| Temperature Memory Effect of Partial Transformation in TiNi Alloys |
| ZHENG Yanjun; CUI Lishan |
| Department of Materials Science and Engineering; University of Petroleum; Beijing 102249 |
|
Cite this article:
ZHENG Yanjun; CUI Lishan. Temperature Memory Effect of Partial Transformation in TiNi Alloys. Acta Metall Sin, 2004, 40(9): 915-919 .
|
|
|
Abstract Temperature memory effect of a prestrained TiNi alloy under constraint condition was studied by
differential scanning calorimetry (DSC). Results showed that the transformation temperature range of the
TiNi alloy can be significantly enlarged upon prestraining and constrained heating, which makes the
temperature memory effect operational also in an enlarged temperature window. Furthermore, the
temperature memory effect of the prestrained and constrained TiNi alloy is more accurate than that of a
TiNi alloy in free conditions. The dislocations at the interface between the parent phase and the remaining
martensite, and the self--accommodating process near the interface are thought to be the mechanism for the
temperature memory effect.
|
|
Received: 31 July 2003
|
|
|
[1] Wei Z G, Sandstrom R. J Mater Sci, 1998; 33: 3743 [2] Wei Z G, Sandstrom R, Miyazaki S. J Mater Sci, 1998;33: 3763 [3] Madangopal K, Banerjee S, Lele S. Acta Metall Mater,1994; 42: 1875 [4] Airoldi G, Riva G. Key Eng Mater, 1990; 48: 5 [5] Airoldi G, Corsi A, Riva R. Mater Sci Eng, 1998; A241:233 [6] Amengual A. Scr Metall Mater, 1992; 26: 1795 [7] Piao M, Otsuka K, Miyazaki S, Horikawa H. Mater TransJIM, 1993; 34: 919 [8] Lin H C, Wu S K, Chou T S, Kao H P. Acta Metall Mater,1991; 39: 2069 [9] Liu Y N, Favier D. Acta Mater, 2000; 48: 3489 [10] Zheng Y J, Cui L S, Zhang F, Yang D Z. J Mater SciTechnol, 2000; 16: 611 [11] Zheng Y J, Cui L S, Zhu D, Yang D Z. Mater Lett, 2000,43(3) : 91 [12] Zheng Y J, Schrooten J, Tsoi K A, Sittner P. Exp Mech,2003; 43: 194 [13] Zheng Y J, Schrooten J, Tsoi K A, Stalmans R. Mater SciEng, 2002; A335: 157 [14] Tong H C, Wayman C M. Acta Metall, 1974; 22: 887 [15] Olson G B, Cohen M. Acta Metall, 1979; 27: 1907 [16] Raghavan V, Cohen M. Acta Metall, 1972; 20: 779 [17] Tadaki T, Kakeshita T, Shimizu K. In: Delaey L, Chan-drasekaran M, eds., Int Conf on Martensitic Transforma-tions(ICOMAT'82) , Heverlee, Belgium: KULeuven, 1982: 191E |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|