| MECHANISM FOR ANOMALOUSLY FAST DIFFUSION OF SOLUTE ATOMS IN HCP CRYSTALS |
| CHEN Ning;YU Zongsen(University of Science and Technology Beijing)(Manuscript received 8 February;1993;in revised form 1 July;1993) |
|
Cite this article:
CHEN Ning;YU Zongsen(University of Science and Technology Beijing)(Manuscript received 8 February;1993;in revised form 1 July;1993). MECHANISM FOR ANOMALOUSLY FAST DIFFUSION OF SOLUTE ATOMS IN HCP CRYSTALS. Acta Metall Sin, 1994, 30(3): 112-116.
|
|
|
Abstract Based on a mechanism proposed for diffusion of a solute atom-vacancy complex the diffusion coefficients and activation energies of some solute atoms,which diffuse anomalously fast in HCP crystals,are calculated.The mechanism could explain this phenomenon very well.Correspondent:CHEN Ning,Department of Physical Chemistry,University of Science and Technology Beijing,Beijing,100083
|
|
Received: 18 March 1994
|
| 1NakamuraY,NakajimaH,IshiokaS,KoiwaM.ActaMetall,1988;36:27872HoodGM.J Phys,F:MetalPhys,1978;8:16773AnthonyTR,DysonBF,TunrnbullD.J Appl Phys,1968;39:13914ShewmonPG.DiffusioninSOlids,NewYork:McGraw-Hill,1990:113-1225余宗森,陈宁.金属学报1992;28:A1046FaulknerRG.J MaterSci,1981;16:3737HoodGM.PhysRev,1981;B23:42538BrandesEA(ed.).SimthellsMetalsReferenceBook,SixthEdition:LondonButterworths,1983:139余宗森,陈宁.中国科学,1992:A(10):111410AustKT,HannemanRE,NiessenP,WestbrookJH.ActaMetall.1968;16:291 |