovsky A, de Boer F R.J Phys F:Met Phys,1987;17:233
[12]Fujita A,Akamatsu Y,Fukamichi K.J Appl Phys,1999; 85:4756
[13]Gschneidner Jr K A,Pecharsky V K.Annu Rev Mater Sci,2000;30:387
[1] DING Zongye, HU Qiaodan, LU Wenquan, LI Jianguo. In Situ Study on the Nucleation, Growth Evolution, and Motion Behavior of Hydrogen Bubbles at the Liquid/ Solid Bimetal Interface by Using Synchrotron Radiation X-Ray Imaging Technology[J]. 金属学报, 2022, 58(4): 567-580.
[2] ZHOU Lijun, WEI Song, GUO Jingdong, SUN Fangyuan, WANG Xinwei, TANG Dawei. Investigations on the Thermal Conductivity of Micro-Scale Cu-Sn Intermetallic Compounds Using Femtosecond Laser Time-Domain Thermoreflectance System[J]. 金属学报, 2022, 58(12): 1645-1654.
[3] Hua JI,Yunlai DENG,Hongyong XU,Weiqiang GUO,Jianfeng DENG,Shitong FAN. The Influence of Welding Line Energy on the Microstructure and Property of CMT Overlap Joint of 5182-Oand HC260YD+Z[J]. 金属学报, 2019, 55(3): 376-388.
[4] Liqun CHEN, Zhengchen QIU, Tao YU. Effect of Ru on the Electronic Structure of the [100](010) Edge Dislocation in NiAl[J]. 金属学报, 2019, 55(2): 223-228.
[5] CAO Lihua, CHEN Yinbo, SHI Qiyuan, YUAN Jie, LIU Zhiquan. Effects of Alloy Elements on the Interfacial Microstructure and Shear Strength of Sn-Ag-Cu Solder[J]. 金属学报, 2019, 55(12): 1606-1614.
[6] HE Xianmei, TONG Liuniu, GAO Cheng, WANG Yichao. Effect of Nd Content on the Structure and Magnetic Properties of Si(111)/Cr/Nd-Co/Cr Thin Films Prepared by Magnetron Sputtering[J]. 金属学报, 2019, 55(10): 1349-1358.
[7] Min ZHANG, Erlong MU, Xiaowei WANG, Ting HAN, Hailong LUO. Microstructure and Mechanical Property of the Welding Joint of TA1/Cu/ X65 Trimetallic Sheets[J]. 金属学报, 2018, 54(7): 1068-1076.
[8] Huijun KANG, Jinling LI, Tongmin WANG, Jingjie GUO. Growth Behavior of Primary Intermetallic Phases and Mechanical Properties for Directionally Solidified Al-Mn-Be Alloy[J]. 金属学报, 2018, 54(5): 809-823.
[9] Ning ZHAO,Jianfeng DENG,Yi ZHONG,Luqiao YIN. Evolution of Interfacial Intermetallic Compounds in Ni/Sn-xCu/Ni Micro Solder Joints Under Thermomigration During Soldering[J]. 金属学报, 2017, 53(7): 861-868.
[10] Zhijie ZHANG,Mingliang HUANG. Liquid-Solid Electromigration Behavior of Cu/Sn-52In/Cu Micro-Interconnect[J]. 金属学报, 2017, 53(5): 592-600.
[11] Dawei WANG,Shichao XIU. Effect of Bonding Temperature on the Interfacial Micro-structure and Performance of Mild Steel/Austenite Stainless Steel Diffusion-Bonded Joint[J]. 金属学报, 2017, 53(5): 567-574.
[12] Zongyue BI,Jun YANG,Haizhang LIU,Wanpeng ZHANG,Yaobin YANG,Lei TIAN,Xiaojiang HUANG. INVESTIGATION ON THE WELDING PROCESS AND MICROSTRUCTURE AND MECHANICAL PROPERTY OF BUTT JOINTS OF TA1/X65 CLAD PLATES[J]. 金属学报, 2016, 52(8): 1017-1024.
[13] Liangshun LUO,Tong LIU,Yanning ZHANG,Yanqing SU,Jingjie GUO,Hengzhi FU. MICROSTRUCTURE EVOLUTION AND GROWTH BE-HAVIORS OF FACETED PHASE IN DIRECTIONALLY SOLIDIFIED Al-Y ALLOYS I. Microstructure Evolution of Directionally Solidified Al-15%Y Hypereutectic Alloy[J]. 金属学报, 2016, 52(7): 859-865.
[14] Manjiao CHEN,Jiankang HUANG,Cuicui HE,Yu SHI,Ding FAN. THERMODYNAMIC ANALYSIS OF THE FORMATION OF Fe-Al-Zn INTERMETALLIC COMPOUNDS IN Al/GALVANIZED STEEL INTERFACE[J]. 金属学报, 2016, 52(1): 113-119.
[15] Wenjing MA,Changbo KE,Minbo ZHOU,Shuibao LIANG,Xinping ZHANG. PHASE-FIELD CRYSTAL SIMULATION ON EVOLU- TION AND GROWTH KINETICS OF KIRKENDALL VOIDS IN INTERFACE AND INTERMETALLIC COMPOUND LAYER IN Sn/Cu SOLDERING SYSTEM[J]. 金属学报, 2015, 51(7): 873-882.
No Suggested Reading articles found!