Please wait a minute...
Acta Metall Sin  1994, Vol. 30 Issue (7): 321-326    DOI:
Current Issue | Archive | Adv Search |
FORMATION AND ROTATION OF γ' RAFTS IN Ni-BASE SINGLE CRYSTAL SUPERALLOY NASA IR100
GUO Xiping; FU Hengzhi (Northwestern Polytechnical University; Xi'an) ; SUNJiahua (Central Iron and Steel Research institute; Ministry of Metallurgical Industry; Beijing)(Manuscript received 12 July; 1993; in revised form 10 January; 1994)
Cite this article: 

GUO Xiping; FU Hengzhi (Northwestern Polytechnical University; Xi'an) ; SUNJiahua (Central Iron and Steel Research institute; Ministry of Metallurgical Industry; Beijing)(Manuscript received 12 July; 1993; in revised form 10 January; 1994). FORMATION AND ROTATION OF γ' RAFTS IN Ni-BASE SINGLE CRYSTAL SUPERALLOY NASA IR100. Acta Metall Sin, 1994, 30(7): 321-326.

Download:  PDF(476KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The formation of γ' rafts and their rotation in the necking zone during high temperature stress-rupture tests of NASA IR100 single crystal superalloy were investigated.It was found that γ' precipitates linked each other in the direction of perpendicular to the stress axis just after the beginning of the stress-rupture test. Perfect and regularγ' rafts formed when the stress-rupture test lasted for about 50 h. After observing the longitudinal sections of ruptured bars by SEM the γ' rafts in the necking zones were found to be not perpendicular to the stress axis, but rotated around the stress axis. The mechanisms of γ' raft formation and rotation were put forward in this paper.Correspondent: GUO Xiping, lecturer,State Key Laboratory of Solidification Processing, Northwestern Polytechnical University, Xi'an 710072
Key words:  single crystal superalloy      high temperature stress-rupture deformation      γ' raft      NASA IR100     
Received:  18 July 1994     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1994/V30/I7/321

1PearsonDD,LemkeyFD,KearBH.In:TienJKetal.eds.,Superalloys1980,MetalsPark,Ohio:ASM,1980:513-5202KhanT.In:BetzWetal.eds.,HighTemperatureAlloysforGasTurbinesandOtherApplications1986,Holland:D.ReidelPublishingCompany,1986:21-503MackayRA,EbertLJ.MetallTrans,1985;16A:19694MackayRA,NathalMV.NASA-TV-STBX88788,1986:1-375NathalMV,EbertJ.MetallTrans,1985;16A:18496胡赓祥,钱苗根.金属学,上海:上海科学技术出版社,1980:1177CaronP,HendersonPJ,KhanT,McLeanM.ScrMetall,1986;20:8758FredholmA,StrudelJL,In:GellMetal.eds.,Superalloys1984,NewYork,NY:AIME,1984:2119ArdellAJ,NicholsonRB,EshelbyJD.ActaMetall,1986;20:87510胡赓祥,钱苗根.金属学,上海:上海科学技术出版社,1980:26911MonikaFK,ThomasL.MetallTrans,1989;20A:1233J
[1] ZHANG Jian, WANG Li, XIE Guang, WANG Dong, SHEN Jian, LU Yuzhang, HUANG Yaqi, LI Yawei. Recent Progress in Research and Development of Nickel-Based Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1109-1124.
[2] LU Nannan, GUO Yimo, YANG Shulin, LIANG Jingjing, ZHOU Yizhou, SUN Xiaofeng, LI Jinguo. Formation Mechanisms of Hot Cracks in Laser Additive Repairing Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1243-1252.
[3] ZHAO Peng, XIE Guang, DUAN Huichao, ZHANG Jian, DU Kui. Recrystallization During Thermo-Mechanical Fatigue of Two High-Generation Ni-Based Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1221-1229.
[4] LI Jiarong, DONG Jianmin, HAN Mei, LIU Shizhong. Effects of Sand Blasting on Surface Integrity and High Cycle Fatigue Properties of DD6 Single Crystal Superalloy[J]. 金属学报, 2023, 59(9): 1201-1208.
[5] WANG Di, HE Lili, WANG Dong, WANG Li, ZHANG Siqian, DONG Jiasheng, CHEN Lijia, ZHANG Jian. Influence of Pt-Al Coating on Tensile Properties of DD413 Alloy at High Temperatures[J]. 金属学报, 2023, 59(3): 424-434.
[6] ZHANG Zixuan, YU Jinjiang, LIU Jinlai. Anisotropy of Stress Rupture Property of Ni Base Single Crystal Superalloy DD432[J]. 金属学报, 2023, 59(12): 1559-1567.
[7] ZHANG Shaohua, XIE Guang, DONG Jiasheng, LOU Langhong. Investigation on Eutectic Dissolution Behavior of Single Crystal Superalloy by Differential Scanning Calorimetry[J]. 金属学报, 2021, 57(12): 1559-1566.
[8] MA Dexin, ZHAO Yunxing, XU Weitai, PI Libo, LI Zhongxing. Surface Effect on Eutectic Structure Distribution in Single Crystal Superalloy Castings[J]. 金属学报, 2021, 57(12): 1539-1548.
[9] HE Siliang, ZHAO Yunsong, LU Fan, ZHANG Jian, LI Longfei, FENG Qiang. Effects of Hot Isostatic Pressure on Microdefects and Stress Rupture Life of Second-Generation Nickel-Based Single Crystal Superalloy in As-Cast and As-Solid-Solution States[J]. 金属学报, 2020, 56(9): 1195-1205.
[10] LIU Jinlai, YE Lihua, ZHOU Yizhou, LI Jinguo, SUN Xiaofeng. Anisotropy of Elasticity of a Ni Base Single Crystal Superalloy[J]. 金属学报, 2020, 56(6): 855-862.
[11] ZHAO Xu,SUN Yuan,HOU Xingyu,ZHANG Hongyu,ZHOU Yizhou,DING Yutian. Effect of Orientation Deviation on Microstructure and Mechanical Properties of Nickel-Based Single Crystal Superalloy Brazing Joints[J]. 金属学报, 2020, 56(2): 171-181.
[12] ZHANG Jian,WANG Li,WANG Dong,XIE Guang,LU Yuzhang,SHEN Jian,LOU Langhong. Recent Progress in Research and Development of Nickel-Based Single Crystal Superalloys[J]. 金属学报, 2019, 55(9): 1077-1094.
[13] LI Jiarong,XIE Hongji,HAN Mei,LIU Shizhong. High Cycle Fatigue Behavior of Second Generation Single Crystal Superalloy[J]. 金属学报, 2019, 55(9): 1195-1203.
[14] HU Bin,LI Shusuo,PEI Yanling,GONG Shengkai,XU Huibin. Influence of Small Misorientation from <111> on Creep Properties of a Ni-Based Single Crystal Superalloy[J]. 金属学报, 2019, 55(9): 1204-1210.
[15] Jinyao MA,Jin WANG,Yunsong ZHAO,Jian ZHANG,Yuefei ZHANG,Jixue LI,Ze ZHANG. Investigation of In Situ 1150 ℃ High Temperature Deformation Behavior and Fracture Mechanism of a Second Generation Single Crystal Superalloy[J]. 金属学报, 2019, 55(8): 987-996.
No Suggested Reading articles found!