|
|
|
| CRYSTALLIZATION PRODUCTS OF AMORPHOUS Fe_(80)B_(20) ALLOY |
| DONG Zhenfu; LU Ke; WEI Wenduo; DING Bingzhe (Stale Key Laboratory of Rapidly Solidified and Non-Equilibrium Alloys; Institute of Metal Research; Chinese Academy of Sciences; Shenyang) |
|
Cite this article:
DONG Zhenfu; LU Ke; WEI Wenduo; DING Bingzhe (Stale Key Laboratory of Rapidly Solidified and Non-Equilibrium Alloys; Institute of Metal Research; Chinese Academy of Sciences; Shenyang). CRYSTALLIZATION PRODUCTS OF AMORPHOUS Fe_(80)B_(20) ALLOY. Acta Metall Sin, 1994, 30(19): 304-308.
|
|
|
Abstract By use of XRD and TEM, structure of the crystalliztion products of amorphous Fe_(80)B_(20)alloy with different regimes of heat treatment was studied. The crystallization products are composed of α-Fe(B) solution and Fe-B compound. The relative quantity of the α- Fe solid solution phase increases with the annealing temperature. The compound phases, Fe_3B and Fe_(3.5)B, change in relative quantity also with heat treatment. The lattice distortion of the crystallization products was detected.
|
|
|
| 1GreerAL.ActaMetall,1982;30:1712RayR,HasegawaR.SolidStateCommun,1978;27:4713RayR,HasegawaR,JApplPhys,1978:49:41744LuK,SuiML.JMaterSciTechnol,1993;9:4195董振奋.中国科学院金属研究所硕士学位论文,1993 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|