Please wait a minute...
Acta Metall Sin  2004, Vol. 40 Issue (2): 191-196     DOI:
Research Articles Current Issue | Archive | Adv Search |
Corrosion Behavior of AZ91D Magnesium Alloy in City Atmosphere
LIN Cui; LI Xiaogang; LI Ming; WANG Fengping
Corrosion and Protection Center; Key Laboratory for Corrosion; Erosion and Surface Technology of Beijing; University of Science and Technology Beijing; Beijing 100083
Cite this article: 

LIN Cui; LI Xiaogang; LI Ming; WANG Fengping. Corrosion Behavior of AZ91D Magnesium Alloy in City Atmosphere. Acta Metall Sin, 2004, 40(2): 191-196 .

Download:  PDF(600KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The surface morphology of corrosion layer, corrosion products and structure of rust layer for AZ91D magnesium alloy in natural city atmosphere were studied by SEM and XRD. The results show that Mg(OH)2 layer forms at the initial corrosion period, then film thickens and cracks appear with continued corrosion under cyclic wet/dry conditions, in the end these cracks develop to reticulate structure. The water vapour is easily condensed and the corrosives gases, salt particles are easily absorbed in the cracks. Meanwhile, the cracks provide the diffusion paths for oxygen and other corrosion pollutants into matrix, which results in severe local corrosion. The major corrosion products are Mg(OH)2, Al(OH)3, Mg2CO3(OH)2•3H2O and Mg2(OH)3Cl•4H2O, which plays a partial role in protecting the matrix, therefore slowing down the average corrosion rate of magnesium alloy in the latter periods.
Key words:  city atmosphere      magnesium alloy      corrosion behavior      
Received:  22 February 2003     
ZTFLH:  TG172.3  

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2004/V40/I2/191

[1] Zhai C Q, Zeng X Q, Ding W J, Wang Q D, L Y Z, Xu X P. Mater Mech Eng, 2001; 25: 6(翟春泉,曾小勤,丁文江,王渠东,吕宜振,徐小平.机械工程材料,2001;25:6)
[2] Zeng X Q, Wang Q D, L Y Z, Ding W J, Zhu Y P. Foundry, 1998; (11) : 39(曾小勤,王渠东,吕宜振,丁文江,朱燕萍.铸造,1998;(11) :39)
[3] Wu Z N, Li P J, Liu S X, Zeng D B. Foundry, 2001; 50: 583(吴振宁,李培杰,刘树勋,曾大本.铸造,2001;50:583)
[4] Xu Y, Chen X, L Z S, Zhou D R, Zhao L C. J Harbin Inst Technol, 2001; 33: 753(许越,陈湘,吕祖舜,周德瑞,赵连城,哈尔滨工业大学学报,2001;33:753)
[5] Ambat R, Aung N N, Zhou W. Corros Sci, 2000; 42: 1433
[6] Gutman E M, Eliezer A, Unigovski Y, Abramov E. Mater Sci Eng, 2001; A302: 63
[7] Lunder O, Lein J E, Aune T Kr, Nisancioglu K. Corrosion, 1989; 45: 741
[8] Baril G, Pebere N. Corros Sci, 2001; 43: 471L
[1] SHAO Xiaohong, PENG Zhenzhen, JIN Qianqian, MA Xiuliang. Unravelling the {101¯2} Twin Intersection Between LPSO Structure/SFs in Magnesium Alloy[J]. 金属学报, 2023, 59(4): 556-566.
[2] ZHU Yunpeng, QIN Jiayu, WANG Jinhui, MA Hongbin, JIN Peipeng, LI Peijie. Microstructure and Properties of AZ61 Ultra-Fine Grained Magnesium Alloy Prepared by Mechanical Milling and Powder Metallurgy Processing[J]. 金属学报, 2023, 59(2): 257-266.
[3] TANG Weineng, MO Ning, HOU Juan. Research Progress of Additively Manufactured Magnesium Alloys: A Review[J]. 金属学报, 2023, 59(2): 205-225.
[4] SONG Jialiang, JIANG Zixue, YI Pan, CHEN Junhang, LI Zhaoliang, LUO Hong, DONG Chaofang, XIAO Kui. Corrosion Behavior and Product Evolution of Steel for High-Speed Railway Bogie G390NH in Simulated Marine and Industrial Atmospheric Environment[J]. 金属学报, 2023, 59(11): 1487-1498.
[5] CHEN Yang, MAO Pingli, LIU Zheng, WANG Zhi, CAO Gengsheng. Detwinning Behaviors and Dynamic Mechanical Properties of Precompressed AZ31 Magnesium Alloy Subjected to High Strain Rates Impact[J]. 金属学报, 2022, 58(5): 660-672.
[6] ZENG Xiaoqin, WANG Jie, YING Tao, DING Wenjiang. Recent Progress on Thermal Conductivity of Magnesium and Its Alloys[J]. 金属学报, 2022, 58(4): 400-411.
[7] LI Shaojie, JIN Jianfeng, SONG Yuhao, WANG Mingtao, TANG Shuai, ZONG Yaping, QIN Gaowu. Multimodal Microstructure of Mg-Gd-Y Alloy Through an Integrated Simulation of “Process-Structure-Property”[J]. 金属学报, 2022, 58(1): 114-128.
[8] WANG Huiyuan, XIA Nan, BU Ruyu, WANG Cheng, ZHA Min, YANG Zhizheng. Current Research and Future Prospect on Low-Alloyed High-Performance Wrought Magnesium Alloys[J]. 金属学报, 2021, 57(11): 1429-1437.
[9] PAN Fusheng, JIANG Bin. Development and Application of Plastic Processing Technologies of Magnesium Alloys[J]. 金属学报, 2021, 57(11): 1362-1379.
[10] WANG Xuemei, YIN Zhengzheng, YU Xiaotong, ZOU Yuhong, ZENG Rongchang. Comparison of Corrosion Resistance of Phenylalanine, Methionine, and Asparagine-Induced Ca-P Coatings on AZ31 Magnesium Alloys[J]. 金属学报, 2021, 57(10): 1258-1271.
[11] ZHANG Yang, SHAO Jianbo, CHEN Tao, LIU Chuming, CHEN Zhiyong. Deformation Mechanism and Dynamic Recrystallization of Mg-5.6Gd-0.8Zn Alloy During Multi-Directional Forging[J]. 金属学报, 2020, 56(5): 723-735.
[12] ZHAO Yanchun, MAO Xuejing, LI Wensheng, SUN Hao, LI Chunling, ZHAO Pengbiao, KOU Shengzhong, Liaw Peter K.. Microstructure and Corrosion Behavior of Fe-15Mn-5Si-14Cr-0.2C Amorphous Steel[J]. 金属学报, 2020, 56(5): 715-722.
[13] CHEN Fang,LI Yadong,YANG Jian,TANG Xiao,LI Yan. Corrosion Behavior of X80 Steel Welded Joint in Simulated Natural Gas Condensate Solutions[J]. 金属学报, 2020, 56(2): 137-147.
[14] Xin LI,Yuecheng DONG,Zhenhua DAN,Hui CHANG,Zhigang FANG,Yanhua GUO. Corrosion Behavior of Ultrafine Grained Pure Ti Processed by Equal Channel Angular Pressing[J]. 金属学报, 2019, 55(8): 967-975.
[15] BAI Yang, WANG Zhenhua, LI Xiangbo, LI Yan. Corrosion Behavior of Al(Y)-30%Al2O3 Coating Fabricated by Low Pressure Cold Spray Technology[J]. 金属学报, 2019, 55(10): 1338-1348.
No Suggested Reading articles found!