3-D MORPHOLOGY OBSERVATION OF DEGENERATE FERRITE IN STEEL Fe-0.28C-3.0Mo USING SERIAL SECTIONING AND COMPUTER-AIDED RECONSTRUCTION
WU Kaiming
Department of Applied Physics; The Hubei Province Key Laboratory of Refractories and Ceramics---Ministry-Province Jointly-Constructed Cultivation Base for State Key Laboratory; Wuhan University of Science and Technology; Wuhan 430081
Cite this article:
WU Kaiming. 3-D MORPHOLOGY OBSERVATION OF DEGENERATE FERRITE IN STEEL Fe-0.28C-3.0Mo USING SERIAL SECTIONING AND COMPUTER-AIDED RECONSTRUCTION. Acta Metall Sin, 2005, 41(12): 1237-1242 .
Abstract 3-D morphology of the degenerate ferrite formed below the
bay of the TTT diagram in an Fe-0.28C-3.0Mo (mass fraction, %) steel
has been revealed by utilizing serial sectioning in conjunction with
computer-aided reconstruction and visualization. The degenerate ferrite
is initially formed at prior austenite boundary and then grows toward
grain interior rather than along the grain boundary. The degenerate
ferrite consists of rod-like subunits, each several micron in length
and 1-2 μm in diameter. The peculiar morphology of ferrite may be
attributed to the repeated nucleation, growth and coalescence of the
adjacent ferrite crystals.
[1] Kinsman K R, Aaronson H I. In: Transformation and Hardenability in Steels. Ann Arbor, MI: Climax Molybdenum Co., 1967: 39 [2] Tsubakino H, Aaronson H I. Metall Trans, 1987; 18A: 2047 [3] Shiflet G J, Aaronson H I. Metall Trans, 1990; 21A: 1413 [4] Reynolds W T Jr, Li F Z, Shui C K, Aaronson H I. Metall Trans, 1990; 21A: 1433 [5] Glodenstein H, Aaronson H I. Uetall Trans, 1990; 21A: 1465 [6] Liu S K, Yang L, Zhu D G, Zhang J. Metall Mater Trans, 1994; 25A: 1991 [7] Kral M V, Spanos G. Acta Mater, 1999; 47: 711 [8] Kral M V, Mangan M A, Spanos G, Rosenberg R O. Mater Charact, 2000; 45: 17 [9] Mangan M A, Lauren P D, Shiflet G J. J Microsc, 1997; 188: 36 [10] Wolfsdorf T L, Bender W H, Voorhees P W. Acta Mater, 1997; 45: 2279 [11] Wu K M, Kagayama M, Enomoto M. Mater Sci Eng, 2003; A343: 143 [12] Wu K M, Yokomizo T, Enomoto M. ISIJ Int, 2002; 42: 1144 [13] Wu K M, Enomoto M, Marukami T, Nanba S. Mater Charact, 2004; 52: 121 [14] Oblak J M,Hehemann R F. In: Transformation and Hard-enability in Steels. Ann Arbor, MI: Climax Molybdenum Co., 1967: 15 [15] Aaronson H I, Spanos G, Masamura R A, Vardiman R G, Moon D W, Menon E S K. Mater Sci Eng, 1995; B32: 10 [16] Spanos G, Aaronson H I. Scr Metall, 1988; 22: 37}