| STUDY ON THE CHEMICAL REACTIONS IN SITU PROCESSING α-Al_2O_3 PARTICLE REINFORCED Al-Cu ALLOY MATRIX COMPOSITES |
| CHEN Gang; ZHU Zhengang (Laboratory of Internal Friction and Defects in Solids; Institute of Solid State Physics; The Chinese Academy of Sciences; Hefei 230031)SUN Guoxiong (Department of Mechanical Engineering; Southeast University; Nanjing 210018) |
|
Cite this article:
CHEN Gang; ZHU Zhengang (Laboratory of Internal Friction and Defects in Solids; Institute of Solid State Physics; The Chinese Academy of Sciences; Hefei 230031)SUN Guoxiong (Department of Mechanical Engineering; Southeast University; Nanjing 210018). STUDY ON THE CHEMICAL REACTIONS IN SITU PROCESSING α-Al_2O_3 PARTICLE REINFORCED Al-Cu ALLOY MATRIX COMPOSITES. Acta Metall Sin, 1998, 34(5): 531-537.
|
|
|
Abstract X-ray diffractometer and scanning electron microscope were applied to examine the specimens processed from CuO/Al powder compacts under different conditions. The influence of temperature and environment medium on the chemical reactions in CuO/Al system is studied,and it is proposed that α-Al2O3 particle reinforced Al-Cu alloy matrix composites can be processed by introducing the chemical reactions in CuO/Al system.
|
|
Received: 18 May 1998
|
1Lewis C F. Mate, Eng, 1986; 103(5): 33 2Lloyd D J. Int Mater, Rev, 1994; 39(1): 1 3Koczak M J,Premkumar M K.JOM ,1993;45(1):44 4Chu M G, Premkumar M K. Metall Trans, 1993; 24A: 2803 5Khatri S, Koczak M. Mater Sci Eng, 1993; A162: 153 6Mitra R, Chiou W A, Weertman J R, Fine M E, Aikin R M. Scr Metall Mater, 1991; 25: 2689 7Westwood A R C. Metall Trans, 1988; 19A: 749 8小桥真,长隆郎.轻金属,1992;42:138(Kobasi Makoto, Choh Tokao. Light Met, 1992; 42: 138) 9林传仙,白正华,张哲儒.矿物及有关化合物的热力学数据手册.北京:科学出版社,1985:97(Lin Chuanxian,Bai Zhenghua ,Zhang Zheru.Handbook of the Thermodynamic Data for Minerals and the Corresponding Compound.Beijing:Science Press,1985:97) 10章燕豪.物理化学.上海:上海交通大学出版社,1988:77(Zhang Yanhao Physical Chemistry.Shanghai:Shamghai Jiaotong University Press,1988:77) |