Please wait a minute...
Acta Metall Sin  1996, Vol. 32 Issue (3): 328-332    DOI:
Current Issue | Archive | Adv Search |
MoSSBAUER SPECTROSCOPY STUDY OF (Sm_(1-x)Y_x)_2Fe_(17)N_y
LUO Guangsheng; HE Lunyan (Nanchang University; Nanchang 330047); ZENG Yiwei (Beijing Normal University; Beijing 100875); YANG Fuming (Institute of Physics; Chinese Academy of Sciences; Beijing 100080)(Manuscript received 1995-06-29; in revised form 1995-10-02)
Cite this article: 

LUO Guangsheng; HE Lunyan (Nanchang University; Nanchang 330047); ZENG Yiwei (Beijing Normal University; Beijing 100875); YANG Fuming (Institute of Physics; Chinese Academy of Sciences; Beijing 100080)(Manuscript received 1995-06-29; in revised form 1995-10-02). MoSSBAUER SPECTROSCOPY STUDY OF (Sm_(1-x)Y_x)_2Fe_(17)N_y. Acta Metall Sin, 1996, 32(3): 328-332.

Download:  PDF(371KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The magnetic properties of(Sm1-xYx)2Fe(17)Ny were studied by Mossbauer spectroscopy. The following conclusions were obtained:The uniaxial anisotropy of Sm sublattice is stronger and is the main mechanism of the total anisotropy; The preferential occupation of Y atom leads to the change of crystal structure and the influence on anisotropy is smaller. Correspondent: L UO Guangsheng, lecturer, Department of Materials, Nanchang University, Nanchang 330047
Key words:  (Sm_(1-x)Y_x)_2Fe_(17)N_y      anisotropy      preferential occupation      saturation atom moment      Mssbauer spectroscopy     
Received:  18 March 1996     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1996/V32/I3/328

1CoeyJMD,SunHong.JMagnMagnMater,1990;87:L2512IsnardO,MiragliaS,SoubeyrouxJL,FruchartD,StergiouA,JLess-CommonMet,1990;162:2733ShigaM,NakamuraY,JPhysSocJpn,1976;40:1295
[1] ZHANG Zixuan, YU Jinjiang, LIU Jinlai. Anisotropy of Stress Rupture Property of Ni Base Single Crystal Superalloy DD432[J]. 金属学报, 2023, 59(12): 1559-1567.
[2] GE Jinguo, LU Zhao, HE Siliang, SUN Yan, YIN Shuo. Anisotropy in Microstructures and Mechanical Properties of 2Cr13 Alloy Produced by Wire Arc Additive Manufacturing[J]. 金属学报, 2023, 59(1): 157-168.
[3] GAO Yubi, DING Yutian, LI Haifeng, DONG Hongbiao, ZHANG Ruiyao, LI Jun, LUO Quanshun. Effect of Deformation Rate on the Elastic-Plastic Deformation Behavior of GH3625 Alloy[J]. 金属学报, 2022, 58(5): 695-708.
[4] LU Lei, ZHAO Huaizhi. Progress in Strengthening and Toughening Mechanisms of Heterogeneous Nanostructured Metals[J]. 金属学报, 2022, 58(11): 1360-1370.
[5] WANG Di, HUANG Jinhui, TAN Chaolin, YANG Yongqiang. Review on Effects of Cyclic Thermal Input on Microstructure and Property of Materials in Laser Additive Manufacturing[J]. 金属学报, 2022, 58(10): 1221-1235.
[6] BI Sheng, LI Zechen, SUN Haixia, SONG Baoyong, LIU Zhenyu, XIAO Bolv, MA Zongyi. Microstructure and Mechanical Properties of Carbon Nanotubes-Reinforced 7055Al Composites Fabricated by High-Energy Ball Milling and Powder Metallurgy Processing[J]. 金属学报, 2021, 57(1): 71-81.
[7] LIU Jinlai, YE Lihua, ZHOU Yizhou, LI Jinguo, SUN Xiaofeng. Anisotropy of Elasticity of a Ni Base Single Crystal Superalloy[J]. 金属学报, 2020, 56(6): 855-862.
[8] HU Bin,LI Shusuo,PEI Yanling,GONG Shengkai,XU Huibin. Influence of Small Misorientation from <111> on Creep Properties of a Ni-Based Single Crystal Superalloy[J]. 金属学报, 2019, 55(9): 1204-1210.
[9] WANG Li,HE Yufeng,SHEN Jian,ZHENG Wei,LOU Langhong,ZHANG Jian. Effect of Secondary Orientation on Oxidation Anisotropy Around the Holes of Single Crystal Superalloy During Thermal Fatigue Tests[J]. 金属学报, 2019, 55(11): 1417-1426.
[10] HE Xianmei, TONG Liuniu, GAO Cheng, WANG Yichao. Effect of Nd Content on the Structure and Magnetic Properties of Si(111)/Cr/Nd-Co/Cr Thin Films Prepared by Magnetron Sputtering[J]. 金属学报, 2019, 55(10): 1349-1358.
[11] Xiaoqin MA, Qingfeng ZHAN, Jincai LI, Qingfang LIU, Baomin WANG, Runwei LI. Influence of Oblique Sputtering on Stripe Magnetic Domain Structure and Magnetic Anisotropy of CoFeB Thin Films[J]. 金属学报, 2018, 54(9): 1281-1288.
[12] Mingliang HUANG, Hongyu SUN. Interaction Between β-Sn Grain Orientation and Electromigration Behavior in Flip-Chip Lead-Free Solder Bumps[J]. 金属学报, 2018, 54(7): 1077-1086.
[13] Xudong LI, Pingli MAO, Yanyu LIU, Zheng LIU, Zhi WANG, Feng WANG. Anisotropy and Deformation Mechanisms ofAs-Extruded Mg-3Zn-1Y Magnesium AlloyUnder High Strain Rates[J]. 金属学报, 2018, 54(4): 557-565.
[14] Peibei JI, Lichu ZHOU, Xuefeng ZHOU, Feng FANG, Jianqing JIANG. Study on Anisotropic Mechanical Properties of Cold Drawn Pearlitic Steel Wire[J]. 金属学报, 2018, 54(4): 494-500.
[15] Shuangming LI, Binqiang WANG, Zhenpeng LIU, Hong ZHONG, Rui HU, Yi LIU, Ximing LUO. Grain Orientation Competitive Growth of High Melting Point Metals Ir and Mo Under Electron Beam Floating Zone Melting[J]. 金属学报, 2018, 54(10): 1435-1441.
No Suggested Reading articles found!