Abstract Theα-Cr precipitation behavior and its effects on the different Cr-containing superalloys, such as GH169, GH625, GH648 and two high-Cr tested alloys, were investigated by microstructure analysis approach in order to compare their behavior and optimize theα-Cr phase morphology. The results show that noα-Cr phase was observed after a standard heat treatment but with long-term aging theα-Cr phase precipitates and grows usually clinging to δ phase in GH169 alloy and clinging to M6C carbide andδphase in GH625 alloy. However, for high Cr-containing alloys (Cr>30%, GH648 and two tested alloys), the α-Cr phase with various morphologies precipitates directly from austenitic matrix and from short-plate to long acicular and lamellar shape. Furthermore, the optimization of α-Cr phase was initially studied by a special heat treatment in order to obtain fine and uniform α-Cr particles.
[1] Radavich J F. Proc Superalloys 718, 6SS and Various Derivative, Pennsylvania, USA: TMS, 1997: 409 [2] Jiang X C, Yoshimura T. J Electrochem Soc, 1992; 139: 1001 [3] Ustinovshikov Y. Acta Mater, 1996; 44: 5021 [4] Wu C W, Dong J X, Zhang M C, Wang G L, Xie X S. Acta Metall Sin, 2001; 37: 1174 (吴翠微,董建新,张麦仓,王改莲,谢锡善.金属学报,2001; 37:1174) [5] Xie X S, Dong J X, Zhang M C, Wang G L. Proc Adv Mater Process Gas Turbines, USA: TMS, 2003: 134 [6] Xie X S, Dong J X, Smith G D, Patel S, Radavich J F. Proc Long Term Stability High Temp Mater, USA: TMS, 1999: 135 [7] Wang G L, Wu C W, Zhang M C, Dong J X, Xie X S. Mater Sci Eng, 2003; A358: 71 [8] Dong J X, Zhang M C, Zeng Y P, Xie X S. Acta. Metall Sin (Engl Lett), 2005; 18: 164 [9] Radavich J. Proc Superalloy 718, 625, 706 and Various Derivatives, USA: TMS, 1996: 409 [10] Dong J X, Zhang M C, Zeng Y P, Xie X S. J Univ Sci Technol Beijing, 2002; 24: 186 (董建新,张麦仓,曾燕屏.谢锡善.北京科技大学学报,2002; 24:186) [11] Shen G, Radavich J, Xie X, Lingdsley B. Proc Superalloy 2000, USA: TMS, 2001: 445 [12] Wang G L, Wu C W, Zhang M C, Dong J X, Xie X S. Rare Met Mater Eng, 2002; 31: 37 (王改莲,吴翠微,张麦仓,董建新,谢锡善.稀有金属材料与 工程,2002;31:37) [13] Lindsley B, Pierron X, Maurer G. Proc Long Time Stability High Temp Mater, USA: TMS, 1999: 123 [14] Shen G., Radavich J, Xie X, Lindsley B. Proc Superalloy 2000, USA: TMS, 2001: 445 [15] Gale W F, Abdo Z A M, Nemani R V. J Mater Sci, 1999; 34: 407 [16] Ustinovshikov Y. Acta Mater, 1996; 44: 5021 [17] Marucco A. Mater Sci Eng, 1995; A194: 225.