| Effects of deformation and aging on microstructure and mechanical properties of AZ91 magnesium alloy |
| ;;;;; |
| 北京科技大学 |
|
Cite this article:
;. Effects of deformation and aging on microstructure and mechanical properties of AZ91 magnesium alloy. Acta Metall Sin, 2007, 43(9): 920-924 .
|
|
|
Abstract Microstructures and mechanical properties of AZ91 magnesium alloy after homogenized, hot extrusion and succedent aging are investigated. The results show that dynamic recrystallization occurs during extrusion at elevated temperatures of 320℃ and 380℃; compared to the as-cast alloy, microstructures of the extruded AZ91 alloy are refined, and the mechanical properties are enhanced remarkably; succedent aging is helpful to improvement of mechanical properties of the extruded AZ91 alloy. In this experiment, the ultimate tensile strength of the AZ91 alloy extruded at 380℃and aged at 200℃×10h is about 357MPa, and the elongation of the alloy reaches about 8%.
|
|
Received: 26 December 2006
|
|
|
[1]Mordike B L,Ebert T.Mater Sci Eng,2001;A302:37 [2]Friedrich H,Schumann S.J Mater Process Technol,2001; 117:276 [3]Matucha K H.In:Cahn R W,Hassen P,Kramer E J, eds.;translated by Ding D Y,et al.,Materials Science and Technology:A Comprehensive Treatment,Vol.8:Struc- ture and Properties of Nonferrous Alloys,Beijing:Science Press,1999:105 (Matucha K H.见:Cahn R W,Hassen P,Kramer E J,主编;丁道云,等,译.材料科学与技术丛书,第8卷:非铁合金的结构和性能,北京:科学出版社,1999:105) [4]Watanabe H,Tsutsui H,Mukai T,Kohzu M,Tanabe S, Higashi K.Int J Plast,2001;17:387 [5]Aghion E,Bronfin B,Eliezer D.J Mater Process Technol, 2001;117:381 [6]Kleiner S,Beffort O,Wahlen A,Uggowitzer P J.J Light Met,2002;2:277 [7]Cizek L,Greger M,Pawlica L,Dobrzanski L A,Tanski T. J Mater Process Technol,2004;157-158:466 [8]Liu Z,Liu C Y,Wang Z G,Wang Y,Han X L.Acta Metall Sin,1999;35:869 (刘正,刘重阳,王中光,王越,韩行林.金属学报,1999;35:869) [9]Mabuchi M,Kubota K,Higashi K.Mater Trans JIM, 1995;36:1249 [10]Yu BY,Bao C L,Song H W,Qiao R J,Liu Z,Yu H P. Hot Work Technol,2005;34(8):30 (于宝义,包春玲,宋鸿武,乔日金,刘正,于海朋.热加工工艺,2005;34(8):30) [11]Jin J B,Wang Z X,Liu X F,Xie J X.Acta Metall Sin, 2006;42:1014 (金军兵,王智祥,刘雪峰,谢建新.金属学报,2006;42:1014) [12]Ion S E,Humphreys F J,White S H.Acta Metall,1982; 30:1909 [13]Mao W M,Zhao X B.Recrystallization and Grain Growth of Metals.Beijing:Metallurgical Industry Press,1994:47 (毛卫民,赵新兵.金属的再结晶与晶粒长大.北京:冶金工业出版社,1994:47) [14]Duly D,Simon J P,Brechet Y.Acta Metall Mater,1995; 43:101 [15]Celotto S.Acta Mater,2000;48:1775 [16]Kubota K,Mabuchi M,Higashi K.J Mater Sci,1999;34: 2255 [17]Wang L Y,Huang G S,Fan Y G,Huang G J.Chin J Nonferrous Met,2003;13:594 (汪凌云,黄光胜,范永革,黄光杰.中国有色金属学报,2003;13:594) |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|