| INVESTIGATION OF LOADED CRACK TIP ON MICA SURFACE BY ATOMIC FORCE MICROSCOPY |
| LI Xiaodong; WANG Yanbin;CHU Wuyang (University of Science and TechnologyBeijing; Beijing 100083); TIAN Fang; WANG Chen; BAI Chunli (Institute Of Chemistry; Chinese Academy of Sciences; Beijing 100080) |
|
Cite this article:
LI Xiaodong; WANG Yanbin;CHU Wuyang (University of Science and TechnologyBeijing; Beijing 100083); TIAN Fang; WANG Chen; BAI Chunli (Institute Of Chemistry; Chinese Academy of Sciences; Beijing 100080). INVESTIGATION OF LOADED CRACK TIP ON MICA SURFACE BY ATOMIC FORCE MICROSCOPY. Acta Metall Sin, 1997, 33(6): 588-594.
|
|
|
Abstract The atomic structure of loaded crack tips on mica (001) surface has been studied by atomic force microscopy. A small severely disorder region in front of the crack tip,around which there exists an abnormally elastic region, was found. The crack tip on mica surface has many branches, which might be made up with many vacancy clusters.
|
|
Received: 18 June 1997
|
1Hahn G T. Atomic Structure and Mechanical Properties of Metals, 1976: 436 2陈奇志,褚武扬,肖纪美.中国科学, 1994; A24: 291 3张跃,褚武扬,王燕斌,肖纪美.中国科学, 1994; A24: 551 4高珂伟,陈奇志,褚武扬,肖纪美.中国科学, 1994; A24: 993 5 Foecke T,King R M,Dale A F,Gerberich W W.J V ac Sci Technol,1991;B9(2):673 6Mller T,Vehoff H,Neumann P.Ultramicroscopy,1992;42-44:1412 7 Goken M,Vehoff H,Neumann P Scr Metall Maler,199533:1187 8李晓冬,王燕斌,褚武扬等.电子显微学报(已接收) 9Garnaes J,Lindgreen H,Hansen P L,Gould S AC,Hansam PK.Ultramicroscopy,1992;42-44:1428 10 Tang H, Joachim C, Devillers J,J Vac Sci Technolg 1994 B12(3): 2179 11李晓冬,王燕斌,褚武扬,王琛,白春礼.已投中国科学1 |