Please wait a minute...
Acta Metall Sin  1995, Vol. 31 Issue (14): 77-85    DOI:
Current Issue | Archive | Adv Search |
SIMULATION OF ELASTO-PLASTIC DEFORMATION OF In-Situ Al-Al_2Cu COMPOSITE BY CRYSTALLINE MACRO-MICRO MECHANICAL APPROACH
WANG Mingzhang; LIN Shi; QIAN Rengen; XIAO Jimei(University of Science and Technology Beijing; 100083)(Manuscript received 94-04-18; in revised form 94-10-07)
Cite this article: 

WANG Mingzhang; LIN Shi; QIAN Rengen; XIAO Jimei(University of Science and Technology Beijing; 100083)(Manuscript received 94-04-18; in revised form 94-10-07). SIMULATION OF ELASTO-PLASTIC DEFORMATION OF In-Situ Al-Al_2Cu COMPOSITE BY CRYSTALLINE MACRO-MICRO MECHANICAL APPROACH. Acta Metall Sin, 1995, 31(14): 77-85.

Download:  PDF(748KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  A crystalline macro-micro mechanical approach is developed to analyze the mechanical behaviour of metal matrix composite numerically,on the basis of the data of single crystal deformation. The tensile deformation is simulated in particular using a model system Al-Al2Cu in-situ composite. The calculated stress-strain curves agree well with the experiment result by Davidson et al. The initiation and growth of matrix slip deformation and the inhomogeneous distribution and variation of the stress in the specimen especially near the interface are obtained.The effect of matrix/ reinforcement interface and interlamellar spacing λ on the stress-strain behaviour of metal matrix composite are investigated. It is shown that the crystal macro-micro mechanical approach, which can provide some useful information to insight into the deformation mechanism, is very helpful to analyze and design the mechanical properties of metal matrix composite.Correspondent: WANG Mingzhang,(Department of Material Physics, University of Science and Technology Beijing, Beijing 100083)
Key words:  metal matrix composite      elasto-plastic deformation      crystalline macro-micro mechanics      finite element method      Al-Al_2Cu     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1995/V31/I14/77

1NakamuraT,SureshS.ActaMetallMater,1993:41:16652RobertsonDD,MallS.JComposTechnolRes,1993:15:1813ChristmanT,NeedlemanA,NuttS,SureshS.MaterSciEngng,1989;107A:494BrockenbroughJR,SureshS,WieneckeHA.ActaMetallMater,1991;39:7355GunawardenaSR,JanssonS.LeckieFA.ActaMetallMater,1993;41:31576LevyA,PapazianJM.MetallTrans,1990;21A:4117AsaroRJ.ActaMetall,1979;27:4458PeirceD,AsaroRJ,NeedlemanA.ActaMetall,1983;31:19519HarrenSV,AsaroRJ.JMechPhysSolids,1989;37:191 10McHughPE,AsaroRJ,ShihCF.ActaMetallMater,1993;41:146111卫超,钱仁根,林实,肖纪美.固体力学学报,1989;10:22712卫超,钱仁根,林 实,肖纪美.金属学报,1989;26:A24813WeiC,LinS,QianRG,HsiaoJM.ActaMetallMater,1991;39,205114CantorB,ChadwickGA.JCrystalGrowth,1974:23:1215EshelmanFR,SmithJF.JApplPhys,1978:49:328416CantorB,ChadwickGA.JMaterSci,1975;10:57817HuntingtonHB.SolidStatePhys,1954;7:21418Dew-HugbesD,RobertsonWD.ActaMetall,1960;8:14719CarlsenKM,HoneycombeRWK.JInstMetals,1954─1955;83,449 20GreethamGG,HoneycombeRWK.JInstMetals,1960─1961;89,1321DavidsionCJ,SmithIO,ChadwickGA.ActaMetall,1980:28:6122MetcalfAG,Ed..InterfacesinMetalMatrixComposites,NewYork:AcadmicPress,197423ChadwickGA.ActaMetall,1976:24:1137
[1] MA Guonan, ZHU Shize, WANG Dong, XIAO Bolv, MA Zongyi. Aging Behaviors and Mechanical Properties of SiC/Al-Zn-Mg-Cu Composites[J]. 金属学报, 2023, 59(12): 1655-1664.
[2] FAN Genlian, GUO Zhiqi, TAN Zhanqiu, LI Zhiqiang. Architecture Design Strategies and Strengthening-Toughening Mechanisms of Metal Matrix Composites[J]. 金属学报, 2022, 58(11): 1416-1426.
[3] LI Shaojie, JIN Jianfeng, SONG Yuhao, WANG Mingtao, TANG Shuai, ZONG Yaping, QIN Gaowu. Multimodal Microstructure of Mg-Gd-Y Alloy Through an Integrated Simulation of “Process-Structure-Property”[J]. 金属学报, 2022, 58(1): 114-128.
[4] ZHU Shize, WANG Dong, WANG Quanzhao, XIAO Bolv, MA Zongyi. Influence of Cu Content on the Negative Effect of Natural Aging in SiC/Al-Mg-Si-Cu Composites[J]. 金属学报, 2021, 57(7): 928-936.
[5] Xuexiong LI,Dongsheng XU,Rui YANG. Crystal Plasticity Finite Element Method Investigation of the High Temperature Deformation Consistency in Dual-Phase Titanium Alloy[J]. 金属学报, 2019, 55(7): 928-938.
[6] Huiyuan WANG,Chao LI,Zhigang LI,Jin XU,Hongjiang HAN,Zhiping GUAN,Jiawang SONG,Cheng WANG,Pinkui MA. Current Research and Future Prospect on the Preparation and Architecture Design of Nanomaterials Reinforced Light Metal Matrix Composites[J]. 金属学报, 2019, 55(6): 683-691.
[7] MA Guonan, WANG Dong, LIU Zhenyu, BI Sheng, ZAN Yuning, XIAO Bolv, MA Zongyi. Effect of Hot Pressing Temperature on Microstructure and Tensile Properties of SiC/Al-Zn-Mg-Cu Composites[J]. 金属学报, 2019, 55(10): 1319-1328.
[8] Bolü XIAO, Zhiye HUANG, Kai MA, Xingxing ZHANG, Zongyi MA. Research on Hot Deformation Behaviors of Discontinuously Reinforced Aluminum Composites[J]. 金属学报, 2019, 55(1): 59-72.
[9] Gaohui WU, Jing QIAO, Longtao JIANG. Research Progress on Principle of Dimensional Stability and Stabilization Design of Al and Its Composites[J]. 金属学报, 2019, 55(1): 33-44.
[10] Tongxiang FAN, Yue LIU, Kunming YANG, Jian SONG, Di ZHANG. Recent Progress on Interfacial Structure Optimization and Their Influencing Mechanism of Carbon Reinforced Metal Matrix Composites[J]. 金属学报, 2019, 55(1): 16-32.
[11] Xuexi ZHANG, Zhong ZHENG, Ying GAO, Lin GENG. Progress in High Throughput Fabrication and Characterization of Metal Matrix Composites[J]. 金属学报, 2019, 55(1): 109-125.
[12] Yanqiu WANG,Kun WU,Fuhui WANG. EFFECTS OF SECOND PHASES ON MICROARC OXIDATION PROCESS OF MAGNESIUM BASE MATERIALS[J]. 金属学报, 2016, 52(6): 689-697.
[13] Yongkui LI, Chunyi QUAN, Shanping LU, Qingyang JIAO, Shijian LI, Zhonghai SUN. STUDY ON SHAPE CORRECTION OF THE THIN PLATE OF TA15 TITANIUM ALLOY BY POST WELD HEAT TREATMENT[J]. 金属学报, 2016, 52(3): 281-288.
[14] ZHU Ruidong, DONG Wenchao, LIN Huaqiang, LU Shanping, LI Dianzhong. FINITE ELEMENT SIMULATION OF WELDING RESIDUAL STRESS FOR BUFFER BEAM OF CRH2A HIGH SPEED TRAIN[J]. 金属学报, 2014, 50(8): 944-954.
[15] LI Yongkui, CHEN Jundan, LU Shanping. RESIDUAL STRESS IN THE WHEEL OF 42CrMo STEEL DURING QUENCHING[J]. 金属学报, 2014, 50(1): 121-128.
No Suggested Reading articles found!