| MICROANALYSES OF PHASES IN Sm-Fe-N ALLOY |
| GUO Yanfeng;XU Leying(Institute of Metal Research; Chinese Academy of Sciences;Shenyang)LIU Zhaoyun;QI Hui (Jilin University; Changchun) |
|
Cite this article:
GUO Yanfeng;XU Leying(Institute of Metal Research; Chinese Academy of Sciences;Shenyang)LIU Zhaoyun;QI Hui (Jilin University; Changchun). MICROANALYSES OF PHASES IN Sm-Fe-N ALLOY. Acta Metall Sin, 1994, 30(19): 330-336.
|
|
|
Abstract The composition and structure of the different phases in the Sm-Fe-N alloy as well as the phase transformation during ion-nitrizing have been studied. The magnetic phase Sm_2Fe_(17)N_x transformed into the amorphous during ion-nitrizing, moreover, partially resolved into SmFe_3N_x and α-Fe.
|
|
|
| 1CoeyJMD,SunHong,OtaniY,In:SankarSGed.,Proc6thIntSymponMagneticAnisotropyandCoercivityinRareEarth-TransitionMetalAlloys,Pittsburgh,PA:CarnegieMellonUniversity,1990:362KatterM,WeckerJ,SchultzL.JApplPhys,1991;70:63YangYingchang,YangJilian.In:Zhangshougonged.,Proc2ndIntConfonRareEarthDevelopmentandApplication,Vol.II,Beijing:InternationalAcademic,1991:5674YangXingbo,MiyazakiT,TakakuraK,HisatakeK,HattoriT,TakahashiM.JMagnMagnMater,1986;62:29 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|