| Neutron Irradiation--Induced Phosphorus Segregation in Reactor Pressure Vessel Steels |
| Z. Lu; R. G. Faulkner; P. E. J. Flewitt |
| PTME; Loughborough University; Loughborough; Leicestershire; LE11 3TU; UK |
|
Cite this article:
Z. Lu; R. G. Faulkner; P. E. J. Flewitt. Neutron Irradiation--Induced Phosphorus Segregation in Reactor Pressure Vessel Steels. Acta Metall Sin, 2005, 41(1): 79-.
|
|
|
Abstract Neutron irradiation--induced phosphorus intergranular
segregation in the reactor pressure vessel steels is
the one of main reasons resulting in brittle fracture of the nuclear
reactor vessel. In this paper, a solute drag model was proposed to
predict the phosphorus inter granular segregation in
reactor pressure vessel steels and compared with the rate
theory model. The predicted results show a good agreement with
experimental data recently
published for pressure vessel steels (C-Mn and MnMoNi steels).
|
|
Received: 25 February 2004
|
|
|
[1] Faulkner R G, Song S H, Flewitt P E J, Victoria M,Marmy P. J Nucl Mater, 1998; 255: 189 [2] Druce S G, English C A, Foreman A J E, McElroy R J, Vatter I A, Bolton C J, Buswell J T, Jones R B. ASTM STP 1270, 1996: 119 [3] McLean D. Grain Boundaries in Metals. Oxford: OxfordUniversity Press, 1957: 131 [4] Perez F J, Smith, R. Nucl Instr Meth, 1999; 136B: 153 [5] Bischler P J E, Wild R K. ASTM STP 1270, 1996: 260 [6] Williams T J, Ellis D. ASTM STP 1405, 2001: 8 [7] Meade D. PhD Thesis, Loughborough: LoughboroughUniversity, 1999 [8] English C A, Ortner S R, Gage G, Server W L, RosinskiS T. ASTM STP 1405, 2001: 151 [9] Williams T J. Rolls Royce Naval Marine. Private communication, 2001 [10] Faulkner R G, Song S, Goodwin C C, Flewitt P E J. Defect Diffus Forum, 1999; 29: 165 [11] Jones R B. Proceedings of EPRI Discussion Meeting,USA: Squaw Valley, 2001: 66 [12] Little E A. J Nucl Mater, 1979; 11: 87 [13] Takeyama T, Takahashi H, Ohnuki S. Bull Fac EngHokkaido Univ, 1984; 85: 121 [14] Honeycombe R W K. Steels, Microstructure and Properties. London: Edward Arnold Ltd, 1981: 5L |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|