TEM INVESTIGATION ON MICROSTRUCTURES OF EUTECTOID CEMENTITE IN HIGH CARBON LOW ALLOY STEELS
ZHU Xiaodong;LI Chengji; ZHANG Shouhua (Department of Materials Science and Engineering; USTB; Beijing 100083)ZOU Ming; SU Shihuai (Panzhihua Iron and Steel [Group] Company; Panzhihua 617067)
Cite this article:
ZHU Xiaodong;LI Chengji; ZHANG Shouhua (Department of Materials Science and Engineering; USTB; Beijing 100083)ZOU Ming; SU Shihuai (Panzhihua Iron and Steel [Group] Company; Panzhihua 617067). TEM INVESTIGATION ON MICROSTRUCTURES OF EUTECTOID CEMENTITE IN HIGH CARBON LOW ALLOY STEELS. Acta Metall Sin, 1998, 34(1): 31-38.
Abstract The eutectoid cementite in several rail steels has been studied by means of TEM.It was found that the eutectoid cementite lamellae arc not of homogeneous structure but contain some ferrite sub-lamellae with different widths and same orientation. The continuity of the eutectoid cementite lamellae was reduced when the ferrite sub-lamellae were incorporated. The planar indices of the ferrite sub-lamellae are found usually close to {211}F.Some contrast fringes observed at the cementite/ferrite interface were analyzed and compared with the sub-lamellae in the eutectoid cementite. The formation mechanism of ferrite sub-lamellae in eutectoid cementite was also discussed.
1 Mehl R F,Hagel W C. Progress in metal Physics.New Youk: Pergaaon Press,1956:74 2 DarkenL S,Fisher R M.In:Zackay V F,Aaronson H I eds.,Decomposition of Austenite by DiffusionalProcesses. New York: Interscience Publishers,1962:249 3 Bramfitt B C,Marder A R.Metallography,1973;6:483 4 Hackney S A.Shiftlet G J Phase Transformations in Ferrous Alloys, Warrendale:The Metallurgical Society of AIME.1984: 237 5 黄孝瑛,郭蔽,潘天喜、赵坚,金属学报,1987;23:A200(Huang Xiaoying.Guo Wei、Pan Tianxi, Zhao Jian. Acta Metall Sin,1987: 23:A200) 6 陈世朴,王永瑞,金属电子显微分析 北京:机械工业出版社,1982:89(Chen Shipo,Wang YOngrui.Electron Micro Analysis of Metal. Beijing:Machine Industry Press;1982:89) 7 Han K,Smith G D W.Edmonds D V Metall Mater Trans, 1995: 26A: 1617 8 朱晓东,李承基,章守华,邹明,苏世怀金属学报,1996;32:300(Zhu Xiaodong;Li Chengji,Zhang Shouhua,Zou Ming;Su Shihuai.Acta Metall Sin,1996;32:300) 9 Fridberg J,Hillert M.Acta Metall,1970 18:1253 10 康沫狂,杨思品,管敦惠,钢中贝氏体上海:上海科学技术出版社,1990:110(Kang Mokuang,Yang Sipin,Guan Dunhui Bainite in Steels, Shanghai:Shanghai Science and Technology Press,1990:110) 11 Hillert M.In:Aaronson H I ed,Solid-Solid Phase Transformations,Warrendale:The Metallurgical Society of AIME.1982:789