| Preparation of Nd Bulk with Ultrafine Nanocrystalline Structure and its Physical Property |
| LU Nianduan; SONG Xiaoyan; ZHANG Jiuxing; LI Erdong |
| Key Lab of Advanced Functional Materials; Ministry of Education; College of Materials Science and Engineering; Beijing University of Technology |
|
Cite this article:
LU Ni; uan; SONG Xiaoyan; ZHANG Jiuxing; LI Erdong. Preparation of Nd Bulk with Ultrafine Nanocrystalline Structure and its Physical Property. Acta Metall Sin, 2007, 43(7): 739-743 .
|
|
|
|
|
Received: 16 November 2006
|
|
|
[1]Tomaszewicz E.J Mater Sci,2006;41:1675 [2]Amelin Y,Rotenberg E.Earth Planet Sci Lett,2004;223: 267 [3]Uda T,Jacob K T,Hirasawa M.Science,2000;289:2326 [4]Harrison P G.,Bailey C,Azelee W.J Catalysis,1999;186: 147 [5]Laurent C,Zoltán A,Gál T P,Braun F J,DiSalvo B B, J(?)rgen H.Solid State Chem,2001;162:90 [6]Soh D B S,Seongwoo Y,Nilsson J,Sahu J K,Kyunghwan O,Seungin B,Yoonchan J,Codemard C,Dupriez P,Jae- sun K,Philippor V.IEEE J Q Wantum Electronic,2004; 40:1275, [7]Kumar G A,Lu J R,Alexander,Kaminskii A,Ueda Ken- I,Member,Yagi Hideki,Yanagitani Takagimi,Unnikrish- nan N V.IEEE J Quantum Electron,2004;40:747 [8]Amadeh A,Pahlevani B,Heshmati-Manesh S.Corros Sci, 2002;44:2321 [9]Yamaguchi K,Itagaki K,Kim D Y,Ohtsuka M.J Alloys Compd,1995;221:161 [10]Fray D J.Science,2000;289:2295 [11]Worrell E,Martin N,Price L.Energy,2002;5:1189 [12]Yada M,Mihara M,Mouri S,Kuroki M,Kijima T.Adv Mater,2002;14:309 [13]Sohei U,Muhamad S,Takayuki I,Takashi N.Symth Met, 2005;154:217 [14]Gleiter H.Prog Mater Sci,1989;33:223 [15]Erb U,El-Sherik A M,Palumbo G,Aust K T.Nanostruct Mater,1993;2:383 [16]Valley R Z,Korznikor A V,Mulyukov R R.Mater Sci Eng,1993;A168:141 [17]Yoshizawa Y,Oguma S,Yamauchi K.J Appl Phys,1988; 64:6044 [18]Zhang H W,Hei Z K,Liu G,Lu J,Lu K.Acta Mater, 2003;51:1871 [19]Dogan C,Rawers J,Govier D,Korth G.Nanostruct Mater,1994;4:631 [20]Lillo T M,Korth G.Nanostruct Mater,1998;10:95 [21]Zhang H W,Gopalan R,Mukai T,Hono K.Scr Mater, 2005;53:863 [22]Song X Y,Zhang J X,Yue M,Li E D,Zeng H,Lu N D, Zhou M L,Zuo T Y.Adv Mater,2006;18:1210 [23]Haia N H,Lemoine R.J Magn Magn Mater,2005;293: 75 [24]Song X Y,Liu X M,Zhang J X.J Am Ceram Soc,2006; 89:494 [25]Yang C C,Jiang Q.Acta Mater,2005;53:3305 [26]Jeong Hee-Won,Hata Seiichi,Shimokohbe Akira.The 15th IEEE Int Conf on MEMS 2002,Las Voges,2002: 372 [27]Han M,Panlsen J A,Snyder J E,Jiles D C,Lograsso T A,Schlagel D L.IEEE Trans Magn,2002;38:5 [28]Kissinger.Anal Chem,1957;29:1702 [29]Lyubina J,Gutfleisch O,Skomski R,Muller K H,Schultz L.Scr Mater,2005;53:469 [30]Hong S J,Moon D G,Han J I,Chang S G,Huh M Y. Sensors Proceding of IEEE,2004;2:183 [31]Peng Y C,Zhao X W,Fu G S,Wang Y L.J Synth Cryst, 2005;34:498 (彭英才,zhao X W,傅广生,王英龙.人工晶体学报.2005; 34:948) [32]Tritt T M,Nolas G S,Slack G A,Cohn J S.J Appl Phys, 1996;11:8412 [33]Gschneidner K A Jr,Eyring L.Handbook on the Physics and Chemistry of Rare Earths.Vol.16,Amsterdam: North-Holland Publishing,1993:111 [34]Lu K,Sui M L.Acta Metall Mater,1995;43:3325 [35]Suryanarayana C,Koch C C.Hyperfine Integer,2000; 130:5 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|