EFFECT OF Ni-La_2O_3 ELECTRODEPOSITED COMPOSITE FILM ON THERMAL CYCLING OXIDATION OF Ni
PENG Xiao; LITiefan; LI Meishuan; MA Xinqing; PING Dehai(State Key Laboratory of Corrosion and Protection; Institute of Corrosion and Protection of Metals; Chinese Academy of Sciences; Shenyang 110015)(Laboratory of Atomic Imaging of Solids; Institute of Metal Reserch; Chinese Academy of Sciences; Shenyang 110015)(Manuscript received 1995-06-07; in revised form 1995-10-06)
Cite this article: 

PENG Xiao; LITiefan; LI Meishuan; MA Xinqing; PING Dehai(State Key Laboratory of Corrosion and Protection; Institute of Corrosion and Protection of Metals; Chinese Academy of Sciences; Shenyang 110015)(Laboratory of Atomic Imaging of Solids; Institute of Metal Reserch; Chinese Academy of Sciences; Shenyang 110015)(Manuscript received 1995-06-07; in revised form 1995-10-06). EFFECT OF Ni-La_2O_3 ELECTRODEPOSITED COMPOSITE FILM ON THERMAL CYCLING OXIDATION OF Ni. Acta Metall Sin, 1996, 32(2): 180-186.

Download:  PDF(593KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The thermal cycling oxidation resistance of Ni with a Ni-La_2O_3 electrodeposited composite film of 30 μm in thickness is significantly improved in comparison to Ni with and without Ni-plating for 100 h-cyclic oxidation at 1273 K. The rapid growth and severe cracking of scale-on Ni with or without Ni-plating occurred during the thermal cycling process, but the application of Ni-La_2O_3 electrodeposited composite film on Ni resulted in a markable reduction of NiO growth and the scale has finer grain, non-cracking morphology. Electron probe microanalyses revealed that in the total NiO scale with an average thickness of about 50 μm, La_2O_3 was located in the region of about 31 μm near the scale / gas interface. High resolution electron microscopy showed that in the codeposited film La_2O_3 nanoparticles below 5 nm is in the dispersive or cluster state- Therefore, it is proposed that the modification of oxidation mechanism and mechanical property of the scale of Ni With Ni-La_2O_3 electrodeposited composite film may resulted from the partial dissolution of La_2O_3 with nano-size, and the segregation of La~(3+) at the NiO grain boundaries, which prevent the short distance diffusion of Ni~(2+).(Correspondent. PENG Xiao, Institute of Corrosion and Protection of Metals, Chinese Academy of Sciences,Shenyang 110015)
Key words:  electrodeposited composite film      Ni      La_2O_3      thermal cycling oxidation     
Received:  18 February 1996     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1996/V32/I2/180

1MorinF,DufourLC,TrudelGOxidMet,1992;37:392WhittleDP,StringerJ.PhilTransRSocLond,1980;A295:3093MoonDP.SurtInterfaceAnal,1988;12:274HampikianJM,DevereuxOF,PotterDI.MaterSciEng,1989;AL16:1195CzerwinskiFandSmeltzerJA.OxidMet,1993;40,5036CzerwinskiF,SzpunarJA,Macaulay-NewcombeRG,SmelterWW.OxidMet,1995;43:257KarchJ,BirringerR,GleiterH,Nature,1987;330:5568彭晓,中国科学院金属腐蚀与防护研究所硕士论文,19929PcttitFS,EdwardJF.JElectrochemSoc,1964;111:13510HaanappelVAC,FransenT,GeerdinkB,GellingsPJ,StroonsnjderMF.OxidMet,1991;35:405
[1] ZHANG Leilei, CHEN Jingyang, TANG Xin, XIAO Chengbo, ZHANG Mingjun, YANG Qing. Evolution of Microstructures and Mechanical Properties of K439B Superalloy During Long-Term Aging at 800oC[J]. 金属学报, 2023, 59(9): 1253-1264.
[2] ZHAO Peng, XIE Guang, DUAN Huichao, ZHANG Jian, DU Kui. Recrystallization During Thermo-Mechanical Fatigue of Two High-Generation Ni-Based Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1221-1229.
[3] BI Zhongnan, QIN Hailong, LIU Pei, SHI Songyi, XIE Jinli, ZHANG Ji. Research Progress Regarding Quantitative Characterization and Control Technology of Residual Stress in Superalloy Forgings[J]. 金属学报, 2023, 59(9): 1144-1158.
[4] ZHENG Liang, ZHANG Qiang, LI Zhou, ZHANG Guoqing. Effects of Oxygen Increasing/Decreasing Processes on Surface Characteristics of Superalloy Powders and Properties of Their Bulk Alloy Counterparts: Powders Storage and Degassing[J]. 金属学报, 2023, 59(9): 1265-1278.
[5] WANG Lei, LIU Mengya, LIU Yang, SONG Xiu, MENG Fanqiang. Research Progress on Surface Impact Strengthening Mechanisms and Application of Nickel-Based Superalloys[J]. 金属学报, 2023, 59(9): 1173-1189.
[6] ZHANG Jian, WANG Li, XIE Guang, WANG Dong, SHEN Jian, LU Yuzhang, HUANG Yaqi, LI Yawei. Recent Progress in Research and Development of Nickel-Based Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1109-1124.
[7] BAI Jiaming, LIU Jiantao, JIA Jian, ZHANG Yiwen. Creep Properties and Solute Atomic Segregation of High-W and High-Ta Type Powder Metallurgy Superalloy[J]. 金属学报, 2023, 59(9): 1230-1242.
[8] GONG Shengkai, LIU Yuan, GENG Lilun, RU Yi, ZHAO Wenyue, PEI Yanling, LI Shusuo. Advances in the Regulation and Interfacial Behavior of Coatings/Superalloys[J]. 金属学报, 2023, 59(9): 1097-1108.
[9] JIANG He, NAI Qiliang, XU Chao, ZHAO Xiao, YAO Zhihao, DONG Jianxin. Sensitive Temperature and Reason of Rapid Fatigue Crack Propagation in Nickel-Based Superalloy[J]. 金属学报, 2023, 59(9): 1190-1200.
[10] DING Hua, ZHANG Yu, CAI Minghui, TANG Zhengyou. Research Progress and Prospects of Austenite-Based Fe-Mn-Al-C Lightweight Steels[J]. 金属学报, 2023, 59(8): 1027-1041.
[11] XU Yongsheng, ZHANG Weigang, XU Lingchao, DAN Wenjiao. Simulation of Deformation Coordination and Hardening Behavior in Ferrite-Ferrite Grain Boundary[J]. 金属学报, 2023, 59(8): 1042-1050.
[12] MU Yahang, ZHANG Xue, CHEN Ziming, SUN Xiaofeng, LIANG Jingjing, LI Jinguo, ZHOU Yizhou. Modeling of Crack Susceptibility of Ni-Based Superalloy for Additive Manufacturing via Thermodynamic Calculation and Machine Learning[J]. 金属学报, 2023, 59(8): 1075-1086.
[13] LI Jingren, XIE Dongsheng, ZHANG Dongdong, XIE Hongbo, PAN Hucheng, REN Yuping, QIN Gaowu. Microstructure Evolution Mechanism of New Low-Alloyed High-Strength Mg-0.2Ce-0.2Ca Alloy During Extrusion[J]. 金属学报, 2023, 59(8): 1087-1096.
[14] CHEN Liqing, LI Xing, ZHAO Yang, WANG Shuai, FENG Yang. Overview of Research and Development of High-Manganese Damping Steel with Integrated Structure and Function[J]. 金属学报, 2023, 59(8): 1015-1026.
[15] ZHANG Haifeng, YAN Haile, FANG Feng, JIA Nan. Molecular Dynamic Simulations of Deformation Mechanisms for FeMnCoCrNi High-Entropy Alloy Bicrystal Micropillars[J]. 金属学报, 2023, 59(8): 1051-1064.
No Suggested Reading articles found!