| THE EFFECT OF Cr ON OXIDATI0N BEHAVIOR OF TiAl INTERMETALLICS |
| TANG Zhaolin; WANG Fuhui; WU Weitao (State Key Laboratory for Corrosion and Protection; Institute of Corrosion and Protection ofMetals; Chinese academy of Sciences. Shenyang 110015) |
|
Cite this article:
TANG Zhaolin; WANG Fuhui; WU Weitao (State Key Laboratory for Corrosion and Protection; Institute of Corrosion and Protection ofMetals; Chinese academy of Sciences. Shenyang 110015). THE EFFECT OF Cr ON OXIDATI0N BEHAVIOR OF TiAl INTERMETALLICS. Acta Metall Sin, 1997, 33(10): 1028-1034.
|
|
|
Abstract The oxidation behavior of Ti-50al, Ti-45al-10Cr and Ti-50al- 10Cr (atomic fraction, %) alloys at 800-1100℃ was investigated. at 800 and 900℃, Ti-45al-10Cr alloy formed a similar layered scale with Tial, consisting of an outer layer of TiO2, an intermediate al2O3 barrier and an inner layer of a mixture of al2O3 and TiO2, exhibited larger weight gains than Ti-50al due to the dopping effect of Cr. at 1000 and 1100℃, however,Ti-45al-10Cr alloy formed a continuous al2O3 enriched scale, which had much smaller weight gains than Tial alloy. Moreover, Ti-50al- 10Cr alloy exhibited an excellent oxidation resistance at 80O-1100℃ due to the formation of a protective al2O3 scale.
|
|
Received: 18 October 1997
|
1 Shida Y, anada H. Corr Sci, 1993; 35: 945 2 Mckee D W, Huang S C. Corr Sci, 1992; 33: 1899 3 McCarron R L, Schaeffer J C, Meier G H, Berztiss D, Perkin R a, Cullinan J In: Froes F H,Caplan I eds,Titanium'92 Sci.and Technol,The Minerals,Metals Matenals Society,1993: 4 Wang F,Lou H,Wu W.Oxid Met;1995;43:395 5 Perkins R a Chiang K T,Meier G H Scr Metall,1987;21:1505 6 Luhtra K L.Oxid Met,1991;36:475 7 Rahmel a Spencer PJ.Oxid Met,1991;35:53 8 Shida Y, anada H. Maler Trans JIM, 1993; 34:236 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|