Please wait a minute...
Acta Metall Sin  1995, Vol. 31 Issue (3): 105-114    DOI:
Current Issue | Archive | Adv Search |
DISLOCATION STRUCTURE OF FATIGUE CRACK TIP
ZHENG Yesha; WANG Zhongguang; AI Suhua (State Key Laboratory of Fatigue and Fracture for Materials; Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110015)
Cite this article: 

ZHENG Yesha; WANG Zhongguang; AI Suhua (State Key Laboratory of Fatigue and Fracture for Materials; Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110015). DISLOCATION STRUCTURE OF FATIGUE CRACK TIP. Acta Metall Sin, 1995, 31(3): 105-114.

Download:  PDF(763KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  It was observed first in this test that the stabilized dislocation cell and wall structures had been formed on near fatigue threshold of physcial short crack in dual-phase steels. There was a probability of forming dislocation cell on ferrite-martensite interfaces in long crack growth threshold. where the dislocation lines were more dense, there were the dislocation lines of single(R = 0,-1) and cross slip(R=-1) in the second stage of long crack growth ;there were obviously rare and lengthened dislocation lines of single and cross slip in the third stage of long crack growth. It is indicated that the dislocation morphologies of fatigue crack tip were the products of strain history. The dislocation cell and wall structures were substable on near physical short crack threshold. it was constituted into dynamic balance with cyclic stress-strain on threshold, and also was one of microstructural parameters.
Key words:  fatigue threshold      crack tip      dislocation structure      dual-phase steel      physical short crack     
Received:  18 March 1995     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1995/V31/I3/105

王栓柱编著.金属疲劳.福建科学与技术出版社.1986年5月2Bao-TongMa.LairdC.ActaMetall,198937(2):325sSureshS著.王中光等译.材料的疲劳.北京:国防工业出版社.19934柴惠芬,汪立勤,LairdC.金属学报,1989;25:A2015WangZG.SunZM.AiSH.MaterSciEng,1989A113:2596ZhengYS.WangZG.AiSH.,MaterSciEngng.1994A176:3937Abdel-RaoufH.PbehamP.PlumtreeA.Can,MetallQ,197110(2):878PolakJ.KlesnilJ.MaterSciEngng,1976;26:1579LawrenceFV,JonesRC.,MetallTrans,1970;1:36710EshelbyJD,FrankFD.NabarroPRN.PhilMag,1951;42:35111HutchinsonJD,MechJ.PhysSolidy,1968.161312RiceJR.ASTMSTP.1966:418:24713SuzukiH.McEvilyAJ.,MetallTrans,1979;10A:47514LucasJR.GerberichWW.FatigueFractEngMaterStruct,19836(3)271
[1] HAN Dong, ZHANG Yanjie, LI Xiaowu. Effect of Short-Range Ordering on the Tension-Tension Fatigue Deformation Behavior and Damage Mechanisms of Cu-Mn Alloys with High Stacking Fault Energies[J]. 金属学报, 2022, 58(9): 1208-1220.
[2] LI Xiucheng,SUN Mingyu,ZHAO Jingxiao,WANG Xuelin,SHANG Chengjia. Quantitative Crystallographic Characterization of Boundaries in Ferrite-Bainite/Martensite Dual-Phase Steels[J]. 金属学报, 2020, 56(4): 653-660.
[3] Weiwei GUO,Chengjun QI,Xiaowu LI. INVESTIGATIONS ON THERMAL STABILITY OF FATIGUE DISLOCATION STRUCTURES IN CONJUGATE AND CRITICAL DOUBLE-SLIP-ORIENTED Cu SINGLE CRYSTALS[J]. 金属学报, 2016, 52(6): 761-768.
[4] YAN Ying, LU Meng, LI Xiaowu. EFFECTS OF PRE-FATIGUE DEFORMATION ON THE  UNIAXIAL TENSILE BEHAVIOR OF COARSEGRAINED PURE Al[J]. 金属学报, 2013, 49(6): 658-666.
[5] BI Zongyue, YANG Jun, NIU Jing, ZHANG Jianxun. FRACTURE TOUGHNESS OF WELDED JOINTS OF X100 HIGH-STRENGTH PIPELINE STEEL[J]. 金属学报, 2013, 49(5): 576-582.
[6] GUO Weiwei, QI Chengjun, LI Xiaowu. INVESTIGATIONS ON THERMAL STABILITY OF FATIGUE DISLOCATION STRUCTURES IN A DOUBLE-SLIPORIENTED Cu SINGLE CRYSTAL[J]. 金属学报, 2013, 49(1): 107-114.
[7] SHENG Hai, DONG Chaofang, XIAO Kui, LI Xiaogang. LOCALIZED ELECTROCHEMICAL CHARACTERIZATION OF HIGH STRENGTH ALUMINIUM ALLOY AT THE CRACK TIP IN 3.5NaCl SOLUTION[J]. 金属学报, 2012, 48(4): 414-419.
[8] NIE Wenjin SHANG Chengjia GUAN Hailong ZHANG Xiaobing CHEN Shaohui. CONTROL OF MICROSTRUCTURES OF FERRITE/ BAINITE (F/B) DUAL-PHASE STEELS AND ANALYSIS OF THEIR RESISTANCE TO DEFORMATION BEHAVIOR[J]. 金属学报, 2012, 48(3): 298-306.
[9] CHEN Chang WANG Mingpu WANG Shan JIA Yanlin ZUO Bo XIA Fuzhong. EVOLUTION OF DISLOCATION MICROSTRUCTURES IN Ta–7.5%W ALLOY FOILS DURING COLD–ROLLING[J]. 金属学报, 2011, 47(8): 984-989.
[10] LI Xiaowu CAO Xinming MA Chaoqun. FATIGUE DEFORMATION FEATURES OF Fe--Cr ALLOY SINGLE CRYSTALS CONTAINING Cr--RICH PRECIPITATES[J]. 金属学报, 2009, 45(7): 801-807.
[11] ZHU Mingliang XUAN Fuzhen ZHU Kuilong WANG Guozhen JIA Tianyao. EFFECT OF HEAT TREATMENT ON FATIGUE BEHAVIOR OF 25Cr2NiMo1V STEEL[J]. 金属学报, 2009, 45(3): 320-325.
[12] XIONG Ying. A TWO-PARAMETER DRIVING FORCE FOR FATIGUE CRACK GROWTH[J]. 金属学报, 2008, 44(11): 1348-1353 .
[13] XIAO Lin(State Key Laboratory for Mechanical Behaviour of Materials; Xi'an Jiaotong University; Xi'an 710049)KUANG Zhenbang(Department of Engineering Mechanics; Shanghai Jiaotong University; Shanghai 200030). MACROSCOPIC RESPONSE AND MICROSCOPIC MECHANISM OF ZIRCALOY-4 UNDER NONPROPORTIONAL LOADING[J]. 金属学报, 1998, 34(3): 242-248.
[14] LI Xiaodong; WANG Yanbin;CHU Wuyang (University of Science and TechnologyBeijing; Beijing 100083); TIAN Fang; WANG Chen; BAI Chunli (Institute Of Chemistry; Chinese Academy of Sciences; Beijing 100080). INVESTIGATION OF LOADED CRACK TIP ON MICA SURFACE BY ATOMIC FORCE MICROSCOPY[J]. 金属学报, 1997, 33(6): 588-594.
[15] Gong Bo;Chen Daolun; Su Huihe; Wang Zhongguang(State Key Laboratory for Fatigue and Fracture of Materials; Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110015). DIRECT OBSERVATION OF DISLOCATION STRUCTURE IN DEFORMED MATERIALS BY SEM──Dislocation Structure in a Fatigued [001] Cu Single Crystal[J]. 金属学报, 1997, 33(6): 561-565.
No Suggested Reading articles found!