| HAZ Corrosion of 22SiMn2TiB Ultra-Strength Steel Weldment in 3.5%NaCl Solution |
| TAN Wei(TAN Way); XU Binshi; HAN Wenzheng; FENG Shaowu; FENG Jianlin; ZHONG Qunpeng |
| School of Materials Science and Engineering; Beijing University of Aeronautics & Astronautics; Beijing 100083 |
|
Cite this article:
TAN WeiTAN Way; XU Binshi; HAN Wenzheng; FENG Shaowu; FENG Jianlin; ZHONG Qunpeng. HAZ Corrosion of 22SiMn2TiB Ultra-Strength Steel Weldment in 3.5%NaCl Solution. Acta Metall Sin, 2004, 40(2): 197-201 .
|
|
|
Abstract Weld heat affected zone (HAZ) microstructures of 22SiMn2TiB
ultra-strength steel were thermally simulated by means of
Gleeble-1500 machine. Polarization measurement of the quenched
zone and tempered zone in 3.5%NaCl solution was conducted
respectively with potentionstat/galvanostat Solaron SL1280B.
The relation between the microstructure and the HAZ corrosion
resistance in 3.5%NaCl solution was established. Carbon and
boron diffusions, segregation and iron carbide or boride
precipitation are dependent on simulated weld thermal cycle peak
temperature θmax and continuous cooling time t8/5,
and induce the microstructure transformation. The polarization
curves and corrosion potentials of the simulated HAZ with different
microstructures in 3.5%NaCl aqueous solution are slightly different;
the limit diffusion current of dissolved oxygen in 3.5%NaCl
solution decides corrosion current. Weld bond, which undergoes anodic
dissolution in couple corroding, needs to be protected carefully.
|
|
Received: 15 April 2003
|
|
|
[1] Huang H H, Tsai W T, Lee J T. Corros Sci, 1994; 36: 1027 [2] Zhao W M, Yu R R, Wang Y, Duan L X. J Univ Petroleum Chin, 1997; 21(5) : 61(赵卫民,俞蓉蓉,王勇,董立先.石油大学学报,1997;21(5) :61) [3] Sigeru E, Sakae F, Moriyasu N, Osamu H. Oil Gas J, 1997; 3: 92 [4] Shanghai Iron and Steel Research Institute. Corrosion Study on Ocean Steel. Shanghai: Shanghai Science and Technology Press, 1978: 29(上海钢铁研究所.海洋用钢腐蚀研究.上海:上海科学技术出版社,1978:29) [5] Tretheweg K R, Chamberlain J. Corrosion. New York: John Wiley & Sons, 1988: 274 [6] Stern M. J Electrochem Soc, 1955; 102: 663 [7] Williams E, Komp M. Corrosion, 1965; 21: 9 [8] Majid T M, Sultan S A R, Mahdi S D, Jasim S. Corrosion, 1990; 46: 37 [9] Huang L M, Xu Z X, Duan S Z. Internal Report, 1995: 1(黄丽明,徐占先,段世铮.内部资料,1995:1) [10] Porter D A, Esterling K E. Phase Transformations in Metals and Alloys. London: Chapman & Hall, 1992: 420 [11] China Corrosion Science and Prevention Society. Metal Corrosion Handbook. Shanghai: Shanghai Science and Technology Press, 1987: 71(中国腐蚀与防护学会.金属腐蚀手册.上海:上海科学技术出版社,1987:71) [12] Tan W, Han W Z, Xu B S, Chen C, Zhang Y H. Trans Chin Weld Inst, 2003; 24(3) : 39(谭伟,韩文政,徐滨士,陈超,张彦华.焊接学报,2003;24(3) :39)1 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|