| PHASE DIAGRAM OF KF-LiCl-CaCl_2 SYSTEM |
| YAN Licheng;FANG Jianhui;XU Jingyan;YANG Jinxiu(Shanghai University of Science and Technology) |
|
Cite this article:
YAN Licheng;FANG Jianhui;XU Jingyan;YANG Jinxiu(Shanghai University of Science and Technology). PHASE DIAGRAM OF KF-LiCl-CaCl_2 SYSTEM. Acta Metall Sin, 1994, 30(19): 301-303.
|
|
|
Abstract Phase diagram of KF-LiCl-CaCl_2 system has been determined by methods of visual variable-temperature, DTA and XRD. A negative deviation for KF occurs in molten salt LiCl-CaCl_2 solution. The semi-quantitative relationship between the relative area of primary crystallization region for fluoride of divalent alkaline metal and the energetic parameter of solution was also discussed together with KF-LiCl-BaCl_2 and KF-LiCl-SrCl_2 systems made previously by the authors.
|
|
|
| 1GrubeG,RucelW.JPhyschemRefData,1975;4:95921942;35:213阎立诚,徐京燕,杨金秀,金属学报,1992;28:B4904陈念贻,张桂成.金属学报,1964;7:1115阎立诚,朱鹦鹦,陈念贻.高等学校化学学报,1984;5:7556阎立城,杨金秀,朱鹦鹦.金属学报,1987:23:B2047阎立诚,杨金秀,郁磊.上海科技大学学报,1988;11(2):18阎立诚,杨金秀,朱鹦鹦.高等学校化学学报,1988;9:7269范谨霞,阎立诚,杨金秀.上海科技大学学报,1990;13(1):8710范谨霞,杨金秀,阎立诚.上海科技大学学报,1990;13(4):8111阎立诚,杨金秀,朱蕾,徐京燕,范瑾霞.金属学报,1990;26:B136 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|