CORROSION BEHAVIORS OF LOW ALLOY STEEL AND CARBON STEEL DEPOSITED WITH NaCl AND NaHSO3 UNDER DRY/HUMID ALTERNATIVE CONDITION
YU Quancheng, WANG Zhenyao, WANG Chuan
State Key Laboratory for Corrosion and Protection, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016
Cite this article: 

YU Quancheng WANG Zhenyao WANG Chuan. CORROSION BEHAVIORS OF LOW ALLOY STEEL AND CARBON STEEL DEPOSITED WITH NaCl AND NaHSO3 UNDER DRY/HUMID ALTERNATIVE CONDITION. Acta Metall Sin, 2010, 46(9): 1133-1140.

Download:  PDF(1633KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  

The corrosion behaviors of low alloy steel P265GH and carbon steel Q235 deposited with NaCl and NaHSO3 under dry/humid alternative condition were investigated by FTIR, XRD, SEM and galvanostatic method. The results reveal that under present experimental condition, corrosion rates of low alloy steel and carbon steel decrease with prolonging time and their mass losses are almost identical. Besides, corrosion resistance of low alloy steel P265GH is not better than that of carbon steel Q235. The corrosion products formed on the two steels are mainly composed of δ-FeOOH, α-FeOOH, Fe3O4γ-FeOOH and sulphate, among which δ-FeOOH is predominant. The existence of δ-FeOOH accounts for the decrease of corrosion rates of the steels.

Key words:  low alloy steel      carbon steel      atmospheric corrosion      dry/humid alternative environment     
Received:  20 May 2010     
Fund: 

Supported by Science and Technology Plan Project of Shenyang (No.1091182-1-00)

URL: 

https://www.ams.org.cn/EN/10.3724/SP.J.1037.2010.00248     OR     https://www.ams.org.cn/EN/Y2010/V46/I9/1133

参考文献 [1] Singh D D N, Yadav S, Saha J K. Corros Sci, 2008; 50: 93 [2] Casta?o J G, Botero C A, Restrepo A H, Agudelo E A, Correa E, Echeverría F. Corros Sci, 2010; 52: 216 [3] Ma Y T, Ying Li, Wang F H. Corros Sci, 2009; 51: 997 [4] Qu Q, Yan C W, Zhang L, Yan Y G, Wan Y, Cao C N. The Chinese journal of Nonferrous Metals, 2002; 12: 1272 (曲庆, 严川伟, 张蕾, 阎一功, 万晔, 曹楚南. 中国有色金属学报, 2002; 12: 1272) [5] Qu Q, Yan C W, Cao C N. CORROSION SCIENC AND PROTECTION TECHNOLOGY, 2001; 13: 432 (曲庆, 严川伟, 曹楚南. 腐蚀科学与防护技术, 2001; 13: 432) [6] Ma Y T, Li Y, Wang F H. Materials Chemistry and Physics, 2008; 06: 066 [7] Qu Q, Yan C W, Bai W, Cao C N. ACTA METALLURGICA SINICA, 2001; 37: 72 (曲庆, 严川伟, 白玮, 曹楚南. 金属学报, 2001; 37: 72) [8] Qu Q, Yan C W, Zhang L, Wan Y, Cao C N. ACTA METALLURGICA SINICA, 2002; 38: 1062 (曲庆, 严川伟, 张蕾, 万晔, 曹楚南. 金属学报, 2002; 38: 1062) [9] Wang Z Y, Zheng Y P, Liu S R. JOURNAL OF CHINESE SOCIETY FOR CORROSION AND PROTECTION, 1994; 14: 240 (王振尧, 郑逸萍, 刘寿荣. 中国腐蚀与防护学报, 1994; 14: 240) [10] Wang Z Y, Yu G C, Han W. CORROSION SCIENCE AND PROTECTION TECHNOLOGY, 2004; 16: 70 (王振尧, 于国才, 韩薇. 腐蚀科学与防护技术, 2004; 16: 70) [11] Misawa T, Kyuno T, Su?taka W, Shimodaira S. Corros Sci, 1971; 11: 35 [12] Raman A, Kuban B, Razvan A. Corros Sci, 1991; 32: 1295 [13] Yamashita M, Konishi H, Kozakura T, Mizuki J, Uchida H. Corros Sci, 2005; 47: 2492 [14] Misawa T, Asami K, Hashimoto K, Shimodaira S. Corros Sci, 1974; 14: 279 [15] Nishimura T, Katayama H, Noda K, Kodama T. CORROSION, 2000; 56: 935 [16] Keiser J T, Brown C W. Corros Sci, 1983; 23: 251
[1] LI Xiaohan, CAO Gongwang, GUO Mingxiao, PENG Yunchao, MA Kaijun, WANG Zhenyao. Initial Corrosion Behavior of Carbon Steel Q235, Pipeline Steel L415, and Pressure Vessel Steel 16MnNi Under High Humidity and High Irradiation Coastal-Industrial Atmosphere in Zhanjiang[J]. 金属学报, 2023, 59(7): 884-892.
[2] LI Qian, LIU Kai, ZHAO Tianliang. Rust Formation Behavior and Mechanism of Q235 Carbon Steel in 5%NaCl Salt Spray Under Elastic Tensile Stress[J]. 金属学报, 2023, 59(6): 829-840.
[3] WANG Zhoutou, YUAN Qing, ZHANG Qingxiao, LIU Sheng, XU Guang. Microstructure and Mechanical Properties of a Cold Rolled Gradient Medium-Carbon Martensitic Steel[J]. 金属学报, 2023, 59(6): 821-828.
[4] SONG Jialiang, JIANG Zixue, YI Pan, CHEN Junhang, LI Zhaoliang, LUO Hong, DONG Chaofang, XIAO Kui. Corrosion Behavior and Product Evolution of Steel for High-Speed Railway Bogie G390NH in Simulated Marine and Industrial Atmospheric Environment[J]. 金属学报, 2023, 59(11): 1487-1498.
[5] PENG Zhiqiang, LIU Qian, GUO Dongwei, ZENG Zihang, CAO Jianghai, HOU Zibing. Independent Change Law of Mold Heat Transfer in Continuous Casting Based on Big Data Mining[J]. 金属学报, 2023, 59(10): 1389-1400.
[6] LIU Yuwei, GU Tianzhen, WANG Zhenyao, WANG Chuan, CAO Gongwang. Corrosion Behavior of Q235 and Q450NQR1 Exposed to Marine Atmospheric Environment in Nansha, China for 34 Months[J]. 金属学报, 2022, 58(12): 1623-1632.
[7] HUANG Songpeng, PENG Can, CAO Gongwang, WANG Zhenyao. Corrosion Behavior of Copper-Nickel Alloys Protected by BTA in Simulated Urban Atmosphere[J]. 金属学报, 2021, 57(3): 317-326.
[8] GUO Zhongao, PENG Zhiqiang, LIU Qian, HOU Zibing. Nonuniformity of Carbon Element Distribution of Large Area in High Carbon Steel Continuous Casting Billet[J]. 金属学报, 2021, 57(12): 1595-1606.
[9] LIU Yuwei, ZHAO Hongtao, WANG Zhenyao. Initial Corrosion Behavior of Carbon Steel and Weathering Steel in Nansha Marine Atmosphere[J]. 金属学报, 2020, 56(9): 1247-1254.
[10] SONG Xuexin, HUANG Songpeng, WANG Chuan, WANG Zhenyao. The Initial Corrosion Behavior of Carbon Steel Exposed to the Coastal-Industrial Atmosphere in Hongyanhe[J]. 金属学报, 2020, 56(10): 1355-1365.
[11] WANG Li,DONG Chaofang,ZHANG Dawei,SUN Xiaoguang,Chowwanonthapunya Thee,MAN Cheng,XIAO Kui,LI Xiaogang. Effect of Alloying Elements on Initial Corrosion Behavior of Aluminum Alloy in Bangkok, Thailand[J]. 金属学报, 2020, 56(1): 119-128.
[12] Qingdong ZHANG,Shuo LI,Boyang ZHANG,Lu XIE,Rui LI. Molecular Dynamics Modeling and Studying of Micro-Deformation Behavior in Metal Roll-Bonding Process[J]. 金属学报, 2019, 55(7): 919-927.
[13] Canshuai LIU,Zhaohui TIAN,Zhiming ZHANG,Jianqiu WANG,En-Hou HAN. Corrosion Behaivour of X65 Low Carbon Steel During Redox State Transition Process of High LevelNuclear Waste Disposal[J]. 金属学报, 2019, 55(7): 849-858.
[14] Xingchen CHEN, Jie WANG, Deren CHEN, Shuncong ZHONG, Xiangfeng WANG. Effect of Na on Early Atmospheric Corrosion of Al[J]. 金属学报, 2019, 55(4): 529-536.
[15] Zibing HOU, Rui XU, Yi CHANG, Jianghai CAO, Guanghua WEN, Ping TANG. Time-Series Fluctuation Characteristics of Segregation Carbon Element Distribution Along Casting Direction in High Carbon Continuous Casting Billet[J]. 金属学报, 2018, 54(6): 851-858.
No Suggested Reading articles found!