MEASUREMENTS OF HYDROGEN DIFFUSION COEFFICIENT FOR TUBE SAMPLES AT MEDIUM AND HIGH TEMPERATURES |
LIU Shi; ZHENG Hua; GUI Quanhong; MA Aihua; YU Hongbo; WANG Longbao |
Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110016 |
|
Cite this article:
LIU Shi; ZHENG Hua; GUI Quanhong; MA Aihua; YU Hongbo; WANG Longbao. MEASUREMENTS OF HYDROGEN DIFFUSION COEFFICIENT FOR TUBE SAMPLES AT MEDIUM AND HIGH TEMPERATURES. Acta Metall Sin, 2004, 40(4): 393-398 .
|
Abstract By using a specially designed device and gas permeation method, the hydrogen diffusion coefficients for the tube--shape samples
of Cr18Ni10Ti austenite steel were measured. The testing temperature covers the range of 360---600℃. The curves of hydrogen permeation
flux and the relation of hydrogen diffusion coefficients and specific time were simulated by finite difference method (FDM). According to the simulated curves the experiment data related to the hydrogen diffusion
coefficients can be treated. The hydrogen diffusion coefficients for
aluminum film inner coated tubes at room temperature is 5.789X10 -20 m2/s, its activation energy of hydrogen
diffusion is 8.144X10 -20 J/mol, which are 5---6 orders lower and 1 times higher than those of uncoated tubes respectively.
|
Received: 28 March 2003
|
|
[1] Masui K, Yoshida H, Watanabe R. Trans ISIJ, 1979; 19: 547 [2] Tanabe T, Yamanishi Y, Imoto S. Mater Trans JIM, 1984;25: 1 [3] Devannathan M A V, Stanchurdki Z. Proc Royal Soc,1962; A2TO: 90 [4] Kalin B A, Yakushin V L, Fomina E P. Fusion Eng &Dev, 1998; 41: 119 [5] Hollenberg G W, Simonen E P, Terlain A. Fusion Eng &Des, 1995; 28: 190 [6] Wu E. J Electrochem Soc, 1987; 134: 2126 [7] McBreen J, Nanis L, Beck W. Ibid, 1966; 113: 1218 [8] Harhai J, Viswanathan T, Davis H. Trans Am Soc Met,1965; 58: 210 [9] Peixuan W, Jiashu S. Helium in Materials and the Permeation of Tritium. Beijing: National Defence IndustryPress, 2002: 69(王佩璇,宋家树.材料中的氦及氚渗透.北京:国防工业出版社,2002:69) |