| MODEL AND EXPERIMENTS ON FATIGUE SHORT CRACK GROWTH IN RESIDUAL STRESS FIELD |
| CUI Zhenqi;XU Kewei; HU Naisai(National Laboratory for Mechanical Behaviour of Metallic Materials;xi'an Jiaotong University) |
|
Cite this article:
CUI Zhenqi;XU Kewei; HU Naisai(National Laboratory for Mechanical Behaviour of Metallic Materials;xi'an Jiaotong University). MODEL AND EXPERIMENTS ON FATIGUE SHORT CRACK GROWTH IN RESIDUAL STRESS FIELD. Acta Metall Sin, 1994, 30(2): 65-69.
|
|
|
Abstract Discussion with experiments was carried out on the model for the effect of residual stress upon crack growth. A rather accurate calculation of crack growth rate in a compressive residual stress field may be made by the equation:The compressive residual stress not only increases the crack closure force but also decreases the maximum stress intensity factor.Both reduce the ΔK_(eff) value and the crack growth driving force, thus the crack growth rate is decreased.HU Naisai, professor,(National Laboratory for Mechanical Behaviour of Metallic Materials,Xi'an Jiaotong University, Xi'an, 710049)
|
|
Received: 18 February 1994
|
| 1ParkerAP.ASTMSTP776,1982:132林立,胡奈赛,何家文.材料科学进展,1990;5:3873NewmanJCJr.ASTMSTP748,1981:534NewmanJCJr.AGARDConfProc,NO.328,19825林立,胡奈赛,陶冶.金属科学与工艺,1991;10(1):1 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|