清华大学机械工程系
Cite this article: 

. . Acta Metall Sin, 2007, 43(10): 1113-1120 .

Download:  PDF(673KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Complex heat radiation transfer exists in the directional solidification process of multiple turbine blades of superalloy investment casting in vacuum Bridgman furnace. In order to control the quality of casting products, avoid the casting defects and increase the productivity at the same time, it is necessary to investigate the temperature distribution of multiple turbine blades during the directional solidification process. In this paper, a ray tracing model was developed based on Monte Carlo method and used to deal with the complex heat radiation transfer among the multiple turbine blades and the furnace wall during the withdrawal process dynamically. The withdrawal rate and furnace geometry were considered in this model, and the temperature distributions during directional solidification process at two different withdrawal rates were investigated. The simulated cooling curves of special sample positions were compared with the experimental ones and agreed well.
Key words:  Directional solidification      multiple blades      furnace geometry      investment casting      superalloy      numerical      
Received:  12 February 2007     
ZTFLH:  TG292  
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2007/V43/I10/1113

[1]Jasinski T,Rohsenow W M,Witt A F,Naumann R J.J Cryst Growth,1984;66:469
[2]Jasinski T,Rohsenow W M,Witt A F.J Cryst Growth, 1983;61:339
[3]Overfelt R A,Wilcox R C.J Cryst Growth,1995;147: 403
[4]Wilcox W R.J Cryst Growth,1980;48:416
[5]Yu K O,Beffel M J,Robinson M,Goettsch D D,Thomas B G,Pinella D,Carlson R G.Trans Am Foundrymens Sac,1990;53:417
[6]Yu K O,Oti J A,Robinson M,Carlson R G.Superalloys 1992.Warrendale,PA:TMS,1992:135
[7]Saitou M,Hirata A.J Cryst Growth,I991;113:147
[8]Ouyang H,Shyy W.Int J Heat Mass Transfer,1996;39: 2039
[9]Ouyang H,Shyy W.Int J Heat Mass Transfer,1997;40: 2293
[10]Galantucci L M,Tricarico L.J Mater Process Technol, 1998;77:160
[11]Wang D,Overfelt R A.In:Cross M,Evans J W eds., Proc Conf Comput Model Mater,Min and Met Process, San Diego,Wanrrendale,Pennsylvania:TMS,2001:461
[12]Zhu J D,Ohnaka I,Kudo K,Obara S,Kimatsuka A,Wang T M,Kinoshita F,Murakami T.In:Stefanescu D M ed., Proc 10th Int Symp Model Cast Weld Adv Solidification Process,Wanrrendale,Pennsylvania:TMS,2003:447
[13]Li J R,Liu S Z,Zhong Z G.J Mater Sci Technol,2002; 18:315
[14]Li J R,Liu S Z,Yuan H L,Zhong Z G.J Mater Sci Tech- nol,2003;19:532
[15]Liang Z J,Li J R,Liu B C,Xu Q Y,Yuan H L,Liu S Z. Multiph Phenom Model Simul Mater Process,Charlotte: TMS,2004:227
[16]Jiang W H.Heat Transfer.Beijing:Higher Education Press,1989:172 (姜为珩.传热学.北京:高等教育出版社,1989:172)
[17]Siegel R,Howell J R.Thermal Radiation Heat Transfer. 3rd Ed,Washington D C,Hemisphere:Hemaisphere and McGraw-Hill,1992.
[1] JIANG He, NAI Qiliang, XU Chao, ZHAO Xiao, YAO Zhihao, DONG Jianxin. Sensitive Temperature and Reason of Rapid Fatigue Crack Propagation in Nickel-Based Superalloy[J]. 金属学报, 2023, 59(9): 1190-1200.
[2] BAI Jiaming, LIU Jiantao, JIA Jian, ZHANG Yiwen. Creep Properties and Solute Atomic Segregation of High-W and High-Ta Type Powder Metallurgy Superalloy[J]. 金属学报, 2023, 59(9): 1230-1242.
[3] BI Zhongnan, QIN Hailong, LIU Pei, SHI Songyi, XIE Jinli, ZHANG Ji. Research Progress Regarding Quantitative Characterization and Control Technology of Residual Stress in Superalloy Forgings[J]. 金属学报, 2023, 59(9): 1144-1158.
[4] ZHENG Liang, ZHANG Qiang, LI Zhou, ZHANG Guoqing. Effects of Oxygen Increasing/Decreasing Processes on Surface Characteristics of Superalloy Powders and Properties of Their Bulk Alloy Counterparts: Powders Storage and Degassing[J]. 金属学报, 2023, 59(9): 1265-1278.
[5] FENG Qiang, LU Song, LI Wendao, ZHANG Xiaorui, LI Longfei, ZOU Min, ZHUANG Xiaoli. Recent Progress in Alloy Design and Creep Mechanism of γ'-Strengthened Co-Based Superalloys[J]. 金属学报, 2023, 59(9): 1125-1143.
[6] ZHANG Jian, WANG Li, XIE Guang, WANG Dong, SHEN Jian, LU Yuzhang, HUANG Yaqi, LI Yawei. Recent Progress in Research and Development of Nickel-Based Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1109-1124.
[7] MA Dexin, ZHAO Yunxing, XU Weitai, WANG Fu. Effect of Gravity on Directionally Solidified Structure of Superalloys[J]. 金属学报, 2023, 59(9): 1279-1290.
[8] CHEN Jia, GUO Min, YANG Min, LIU Lin, ZHANG Jun. Effects of W Concentration on Creep Microstructure and Property of Novel Co-Based Superalloys[J]. 金属学报, 2023, 59(9): 1209-1220.
[9] ZHAO Peng, XIE Guang, DUAN Huichao, ZHANG Jian, DU Kui. Recrystallization During Thermo-Mechanical Fatigue of Two High-Generation Ni-Based Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1221-1229.
[10] LI Jiarong, DONG Jianmin, HAN Mei, LIU Shizhong. Effects of Sand Blasting on Surface Integrity and High Cycle Fatigue Properties of DD6 Single Crystal Superalloy[J]. 金属学报, 2023, 59(9): 1201-1208.
[11] GONG Shengkai, LIU Yuan, GENG Lilun, RU Yi, ZHAO Wenyue, PEI Yanling, LI Shusuo. Advances in the Regulation and Interfacial Behavior of Coatings/Superalloys[J]. 金属学报, 2023, 59(9): 1097-1108.
[12] WANG Lei, LIU Mengya, LIU Yang, SONG Xiu, MENG Fanqiang. Research Progress on Surface Impact Strengthening Mechanisms and Application of Nickel-Based Superalloys[J]. 金属学报, 2023, 59(9): 1173-1189.
[13] LU Nannan, GUO Yimo, YANG Shulin, LIANG Jingjing, ZHOU Yizhou, SUN Xiaofeng, LI Jinguo. Formation Mechanisms of Hot Cracks in Laser Additive Repairing Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1243-1252.
[14] MU Yahang, ZHANG Xue, CHEN Ziming, SUN Xiaofeng, LIANG Jingjing, LI Jinguo, ZHOU Yizhou. Modeling of Crack Susceptibility of Ni-Based Superalloy for Additive Manufacturing via Thermodynamic Calculation and Machine Learning[J]. 金属学报, 2023, 59(8): 1075-1086.
[15] LIU Xingjun, WEI Zhenbang, LU Yong, HAN Jiajia, SHI Rongpei, WANG Cuiping. Progress on the Diffusion Kinetics of Novel Co-based and Nb-Si-based Superalloys[J]. 金属学报, 2023, 59(8): 969-985.
No Suggested Reading articles found!