| STUDY ON THE SIMULATION OF SOLIDIFICATION STRUCTURE |
| JIN Junze; WANG Zongting; ZHENG Xianshu; YAO Shan (Engineering Research Center of Foundry; Dalian University of Technology; Dalian 116024)Correspondent: JIN Junze; professor; Tel & Fax: (0411)4709443(H);E-mail: jinjunze@gingko. dlut. edu. cn |
|
Cite this article:
JIN Junze; WANG Zongting; ZHENG Xianshu; YAO Shan (Engineering Research Center of Foundry; Dalian University of Technology; Dalian 116024)Correspondent: JIN Junze; professor; Tel & Fax: (0411)4709443(H);E-mail: jinjunze@gingko. dlut. edu. cn. STUDY ON THE SIMULATION OF SOLIDIFICATION STRUCTURE. Acta Metall Sin, 1998, 34(9): 928-932.
|
|
|
Abstract The Monte Carlo simulation method for crystal growth is explored by including the macroscopic temperature, solute redistribution within the liquid phase and the thermodynamics in metal solidification process. A model coupling macro and micro is created to describe solidification structure formation in solidification process. The Al-4.5%Cu (mass fraction) alloy is used in the simulation. Finally, the simulation results are compared to experimental results. It shows that this simulation method is feasible.
|
|
Received: 18 September 1998
|
1 Spittle JA,Brown S G. R .Acta Metall,1989;37:1803 2 Brown S G R; SPittle J A. Mater Sci Technol; 1989; 5: 362 3 Spittle J A, Brown S G R. J Mater Sci, 1989; 23: 1777 4 Srolovitz D J, Anderson M P, Sahni P S, Gerst G S. Acta Metall, 1984 32: 793 5 Sholovitz D J, Anderson M P, Grest G S, Sahni P S. Acta Metall, 1984; 32: 1429 6 Zhu Panping, Smith R W. Acta Metall; 1992; 40: 683 7 Zhu Panping, Smith R W. Acta Metall. 1992 40:3369 8 Ozisik M N著,俞昌铭译.热传导北京:高等教育出版社, 1983: 531(Ozisik M N. Heat Conduction. Translation by Yu Changming Beijing: HighEducation Press, 1983:531) 9 Rappaz M, Gandin Ch—A Acta Metall, 1993; 41: 345 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|