BAINITIC TRANSFORMATIONS IN SILICON-CONTAINING STEELS
KANG Mokuang; YANG Yanqing; ZHANG Xiyan; SUN Jialin; JIA Husheng; WU Hiaolei (Northwestern Polytechnical University; Xi'an 710072)
Cite this article: 

KANG Mokuang; YANG Yanqing; ZHANG Xiyan; SUN Jialin; JIA Husheng; WU Hiaolei (Northwestern Polytechnical University; Xi'an 710072). BAINITIC TRANSFORMATIONS IN SILICON-CONTAINING STEELS. Acta Metall Sin, 1996, 32(9): 897-903.

Download:  PDF(569KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The meta-bainite which is composed of bainitic ferrite(BF) and retained austenite(A_R) was obtained in silicon-containing steels held in the temperature range of bainite formation for a short time. It was confirmed that BF is supersatuated with carbon by the facts that Spinodal decomposition occurs in BF and that the quantitative data of carbon content in BF was obtained by a new equation based on the X-ray diffraction data. The dislocation loops at BF/A_R boundary, which is very similar to that of lath martensite, and stacking faults in A_R and twins in BF were found by TEM. Based on the results, a three-dimensional model of hainite shear formation controlled by diffusion of carbon was suggested.
Key words:  silicon-containing steel      bainite      phase transformation      carbon content      interfacial dislocation     
Received:  18 September 1996     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1996/V32/I9/897

1DavenportDS,BainCB.TMSAIVE,1930;90:1172KoT,CottrelSA.JIronSteelInst,1952;173:3073AaronsonHI.In:AaronsonHIed.,DecompositionofAustenitebyDiffusionalProcesses.NewYork:Intersciences,1962:3874HehemannRF,KinsmanKR,AaronsonHI.MetallTrans,1972;5A:10775CohenM.MetallTrans,1990;21A:767,13436WaymanCM,AaronsonHI,HirthJP.MetallMaterTrans,1994;25A:1787,25557KangMK(康沫狂),SunJL(孙加林),YangQM(杨全民),MetallTrans.1990;21A:8538NagaknraS,HirotsoY,KusunokiM,SuzukiJ,NagakuraYMetallTrans,1983,14A:10259LiuX(刘晓),ZhongF(钟凡),KangMK(康沫狂).PhysRev,1995;B52:inpress10YangYQ(杨延清),KangMK(康沫狂),ZhouZG(周振刚).ProcIstPacificRimIntConfonAdvancedMaterialsandProcessing,TMS,1993:46911RigsbeeTM,AaronsonHI.ActaMelall,1979;27:35112李承基.材料科学进展,1988;3:7513张喜燕.西北工业大学博士学位论文,199414SandvikBPJ,WaymanCM.MetallTrans,1983;14A:82315SandvikBPJ.MetallTrans,1982;13A:78416孙加林,康沫狂.金属学报,1991;27:A23217WuXL(武小雷),ZhangXY(张喜燕),KangMK(康沫狂),YangYQ(杨延清).MaterTransJIM,1994;35:78218FriedelJ著,王煜译.位错.北京:科学出版社,1984:5519魏秋明,西北工业大学博士学位论文,1991
[1] BAI Jiaming, LIU Jiantao, JIA Jian, ZHANG Yiwen. Creep Properties and Solute Atomic Segregation of High-W and High-Ta Type Powder Metallurgy Superalloy[J]. 金属学报, 2023, 59(9): 1230-1242.
[2] FENG Aihan, CHEN Qiang, WANG Jian, WANG Hao, QU Shoujiang, CHEN Daolun. Thermal Stability of Microstructures in Low-Density Ti2AlNb-Based Alloy Hot Rolled Plate[J]. 金属学报, 2023, 59(6): 777-786.
[3] ZHAO Yafeng, LIU Sujie, CHEN Yun, MA Hui, MA Guangcai, GUO Yi. Critical Inclusion Size and Void Growth in Dual-Phase Ferrite-Bainite Steel During Ductile Fracture[J]. 金属学报, 2023, 59(5): 611-622.
[4] WANG Chongyang, HAN Shiwei, XIE Feng, HU Long, DENG Dean. Influence of Solid-State Phase Transformation and Softening Effect on Welding Residual Stress of Ultra-High Strength Steel[J]. 金属学报, 2023, 59(12): 1613-1623.
[5] ZHANG Kaiyuan, DONG Wenchao, ZHAO Dong, LI Shijian, LU Shanping. Effect of Solid-State Phase Transformation on Stress and Distortion for Fe-Co-Ni Ultra-High Strength Steel Components During Welding and Vacuum Gas Quenching Processes[J]. 金属学报, 2023, 59(12): 1633-1643.
[6] LI Xiaobing, QIAN Kun, SHU Lei, ZHANG Mengshu, ZHANG Jinhu, CHEN Bo, LIU Kui. Effect of W Content on the Phase Transformation Behavior in Ti-42Al-5Mn- xW Alloy[J]. 金属学报, 2023, 59(10): 1401-1410.
[7] LI Sai, YANG Zenan, ZHANG Chi, YANG Zhigang. Phase Field Study of the Diffusional Paths in Pearlite-Austenite Transformation[J]. 金属学报, 2023, 59(10): 1376-1388.
[8] ZHU Bin, YANG Lan, LIU Yong, ZHANG Yisheng. Micromechanical Properties of Duplex Microstructure of Martensite/Bainite in Hot Stamping via the Reverse Algorithms in Instrumented Sharp Indentation[J]. 金属学报, 2022, 58(2): 155-164.
[9] ZHU Dongming, HE Jiangli, SHI Genhao, WANG Qingfeng. Effect of Welding Heat Input on Microstructure and Impact Toughness of the Simulated CGHAZ in Q500qE Steel[J]. 金属学报, 2022, 58(12): 1581-1588.
[10] LI Xueda, LI Chunyu, CAO Ning, LIN Xueqiang, SUN Jianbo. Crystallography of Reverted Austenite in the Intercritically Reheated Coarse-Grained Heat-Affected Zone of High Strength Pipeline Steel[J]. 金属学报, 2021, 57(8): 967-976.
[11] FENG Miaomiao, ZHANG Hongwei, SHAO Jingxia, LI Tie, LEI Hong, WANG Qiang. Prediction of Macrosegregation of Fe-C Peritectic Alloy Ingot Through Coupling with Thermodynamic Phase Transformation Path[J]. 金属学报, 2021, 57(8): 1057-1072.
[12] JIANG Zhonghua, DU Junyi, WANG Pei, ZHENG Jianneng, LI Dianzhong, LI Yiyi. Mechanism of Improving the Impact Toughness of SA508-3 Steel Used for Nuclear Power by Pre-Transformation of M-A Islands[J]. 金属学报, 2021, 57(7): 891-902.
[13] LI Jinshan, TANG Bin, FAN Jiangkun, WANG Chuanyun, HUA Ke, ZHANG Mengqi, DAI Jinhua, KOU Hongchao. Deformation Mechanism and Microstructure Control of High Strength Metastable β Titanium Alloy[J]. 金属学报, 2021, 57(11): 1438-1454.
[14] LIU Chenxi, MAO Chunliang, CUI Lei, ZHOU Xiaosheng, YU Liming, LIU Yongchang. Recent Progress in Microstructural Control and Solid-State Welding of Reduced Activation Ferritic/Martensitic Steels[J]. 金属学报, 2021, 57(11): 1521-1538.
[15] CHEN Xiang,CHEN Wei,ZHAO Yang,LU Sheng,JIN Xiaoqing,PENG Xianghe. Assembly Performance Simulation of NiTiNb Shape Memory Alloy Pipe Joint Considering Coupling Effect of Phase Transformation and Plastic Deformation[J]. 金属学报, 2020, 56(3): 361-373.
No Suggested Reading articles found!