| HREM STUDY OF TEXTURE OF γ/γ'-αDS EUTECTIC ALLOY DURING AGING |
| DAI Jiyan;ZHANG Jinghua;JIN Zhixiong;LI Douxing;YE Hengqiang;(Laboratory of Atomic Image of Solids;Institue of Metal Research;Chinese Acadmy of Sciences;Shenyang)(Manuscript received 5 October;1993) |
|
Cite this article:
DAI Jiyan;ZHANG Jinghua;JIN Zhixiong;LI Douxing;YE Hengqiang;(Laboratory of Atomic Image of Solids;Institue of Metal Research;Chinese Acadmy of Sciences;Shenyang)(Manuscript received 5 October;1993). HREM STUDY OF TEXTURE OF γ/γ'-αDS EUTECTIC ALLOY DURING AGING. Acta Metall Sin, 1994, 30(1): 1-6.
|
|
|
Abstract The texture of γ/γ'-αDS eutectic alloy during aging has been investigated by means of high resolution electron microscopy(HREM) and analytical transmission electron microscopy.It has been found that the products of phase transformation in γphase are different during aging at temperatures of 850 and 650℃.Stick-like orthorhombic Ni3Mo was precipitated inα fibers,the γ-N i3Al with lamella twin structure can also be found to coexist with Ni3Mo.EDAX analysis shows the solid solution of Ni,Al and small amount of V inαfibers.Correspondent:DAI Jiyan,(Institute of Metal Research,Chinese Acadamy of Sciences,Shenyang 110015)
|
|
Received: 18 January 1994
|
| 1PearsonDD,KearBH,LemkyFD.In:WilshireBetaleds.IntConfonCreepandFractureofEngineeringMaterialsandStructures,PineRidge,1981:2132TartagliaJM,StoloffNS.MetallTrans,1981;12A:11193KaufmanMJ,EadesJA,LorettoMH,FraserHL.MetallTrans,1983;14A:15614SnowDB,BreinanEM,KearBH.In:TienJKetaleds.,SuperalloysProc.ofthe4ihInt.Symp. onSuperalloys,ASM,MetalPark,Ohio,1980:1895张静华,张玉生,张志亚,徐永波,唐亚俊,胡壮麒.金属学报,1983;19:A 3096DaiJY,L1DX,YeHQ,JinZX,ZhangJH.J MaterSci,tobepublished7VanTendelooG,DeRidderR,AmelinckxS.PhysStatSol1975;27A:4578MartinPL,WilliamsJC.ActaMetall,1984;32:16819SriramamurtyAM,BanerjeeD,TewariSN.AclaMelall,1982;30:123110PearsonDD,LemkeyFD.Proc.Int.Conf.Solidification,1979,MetalsSociety,UK,1979:526 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |