FURTHER INVESTIGATION OF EFFECTS OF ATOMIC HYDROGEN AND FLAKES ON MECHANICAL PROPERTIES OF WHEEL STEEL |
Xuechong Ren |
北京科技大学材料科学与工程学院 |
|
Cite this article:
Xuechong Ren. FURTHER INVESTIGATION OF EFFECTS OF ATOMIC HYDROGEN AND FLAKES ON MECHANICAL PROPERTIES OF WHEEL STEEL. Acta Metall Sin, 2007, 42(1): 53-58 .
|
Abstract The effects of hydrogen and flakes on impact toughness and fatigue properties of a wheel steel have been investigated. The results show that atomic hydrogen has no effect on impact toughness when the diffusible hydrogen concentration is low (C0≤0.7×10-6). The flakes decrease and fluctuate impact toughness. Atomic hydrogen has no effect on fatigue properties when the diffusible hydrogen concentration is low (C0≤0.7×10-6). But atomic hydrogen can promote the initiation of fatigue cracks and increase the fatigue crack growth rate when the hydrogen concentration is high enough (C0≥2.5×10-6). The flakes increase and undulate the fatigue crack growth rate.
|
Received: 21 July 2006
|
|
[1]Ren X C,Chu W Y,Li J x,Qiao L J,Jiang B,Chen G, Cui Y H.Acta Metall Sin,2006;42:153 (任学冲,褚武扬,李金许,乔利杰,江波,陈刚,崔银会.金属学报,2006;42:153) [2]Kelestemur M H,Chaki T K.Int J Fatigue,2001;23:169 [3]Oda Y,Noguchi H.Int J Fract,2005;132(2):99 [4]Barbangelo A.J Eng Mater Technol,1987;109:119 [5]Nong G,Yao W X,Cao Y z.Mater Charact,1992;28:15 [6]Wang G Z,Ren X C,Chen J H.Metall Mater Trans, 2004; 35:1765 [7] Griffith J R,Owen D R J.J Mech Phys Solids,197l;19: 419 [8]Ritchie R O,Knott J F,Rice J R. J Mech Phys Solids, 1973;21:395 [9] Chen J H,Wang Q,Wang G Z,Li Z. Acta Mater,2003; 51:1841 [10]Curry D A,Knott J F.Met Sci,1978;12:511 [11]Robertson I M.Eng Fract Mech,2001;68:671 [12]Neumann P.Acta Metall Mater,1990;38:1933 [13]Vinogardov A,Hashimoto S,Miura S.Acta Metall Mater, 1995;43:6750 |
No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|