| STRUCTURAL CHARACTERIZATION OF THE Y_3(Fe, Mo)_(29) INTERMETALLIC COMPOUND |
| PAN Hongge; DU Honglin; CHEN Changpin; HAN Xiufeng; YANG Fuming (Department of Materials Science and Engineering; Zhejiang University; Hangzhou 310027)(State Key Laboratory for Magnetism; Institute of Physics; The Chinese Academy of Sciences; Beijing 100080)(Institute of Chinese Atomic Energy; Beijing 102413) |
|
Cite this article:
PAN Hongge; DU Honglin; CHEN Changpin; HAN Xiufeng; YANG Fuming (Department of Materials Science and Engineering; Zhejiang University; Hangzhou 310027)(State Key Laboratory for Magnetism; Institute of Physics; The Chinese Academy of Sciences; Beijing 100080)(Institute of Chinese Atomic Energy; Beijing 102413). STRUCTURAL CHARACTERIZATION OF THE Y_3(Fe, Mo)_(29) INTERMETALLIC COMPOUND. Acta Metall Sin, 1998, 34(5): 473-482.
|
|
|
Abstract The X-ray diffraction and neutron diffraction patterns of Y3(Fe, Mo)29 compound have been analysed by Rietveld method. The structural relationship of the 3:29 phase with 2:17 and 1:12 phases has been studied by coordinate transformation. The results show that the 3:29 compound belongs to A2/m space group and the 3:29 compound is a kind of mixed structure of 2:17 and 1:12 structures.
|
|
Received: 18 May 1998
|
1 Collocott S J, Day R K; Dunlop J B, Davis R L Camberra, 1992: 7: 137 2 Saito H, Takahashi M, Wakiyama T J Appl Phys. 1988 64: 5965 3 Katter M, Weeker J, Schultz L J Appl Phys, 1991; 70: 3188 4 Cadogan J M, Li H S, Davis R L, Margarian A, Dunlop J B, Gwan P B J Appl Phys, 1994 75: 7120 5 Ivanova G V, Shcherbakova Y V, Belozerov Y V, Yermolenko A S, Teytel Y I Phys Met Metallogr, 1990; 70:63 6 Fuerst C D, Pinkerton; Herbst J F J Magn Magn Mater, 1994; 129: L115 7 Hu Z, Yelon W B Sokid State Commun,1994; 91(3): 223 8 Kalogirou O, Psycharis V Saettas L, Niarchos D J Magn Magn Mater. 1995; 146: 235 9 Margarian A, Dunolp J B, Collocatt S J, Li H S, Cadogan J M, Davis R L to be published 10 Pan H G, Yang G M, Chen C P, Han X F; Tang N; Wang Q D J Magn Magn Mater, 1996: 163: 221 11 Young R A, Makile P E, von Dreele P B J Appl Cryst; 1977: 10: 262 12 梁敬魁.相图与相结构(下册)北京:科学出版社,1993:769 (Liang Jingkui. Phase Diagram and Phase Structre Beijing: Science Press. 1993: 769) 13 Cadogen J M, Li H S, Margarian A, Dunlop J B. Ryan D H, Collocott S J Davis S L J Appl Phus,1994 76:6138 14 Hu B P.Intrinsic Magnetic Properties of the ThMn12 structure Compounds RE(Fe11 Ti) (RE=Rare Earth),PhD Dissertation, Dublin University, 1990 |