| TWINS AND ITS FORMATION MECHANISM IN LOWER META-BAINITE |
| LUAN Daocheng; WEI Chengfu;YANG Ge (Department of Materials Science and Engineering; Sichuan Institute of Technology; Chengdu 611744) |
|
Cite this article:
LUAN Daocheng; WEI Chengfu;YANG Ge (Department of Materials Science and Engineering; Sichuan Institute of Technology; Chengdu 611744). TWINS AND ITS FORMATION MECHANISM IN LOWER META-BAINITE. Acta Metall Sin, 1998, 34(1): 24-30.
|
|
|
Abstract By TEM it has been confirmed that twin substructures exist in lower metabainite in silicon-containing steel. A large number of twins was found in bainitic midribs for first time. Twins in midribs (M-M) as well as retained austenite (Ar) are deformation twins formed by coordinating uniform shear deformation as bainitic ferrite lath grows, twins in bainitic ferrite (BF)mainly are those inherited in retained austenite as BF thickens by shear mechanism in broad face. and twin planes correspond to the interface ledges, which shows ledges can not migrate along side direction of broad face. Based on the results, a model of twin formation in lower meta-bainite was suggested.
|
|
Received: 18 January 1998
|
1 Sandvik B P J, Metall Trans, 1982 13A: 777 2 Kang M K,Sun J L,Yang Q M.Metall Trzns,1990; 21A: 853 3 Huang D H,Thomas G Metall Trans,1977;8A:1661 4 张喜燕,康沫狂,陈大明,武小雷.金属学报,1994;30:A109(Zhang Xiyan.Kang Mokuang,Chen Daming,Wu Xiaolei.Acta Metall Sin,1994:30:A109) 5 康沫狂,杨延清,张喜燕.孙加林,贾虎生,武小雷金属学报,1996;32:A897(Kang Mokuang, Yang Yanqing; Zhang Xlvan, Sun Jialin; Jia Husheng,Wu Xiaolei. Acta Metall Sin,1996, 22:897) 6 Okamoto H, Oka M,Metall Trans, 1986;17A:1113 7 杨立波,刘文西,陈玉如,龚方岳,陈金铭钢铁,1989;24(9):43(Yang Libo;Liu Wenxi,Chen Yuru,Gong Fangyue,Chen Jinming.Iron Steel, 1989; 24(9): 43) 8 孙加林,康沫狂。西北工业大学学报, 1990;(SuPPl): 73(Sun Jialin,Kang Mokuang.J Northwestern Poly Uni,1990;(Suppl):73) 9 栾道成,魏成富,杨哿.钢铁研究学报,1996;8(6):24(Luan Daocheng, Wei Chengfu; Yang Ge.J Iron Steel Res,1996 8(6): 24) 10 Sandvik B P J,Wayman C M Metall Trans,1983 14A: 823 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|