| EFFECTS OF WC ADDITION ON MICROSTRUCTURE AND MAGNETIC PROPERTIES OF SINTERED Nd-Fe-B MAGNETS |
| ZHAO Guoxian; SONG Hiaoping; CHEN Zhongmin; YAN Aru; WANG Hiaotian (Xi'an Jiaotong Univerrity; Xi'an 710049) (Manuscript received 1995-09-01) |
|
Cite this article:
ZHAO Guoxian; SONG Hiaoping; CHEN Zhongmin; YAN Aru; WANG Hiaotian (Xi'an Jiaotong Univerrity; Xi'an 710049) (Manuscript received 1995-09-01). EFFECTS OF WC ADDITION ON MICROSTRUCTURE AND MAGNETIC PROPERTIES OF SINTERED Nd-Fe-B MAGNETS. Acta Metall Sin, 1996, 32(4): 413-416.
|
|
|
Abstract The coercivity of sintered Nd-Fe-B magnets is enhanced by the addition of a small amount of WC and the highest one corresponds to an amount of 0.6% WC addition. But a higher amount of WC addition leads to the decrease in coercivity. The grain size decreases first and then increases with increasing the WC content. SEM observation revealed that W-Fe-B phase with colony-like shape appears at grain boundaries or in some matrix regions, and that the contents of C and W in the regions near to W-Fe-B phase are higher than other regions. Correspondent: SONG Xiaoping,(College of Materials Science, Xi'an Jiaotong University, Xi'an 710049)
|
|
Received: 18 April 1996
|
| 1HirosawaS,TsubokawaY.JMagnMagnMater,1990;84:3092周寿增,唐伟忠,王润,金属学报,1990;26:B2903HirosawaS,TokuharaK,MatsuuraY,YamamotoHFujimuraS.JMagnMagnMater,1986;61:3634RodewaldW,SchreyP.JMagnMagnMater,1990;83:2065BuschowKHJ,deMooijDB,DenissenCJM.JLess-CommonMet,1988,142:L136ChuTY,ChinTS,LinCH,YaoJM.JApplPhys,1994;76:68347AiL,LianFZ,ZhangXS,WuJF,ZhaoHM,FuYJ,ZhaoQH,LIHW,MaoXY,YuYB.Proc2ndIntSymponPhysicsofMagneticMaterials,Beijing,1992:729@ |