| IMAGE ANALYSIS OF LC4CS ALUMINUM ALLOY SIMULATIVE AND ACCELERATED CORROSION SAMPLE |
| Song S Z |
| 天津大学材料学院 |
|
Cite this article:
Song S Z. IMAGE ANALYSIS OF LC4CS ALUMINUM ALLOY SIMULATIVE AND ACCELERATED CORROSION SAMPLE. Acta Metall Sin, 2006, 42(4): 426-430 .
|
|
|
Abstract Image recognition was used to study the corrosion morphology of LC4CS aluminum alloy samples with periodic rain tests, and the concept of image feature δ was introduced. The effects of each orthogonal experiment factor on acceleration were analyzed by image feature δ, the best combination of factor lever for accelerated corrosion test was also obtained. The conclusion was consistent with the result based on the corrosion weight loss.
|
|
Received: 21 July 2005
|
|
|
[1] Li J, Li M, Sun Z. Corrosion, 1999; 55: 498 [2] Lin C, Wang F P, Li X G. J Chin Soc Corros Prot, 2004; 24:249 (林 翠,王凤平,李晓钢.中国腐蚀与防护学报, 2004;24: 249) [3] Nishikata A, Yamashita Y, Katayama H, Tsuru T, Usami A, Tanabe K, Mabuchi H. Corros Sci, 1995; 37: 2095 [4] Yadav A P, Nishikata A, Tsuru T. Corros Sci, 2004; 46: 169 [5] Song S Z, Wang S Y, Gao Z M, Zhang X Y, Ma Y J, Li J Z. Acta Metall Sin, 2002; 38: 893 (宋诗哲,王守琰,高志明,张晓云,马颐军,李家柱.金属学 报,2002;38:893) [6] Wang S Y, Song S Z. Mater Sci Eng, 2004; A385: 377 [7] Liu M, Zhang X Y, Lu F, Tao C H, Wang Y Z, Cai J P, Li M Z. Corros Sci Prot Technol, 2005; 17: 271 (刘明,张晓云,陆峰,陶春虎,王永哲,蔡健平,李牧铮. 腐蚀科学与防护技术,2005;17:271) [8] Hou H G, Wang Y M. Orthogonal Experiment. Changchun: Jilin People's Publishing Press, 1985: 8 (侯化国,王玉民.正交试验法.长春:吉林人民出版社,1985: 8)K |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|