Please wait a minute...
Acta Metall Sin  2007, Vol. 43 Issue (9): 913-919     DOI:
Research Articles Current Issue | Archive | Adv Search |
CRYSTAL PLASTICITY ANALYSIS OF GRAIN ORIENTATION EVOLUTION OF POLYCRYSTALLINE COPPER DURING UNIAXIAL COMPRESSION
;;;
清华大学机械工程系先进成形制造教育部重点实验室
Cite this article: 

;. CRYSTAL PLASTICITY ANALYSIS OF GRAIN ORIENTATION EVOLUTION OF POLYCRYSTALLINE COPPER DURING UNIAXIAL COMPRESSION. Acta Metall Sin, 2007, 43(9): 913-919 .

Download:  PDF(443KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The initial morphology and mean orientation of columnar-grains of pure copper was obtained by electron backscattering diffraction (EBSD). A finite element model based on crystal plasticity was established to simulate the orientation and deformation band evolution of individual grain during uniaxial compression. Corresponding compression test was carried out to obtain experimental data which showed the actual evolution of orientation and band morphology in the polycrystalline sample. A series of statistical results of grain orientation evolution were obtained, and the calculated results were compared to experimental data.
Key words:  columnar grain      pure copper      grain orientation      
Received:  18 December 2006     
ZTFLH:  TG146.1  
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2007/V43/I9/913

[1]Taylor G I.J Inst Met,1938;62:307
[2]Sachs G.Z Ver Deut Ing,1928;72:734
[3]Bronkhorst C A,Kalidindi S R,Anand L.Philos Trans R Soc London,1992;341:443
[4]Kalidindi S R,Bronkhorst C A,Anand L.J Mech Phys Solids,1992;40:537
[5]Peirce D,Asaro R J,Needleman A.Acta Metall,1982;30: 1087
[6]Wu P D,Neale K W,van der Giessen E.Int J Plast,1996; 12:1199
[7]Delannay L,Kalidindi S R,van Houtte P.Mater Sci Eng, 2002;A336:233
[8]Delannay L,Loge R E,Chastel Y,Van Houtte P.Acta Mater,2002;50:5127
[9]Van Houtte P,Delannay L,Kalidindi S R.Int J Plast, 2002;18:359
[10]Dong X H,Zheng Y,Li Z G.Chin Mech Eng,2003;15: 1339 (董湘怀,郑莹,李志刚.中国机械工程,2003;15:1339)
[11]Bhattacharyya A,El-Danaf E,Kalidindi S R,Doherty R D.Int J Plast,2001;17:861
[12]Panchanadeeswaran S,Doherty R D,Becket R.Acta Mater,1996;44:1233
[13]Raabe D,Sachtleber M,Zhao Z,Roters F,Zaefferer S. Acta Mater,2001;49:3433
[14]Delannay L,Jacques P J,Kalidindi S R.Int J Plast,2006; 22:1879
[15]Deng Y L,Zhang X M,Tang J G,Liu Y,Chen Z Y,Zhou Z P.Acta Metall Sin,2005;41:477 (邓运来,张新明,唐建国,刘瑛,陈志勇,周卓平.金属学报,2005;41:477)
[16]van Houtte P,Li S,Seefeldt M,Delannay L.Int J Plast, 2005;21:589a
[1] JIANG Weining, WU Xiaolong, YANG Ping, GU Xinfu, XIE Qingge. Formation of Dynamic Recrystallization Zone and Characteristics of Shear Texture in Surface Layer of Hot-Rolled Silicon Steel[J]. 金属学报, 2022, 58(12): 1545-1556.
[2] Shuangming LI, Binqiang WANG, Zhenpeng LIU, Hong ZHONG, Rui HU, Yi LIU, Ximing LUO. Grain Orientation Competitive Growth of High Melting Point Metals Ir and Mo Under Electron Beam Floating Zone Melting[J]. 金属学报, 2018, 54(10): 1435-1441.
[3] Hai ZHANG,Shilei LI,Gang LIU,Yanli WANG. Effects of Hot Working on the Microstructure and Thermal Ageing Impact Fracture Behaviors of Z3CN20-09MDuplex Stainless Steel[J]. 金属学报, 2017, 53(5): 531-538.
[4] Yongjun FU, Ping YANG, Qiwu JIANG, Xiaoda WANG, Wenxu JIN. EVOLUTION OF TEXTURES OF COLUMNAR GRAINS IN Fe-3%Si ELECTRICAL STEEL SLABS[J]. 金属学报, 2015, 51(5): 545-552.
[5] TANG Ning, WANG Yanli, XU Qingyan, ZHAO Xihong, LIU Baicheng. NUMERICAL SIMULATION OF DIRECTIONAL SOLIDIFIED MICROSTRUCTURE OF WIDE-CHORD AERO BLADE BY BRIDGEMAN PROCESS[J]. 金属学报, 2015, 51(4): 499-512.
[6] LIU Yongkang, HUANG Haiyou, XIE Jianxin. ANISOTROPIC DEFORMATION BEHAVIOR OF CONTINUOUS COLUMNAR-GRAINED CuNi10Fe1Mn ALLOY[J]. 金属学报, 2015, 51(1): 40-48.
[7] SHAO Yuanyuan, YANG Ping, MAO Weimin. ANALYSIS ON GRAIN BOUNDARY EFFECTS OF COLUMNAR GRAINED ELECTRICAL STEEL[J]. 金属学报, 2014, 50(3): 259-268.
[8] XIA Dongsheng, YANG Ping, XIE Li, MAO Weimin. INFLUENCE OF HEATING RATE ON THE DECARBU- RIZED ANNEALING MICROSTRUCTURE AND TEXTURE IN LOW-CARBON NON-ORIENTED ELECTRICAL STEEL[J]. 金属学报, 2014, 50(12): 1437-1445.
[9] MO Yongda, JIANG Yanbin, LIU Xinhua, XIE Jianxin. MECHANICAL PROPERTIES AND WORK HARDENING BEHAVIOR OF COLUMNAR-GRAINED HAl77-2 BRASS[J]. 金属学报, 2014, 50(11): 1367-1376.
[10] ZHANG Hang, XU Qingyan, SUN Changbo, QI Xiang,TANG Ning, LIU Baicheng. SIMULATION AND EXPERIMENTAL STUDIES ON GRAIN SELECTION BEHAVIOR OF SINGLE CRYSTAL SUPERALLOY :I. Starter Block[J]. 金属学报, 2013, 49(12): 1508-1520.
[11] ZHANG Hang, XU Qingyan, SUN Changbo, QI Xiang,TANG Ning, LIU Baicheng. SIMULATION AND EXPERIMENTAL STUDIES ON GRAIN SELECTION BEHAVIOR OF SINGLE  CRYSTAL SUPERALLOY :II. Spiral Part[J]. 金属学报, 2013, 49(12): 1521-1531.
[12] XU Jiayu CHEN Hongtao LI Mingyu. STUDY ON LEAD-FREE SOLDER JOINT RELIABILITY BASED ON GRAIN ORIENTATION[J]. 金属学报, 2012, 48(9): 1042-1048.
[13] ZHANG Ning YANG Ping MAO Weimin. INFLUENCE OF COLUMNAR GRAINS ON THE COLD ROLLING TEXTURE EVOLUTION IN Fe-3%Si\ ELECTRICAL STEEL[J]. 金属学报, 2012, 48(7): 782-788.
[14] WANG Zhen LIU Xuefeng XIE Jianxin. MICROSTRUCTURE AND MECHANICAL PROPERTIES EVOLUTIONS OF CONTINUOUS COLUMNAR-GRAINED CuAlNi ALLOY WIRES DURING DIELESS DRAWING PROCESS[J]. 金属学报, 2012, 48(7): 867-874.
[15] ZHANG Ning YANG Ping MAO Weimin. INFLUENCE OF COLUMNAR GRAINS ON THE RECRYSTALLIZATION TEXTURE EVOLUTION IN Fe-3%Si ELECTRICAL STEEL[J]. 金属学报, 2012, 48(3): 307-314.
No Suggested Reading articles found!