CHANGES OF ATOMIC ORDER IN Cu-Al-Ni-Mn-Ti SHAPE MEMORY ALLOY DURING AGING
WEI Zhongguo; YANG Dazhi (Dalian University of Technology; Dalian 116024)
Cite this article: 

WEI Zhongguo; YANG Dazhi (Dalian University of Technology; Dalian 116024). CHANGES OF ATOMIC ORDER IN Cu-Al-Ni-Mn-Ti SHAPE MEMORY ALLOY DURING AGING. Acta Metall Sin, 1996, 32(6): 578-584.

Download:  PDF(459KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The changes of atomic order state during aging of the parent phase and martensite in an as-quenched Cu-Al-Ni-Mn-Ti shape memory alloy were investigated by X-ray diffraction and in situ electrical resistivity measurements. It was shown that the aging mechanisms of the parent phase and martensite are different. During parent phase aging, DO_3 atomic reordering occurs, leading to an increase in the degree of long range order. During martensite aging, however, short range atomic disordering takes place, resulting in the stabilization of martensite.
Key words:  Cu-Al-Ni-Mn-Ti shape memory alloy      martensite      aging      long range order      disorder     
Received:  18 June 1996     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1996/V32/I6/578

1AhersM.In:ProcICOMAT-86,Nara:JIM,1986:7862YangDZ,WeiZG.In:ChuYYed.,ShapeMemoryMaterials94,Beijing:InternationalAcademicPublishers,1994:3193DunneDP,KennonNF.MetalsForum,1981:4:1764WeiZG,YangDZMaterSciEng,1989;119A:1455ScarsbrookG,CookJ,StobbsWMJPhysColloq,1982;43(C4):7036Abu-ArabA,AhersM.ActaMetall,1988;36:26277RossiterPL.TheElectricalResistivityofMetalsandAlloys.Cambridge:CambridgeUniversityPress,1987:1378ZouWH,PengHY,WangR,GuiJ,YangDZActaMetallMater,1995;43:30099CooremanL,HumbeeckJ,DelaeyL,ActaMetallMater,1990;38:266310HumbeeckJV,JanssenJDelaeyL.ScrMetall.1984;18:89311ShimizuK,TadakiMaterTransJIM,1992;33:16512HashiguchiY,HiguchiH,MatsuiI,NitaniT,TokunohH.In:ProcICOMAT-86,Nara:JIM,1986:832
[1] ZHANG Leilei, CHEN Jingyang, TANG Xin, XIAO Chengbo, ZHANG Mingjun, YANG Qing. Evolution of Microstructures and Mechanical Properties of K439B Superalloy During Long-Term Aging at 800oC[J]. 金属学报, 2023, 59(9): 1253-1264.
[2] LIANG Kai, YAO Zhihao, XIE Xishan, YAO Kaijun, DONG Jianxin. Correlation Between Microstructure and Properties of New Heat-Resistant Alloy SP2215[J]. 金属学报, 2023, 59(6): 797-811.
[3] WANG Zhoutou, YUAN Qing, ZHANG Qingxiao, LIU Sheng, XU Guang. Microstructure and Mechanical Properties of a Cold Rolled Gradient Medium-Carbon Martensitic Steel[J]. 金属学报, 2023, 59(6): 821-828.
[4] LIU Manping, XUE Zhoulei, PENG Zhen, CHEN Yulin, DING Lipeng, JIA Zhihong. Effect of Post-Aging on Microstructure and Mechanical Properties of an Ultrafine-Grained 6061 Aluminum Alloy[J]. 金属学报, 2023, 59(5): 657-667.
[5] WANG Changsheng, FU Huadong, ZHANG Hongtao, XIE Jianxin. Effect of Cold-Rolling Deformation on Microstructure, Properties, and Precipitation Behavior of High-Performance Cu-Ni-Si Alloys[J]. 金属学报, 2023, 59(5): 585-598.
[6] WANG Bin, NIU Mengchao, WANG Wei, JIANG Tao, LUAN Junhua, YANG Ke. Microstructure and Strength-Toughness of a Cu-Contained Maraging Stainless Steel[J]. 金属学报, 2023, 59(5): 636-646.
[7] MA Guonan, ZHU Shize, WANG Dong, XIAO Bolv, MA Zongyi. Aging Behaviors and Mechanical Properties of SiC/Al-Zn-Mg-Cu Composites[J]. 金属学报, 2023, 59(12): 1655-1664.
[8] GONG Xiangpeng, WU Cuilan, LUO Shifang, SHEN Ruohan, YAN Jun. Effect of Natural Aging on Artificial Aging of an Al-2.95Cu-1.55Li-0.57Mg-0.18Zr Alloy at 160oC[J]. 金属学报, 2023, 59(11): 1428-1438.
[9] CHEN Xueshuang, HUANG Xingmin, LIU Junjie, LV Chao, ZHANG Juan. Microstructure Regulation and Strengthening Mechanisms of a Hot-Rolled & Intercritical Annealed Medium-Mn Steel Containing Mn-Segregation Band[J]. 金属学报, 2023, 59(11): 1448-1456.
[10] HOU Xuru, ZHAO Lin, REN Shubin, PENG Yun, MA Chengyong, TIAN Zhiling. Effect of Heat Input on Microstructure and Mechanical Properties of Marine High Strength Steel Fabricated by Wire Arc Additive Manufacturing[J]. 金属学报, 2023, 59(10): 1311-1323.
[11] LI Xiaolin, LIU Linxi, LI Yating, YANG Jiawei, DENG Xiangtao, WANG Haifeng. Mechanical Properties and Creep Behavior of MX-Type Precipitates Strengthened Heat Resistant Martensite Steel[J]. 金属学报, 2022, 58(9): 1199-1207.
[12] GENG Yaoxiang, TANG Hao, XU Junhua, ZHANG Zhijie, YU Lihua, JU Hongbo, JIANG Le, JIAN Jianglin. Formability and Mechanical Properties of High-Strength Al-(Mn, Mg)-(Sc, Zr) Alloy Produced by Selective Laser Melting[J]. 金属学报, 2022, 58(8): 1044-1054.
[13] GAO Chuan, DENG Yunlai, WANG Fengquan, GUO Xiaobin. Effect of Creep Aging on Mechanical Properties of Under-Aged 7075 Aluminum Alloy[J]. 金属学报, 2022, 58(6): 746-759.
[14] REN Ping, CHEN Xingpin, WANG Cunyu, YU Feng, CAO Wenquan. Effects of Pre-Strain and Two-Step Aging on Microstructure and Mechanical Properties of Fe-30Mn-11Al-1.2C Austenitic Low-Density Steel[J]. 金属学报, 2022, 58(6): 771-780.
[15] ZHU Bin, YANG Lan, LIU Yong, ZHANG Yisheng. Micromechanical Properties of Duplex Microstructure of Martensite/Bainite in Hot Stamping via the Reverse Algorithms in Instrumented Sharp Indentation[J]. 金属学报, 2022, 58(2): 155-164.
No Suggested Reading articles found!