| THERMODYNAMICS OF SHEAR MECHANISM OF BAINITIC FORMATION IN CARBON-DEPLETED REGIONS OF AUSTENITE IN Fe-C ALLOYS |
| WU Xiaolei; ZHANG Xiyan; KANG Mokuang; YANG Yanqing (Northwestern Polytechnical University; Xi'an 710072) |
|
Cite this article:
WU Xiaolei; ZHANG Xiyan; KANG Mokuang; YANG Yanqing (Northwestern Polytechnical University; Xi'an 710072). THERMODYNAMICS OF SHEAR MECHANISM OF BAINITIC FORMATION IN CARBON-DEPLETED REGIONS OF AUSTENITE IN Fe-C ALLOYS. Acta Metall Sin, 1995, 31(3): 115-119.
|
|
|
Abstract Thermodynamic analysis for shear formation of bainitic ferrite in carbon-depleted regions of austenite is conducted. The driving force of bainitic formation in carbon-depleted region increases with the reduction of carbon concentration in this region and can overcome the energy resistance. The critical driving force (absolute value) at Bs temperature is 470─1200 J/mol. The freshly-formed bainitic ferrite is with partial supersaturation of carbon, which increases with decreasing the reaction temperature. Finally,it is concluded that the shear mechanism of bainitic formation in carbon-depleted region is thermodynamically feasible within the whole temperature range of bainitic reaction.
|
|
Received: 18 March 1995
|
| 1冯华,康沫狂,李春信材料科学进展,1988;2:122武小雷,张喜燕,康沫汪.金属热处理学报,1994;15(3):123KangMK,YangYQetalMetallTrans,1994:25:inpress4张喜燕,武小雷,康沫狂等.金属学报,1994,30:A3275KangMK,SunJL.YangQM.MetallTrans,1990;21:8536AgrenJ.MetallTrans,1979;10:7777ShifletGJ,BradleyJR,AaronsonHLMetallTrans,1978;9:9998XieZY,KangMK,WuXL.Actametallmater,1994;42:18259AckertRL,ParrJG,JISI.1971:209:91210杨全民,康沫狂,金属学报,1989:25:25711ChristianJW,EdmondsDV.PhaseTransformationinFerrousAllovs.MarderARandGoldsteinJIeds.AIME.Warrendale,PA.1983:29312武小雷,张喜燕.康沫狂等.自然科学进展——国家重点实验室通讯.1994:4(6):257 |