A NEW THERMODYNAMIC CALCULATION FORMULA FOR ACTIVITY OF COMPONENT IN BINARY SYSTEM
DING Xueyong;WANG Wenzhong(Northeastern University;Shenyang)
Cite this article: 

DING Xueyong;WANG Wenzhong(Northeastern University;Shenyang). A NEW THERMODYNAMIC CALCULATION FORMULA FOR ACTIVITY OF COMPONENT IN BINARY SYSTEM. Acta Metall Sin, 1994, 30(22): 444-447.

Download:  PDF(247KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  A new formula for calculating the activities of the components in any binary system has been proposed based on Miedema's model for calculating the formation heat of binary alloys.The formula can be used in both solid and liquid solutions. This method has been used to calculate the activities in the binary system taken from 75 elements. The results show that this method is feasible and agrees very well with the experimental data for most systems. The ratio of the same sign of either the positive deviation or the negative deviation to solution reaches 87.5 %.
Key words:  binary system      activity      thermodynamic calculation     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1994/V30/I22/444

1MargulesM.SitzungsberAkadWissWien,1895;104:12432PorterAW.TransFaradaySoc,1921;16:3363HildebrandJ.H.ProcNatAcadSciUSA,192;13:2674GueggenheimEA.Mixtures,Oxhrd:OxhrdUniversityPress,19525LupisCHP,EllliottJF.ActaMelall.1967:15:2656MiedemaAR,DeChatelPF,DeBoerFR.Physica,1980;100B:17PhillipsJC.In:BennettLHed.TheoryofAlloyphaseFormation,MetallSocAIME,1980;3308Kaufman,Calphad,1977;1:3009丁学勇,范鹏,韩其勇.金属学报,1994:30:B4910TanakaT,GokcenNA,MoritaZ.ZMetallkunde,1990:81:4911DinsdaleAT.Calphad,1991:15:31712HultgrenR,DesaiPD,HawkinsDT,GleiserM,KelleyKK.SelectedValuesofTheThermodynamicPropertiesofBinaryAlloys,Ohio;ASM,MetalsPark,1973
[1] MU Yahang, ZHANG Xue, CHEN Ziming, SUN Xiaofeng, LIANG Jingjing, LI Jinguo, ZHOU Yizhou. Modeling of Crack Susceptibility of Ni-Based Superalloy for Additive Manufacturing via Thermodynamic Calculation and Machine Learning[J]. 金属学报, 2023, 59(8): 1075-1086.
[2] JU Tianhua, SHU Nian, HE Wei, DING Xueyong. A Predicted Model for Activity Interaction Coefficient Between Solutes in Alloy Solutions[J]. 金属学报, 2023, 59(11): 1533-1540.
[3] CHEN Wei, CHEN Hongcan, WANG Chenchong, XU Wei, LUO Qun, LI Qian, CHOU Kuochih. Effect of Dilatational Strain Energy of Fe-C-Ni System on Martensitic Transformation[J]. 金属学报, 2022, 58(2): 175-183.
[4] YU Jiaying, WANG Hua, ZHENG Weisen, HE Yanlin, WU Yurui, LI Lin. Effect of the Interface Microstructure of Hot-Dip Galvanizing High-Strength Automobile Steel on Its Tensile Fracture Behaviors[J]. 金属学报, 2020, 56(6): 863-873.
[5] Rongyao MA, Lin ZHAO, Changgang WANG, Xin MU, Xin WEI, Junhua DONG, Wei KE. Influence of Hydrostatic Pressure on the Thermodynamics and Kinetics of Metal Corrosion[J]. 金属学报, 2019, 55(2): 281-290.
[6] Yu HUANG, Guoguang CHENG, You XIE. Modification Mechanism of Cerium on the Inclusions in Drill Steel[J]. 金属学报, 2018, 54(9): 1253-1261.
[7] Xiaofeng LU, Ming XIAO, Yangmei CHEN, Bangcheng YANG. Bioactivity of Titanium Metal Hybridized with Inactivated Bacterial Biofilm[J]. 金属学报, 2017, 53(10): 1402-1412.
[8] Muqin LI, Haitao YAO, Fanghong WEI, Mingda LIU, Zan WANG, Shuhao PENG. The Microstructure and in Vivo and in Vitro Property of Multi-Component Composite Films on the Biomedical Pure Magnesium Surface[J]. 金属学报, 2017, 53(10): 1337-1346.
[9] Xiaoyan CHEN,Zhe JIN,Xuefeng BAI,Yizhou ZHOU,Tao JIN,Xiaofeng SUN. EFFECT OF C ON THE INTERFACIAL REACTION AND WETTABILITY BETWEEN A Ni-BASED SUPERALLOY AND CERAMIC MOULD[J]. 金属学报, 2015, 51(7): 853-858.
[10] Dongsong RONG,Yong JIANG,Jianming GONG. EXPERIMENTAL RESEARCH AND THERMODYNAMIC SIMULATION OF LOW TEMPERATURE COLOSSAL CARBURIZATION OF AUSTENITIC STAINLESS STEEL[J]. 金属学报, 2015, 51(12): 1516-1522.
[11] HAN Guomin, HAN Zhiqiang, Alan A. Luo, Anil K. Sachdev, LIU Baicheng. PHASE FIELD SIMULATION ON MORPHOLOGY OF CONTINUOUS PRECIPITATE Mg17Al12IN Mg-Al ALLOY[J]. 金属学报, 2013, 49(3): 277-283.
[12] LIANG Jingjing, ZHU Ming, YUAN Zhonghua, WANG Junwu, JIN Tao,SUN Xiaofeng, HU Zhuangqi. INFLUENCE OF Re ON THE PHASE CONSTITUENT OF A NiCoCrAlY COATING ALLOY[J]. 金属学报, 2013, 49(3): 330-340.
[13] MA Yue SU Hang PAN Tao YU Yinhong YANG Caifu ZHANG Yongquan PENG Yun. STUDY OF COMPLEX DUCTILE INCLUSIONS CONTROLLING IN MEDIUM-HIGH CARBON STEELS[J]. 金属学报, 2012, 48(11): 1321-1328.
[14] WANG Yi SUN Feng DONG Xianping ZHANG Lanting SHAN Aidang. THERMODYNAMIC STUDY ON EQUILIBRIUM PRECIPITATION PHASES IN A NOVEL Ni-Co BASE SUPERALLOY[J]. 金属学报, 2010, 46(3): 334-339.
[15] Chun-guang Kuai; Zhifang Peng. ELEMENTAL PARTITIONING CHARACTERISTICS AND STABILITY OF EQUILIBRIUM PHASES DURING 450-1200℃ IN T/P91 HEAT-RESISTANT STEEL[J]. 金属学报, 2008, 44(8): 897-900 .
No Suggested Reading articles found!