Please wait a minute...
Acta Metall Sin  1996, Vol. 32 Issue (3): 294-302    DOI:
Current Issue | Archive | Adv Search |
OXIDATION OF Fe-Nb ALLOYS UNDER 0.1 Mpa PURE OXYGEN AT 600─800℃
NIU Yan; WU Weitao; FGESMUNDO; FC.RIZZO;(State Key Laboratory for Corrosion and Protection; Institute of Corrosion and Protection of Metals; Chinese Academy of Sciences; Shenyang 1 100015 )(Istituto di Chimica; Facolta di Ingegneria; Universita' di Genova; Fiera del Mare;Pad. D; 16129 Genova; Italy )(Departamento de Ciencia dos Materiais e Metalurgia; Pontificia Universidade Catolica do Rio de Janeiro; Caixa Postal 38008; 22453-900; RJ; Brazil )(Manuscript received 1995-05- 19; in revised form 1 995-09-08)
Cite this article: 

NIU Yan; WU Weitao; FGESMUNDO; FC.RIZZO;(State Key Laboratory for Corrosion and Protection; Institute of Corrosion and Protection of Metals; Chinese Academy of Sciences; Shenyang 1 100015 )(Istituto di Chimica; Facolta di Ingegneria; Universita' di Genova; Fiera del Mare;Pad. D; 16129 Genova; Italy )(Departamento de Ciencia dos Materiais e Metalurgia; Pontificia Universidade Catolica do Rio de Janeiro; Caixa Postal 38008; 22453-900; RJ; Brazil )(Manuscript received 1995-05- 19; in revised form 1 995-09-08). OXIDATION OF Fe-Nb ALLOYS UNDER 0.1 Mpa PURE OXYGEN AT 600─800℃. Acta Metall Sin, 1996, 32(3): 294-302.

Download:  PDF(747KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The oxidation of two Fe-Nb alloys containing 15 and 30% Nb(mass fraction) has been studied at 600─800℃ under 0.1 MPa pure oxygen.The reaction followed the parabolic rate law to a reasonable approximation with rate constants much lower than that for the oxidation of pure iron under the same condition. Internal oxidation and depletion of niobium in the alloy have not been observed. The external scales were composed of Fe2O3 and a dispersion of double Fe-Nb oxide, while FeO and Fe2O3 were not observed.The oxidation behavior of these alloys is interpreted with reference to an approximate phase diagram of the ternary system Fe-Nb-O, taking into account the effects of the low solubility of niobium in the base metal and of the presence of two metallic phases in the alloy. Correspondent: NIU Yan, State Key Laboratory for Corrosion and Protection, ICPM Shenyang 110015
Key words:  Fe-Nb alloy      high temperature oxidation      pure oxygen     
Received:  18 March 1996     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1996/V32/I3/294

1NiuY,GesmundoF,VianiF.CorrosSci,1994;36:8832CastroM,NiuY,RizzoF,GesmundoF.OxidMet,1995;43:5613NiuY,GesmundoF,VianiF.CorrosSci,inprint4SvedbergRC.in:ForoulisZA,PettitFS,Eds,PropertiesofHighTemperatureAlloys,Princeton,NJ:TheElectrochemSoc,1977.3315RappRA,Corrosion,1965;21:3826GesmundoF,NiuY,VianiF,KizzoF.OxidMet,tobepublished7GesmundoF,NiuY,VianiF.OxidMet.1995;43:3798GesmundoF,VianiF,NiuY,DouglassDL.OxidMet,1994;42:4659GesmundoF,VianiF.OxidMet,1986;25:26910GesmundoF,VianiF,NiuY.OxidMet,1994;42:40911MrowecS.GasCorrosionofMetals,Washington:NationalBureauofstandards,197812BirchenallCE.In:DouglassDL,ed,OxidationofMetalsandAlloys,AmericanSoc.forMetals,MetalsPark,1971:17713PaidassiJ.In:BenardJ,ed,L′OxydationdesMetaux,Paris:Gauthier-Villars,1964,vol.Ⅱ,p.13x
[1] XU Wenguo, HAO Wenjiang, LI Yingju, ZHAO Qingbin, LU Bingyu, GUO Heyi, LIU Tianyu, FENG Xiaohui, YANG Yuansheng. Effects of Trace Aluminum and Titanium on High Temper-ature Oxidation Behavior of Inconel 690 Alloy[J]. 金属学报, 2023, 59(12): 1547-1558.
[2] XIE Leipeng, SUN Wenyao, CHEN Minghui, WANG Jinlong, WANG Fuhui. Effects of Processing on Microstructures and Properties of FGH4097 Superalloy[J]. 金属学报, 2022, 58(8): 992-1002.
[3] YANG Liang, LV Haotian, WAN Chunlei, GONG Qianming, CHEN Hao, ZHANG Chi, YANG Zhigang. Review: Mechanism of Reactive Element Effect—Oxide Pegging[J]. 金属学报, 2021, 57(2): 182-190.
[4] Mingyu ZHAO,Huijuan ZHEN,Zhihong DONG,Xiuying YANG,Xiao PENG. Preparation and Performance of a Novel Wear-Resistant and High Temperature Oxidation-Resistant NiCrAlSiC Composite Coating[J]. 金属学报, 2019, 55(7): 902-910.
[5] GAO Bo, WANG Lei, SONG Xiu, LIU Yang, YANG Shuyu, CHIBA Akihiko. Effect of Pre-Oxidation on High Temperature Oxidation and Corrosion Behavior of Co-Al-W-Based Superalloy[J]. 金属学报, 2019, 55(10): 1273-1281.
[6] Yin BAI, Zhengdong LIU, Jianxin XIE, Hansheng BAO, Zhengzong CHEN. Effect of Pre-Oxidation Treatment on the Behavior of High Temperature Oxidation in Steam of G115 Steel[J]. 金属学报, 2018, 54(6): 895-904.
[7] Yuxiang ZENG,Xiping GUO,Yanqiang QIAO,Zhongyi NIE. EFFECT OF Zr ADDITION ON MICROSTRUCTURE AND OXIDATION RESISTANCE OF Nb-Ti-Si BASE ULTRAHIGH-TEMPERATURE ALLOYS[J]. 金属学报, 2015, 51(9): 1049-1058.
[8] Haigen ZHAO,Shusuo LI,Yanling PEI,Shengkai GONG,Huibin XU. MICROSTRUCTURE AND MECHANICAL PROPERTIES OF Ni3Al-BASED SINGLE CRYSTSAL ALLOY IC21[J]. 金属学报, 2015, 51(10): 1279-1287.
[9] ZHOU Xiaowei SHEN Yifu GU Dongdong. MICROSTRUCTURE AND HIGH TEMPERATURE OXIDATION RESISTANCE OF NANOCRYSTALLINE Ni–CeO2 COMPOSITE COATINGS DEPOSITED BY DOUBLE–PULSED ELECTRO DEPOSITION[J]. 金属学报, 2012, 48(8): 957-964.
[10] YU Daqian, LU Xuyang, MA Jun, JIANG Sumeng, LIU Shanchuan, GONG Jun, SUN Chao. STUDY OF OXIDATION BEHAVIOR OF THE GRADIENT NiCrAlY COATING AT 1000 AND 1100 ℃[J]. 金属学报, 2012, 48(6): 759-768.
[11] SONG Peng LU Jiansheng ZHANG Defeng LU Jianguo LI Dejiang. EFFECT OF La AND Hf DOPANT ON THE HIGH TEMPERATURE OXIDATION OF CoNiCrAl ALLOYS[J]. 金属学报, 2011, 47(6): 655-662.
[12] PENG Xin JIANG Sumeng DUAN Xuhai GONG Jun SUN Chao. HIGH TEMPERATURE OXIDATION BEHAVIOR OF A (MCrAlY+AlSiY) COMPOSITE COATING[J]. 金属学报, 2009, 45(3): 378-384.
[13] Xinqing Zhao. THE EFFECT OF Nb ON THE OXIDATION BEHAVIOR OF TiNiAl ALLOYS[J]. 金属学报, 2006, 42(8): 820-826 .
[14] ZHANG Xuejun; WU Weitao; NIU Yan. Effect Of Silver Addition On Surface Morphology Of Al2O3 Scales During Oxidation Of β-NiAl[J]. 金属学报, 2005, 41(4): 369-374 .
[15] GUO Minghu; WANG Qimin; KE Peiling; CUI Yuyou; GONG Jun; SUN Chao; WEN Lishi. Effect of Ni-Al coating on high temperature oxidation behaviors of Ti-22Al-26Nb alloy[J]. 金属学报, 2005, 41(3): 312-316 .
No Suggested Reading articles found!