FRACTAL ANALYSES OF MCIN A DIRECTIONALLY SOLIDIFIED NICKEL-BASE SUPERALLOY
SUN Liling;DONG Lianke;ZHANG Jinghua;HU Zhuangqi Institute of Metal Research; Academia Sinica; Shenyang
Cite this article: 

SUN Liling;DONG Lianke;ZHANG Jinghua;HU Zhuangqi Institute of Metal Research; Academia Sinica; Shenyang. FRACTAL ANALYSES OF MCIN A DIRECTIONALLY SOLIDIFIED NICKEL-BASE SUPERALLOY. Acta Metall Sin, 1993, 29(9): 6-10.

Download:  PDF(1240KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The growth morphologies of MC type carbide in a directional solidificationwas described quantitatively by means of the fractal analysis. The relationship between the in-formation dimensionality of MC evolved from the lenient branch-leaves into developedbranch-cluster with the increase of the solidiflcation rate, and the information dimensionalityof MC presented the exponential law with the change of solidification rate. In combinationwith the thermodynamic of nonequilibrium, the physical mechanism of MC morphology evo-lution was discussed when the controlled parameter-solidification rate changed.
Key words:  fractal dimension      MC type carbide      directional solidification      superalloy     
Received:  18 September 1993     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1993/V29/I9/6

1 Fehandez R, Lecomte J C, Kattamis J Z. Metall Trans, 1978; 9A: 1318
2 Shi Gongqi, Ding Peidao. Mater Sci Technol, 1992; 8: 449
3 Matsushita M. J Iron Steel Inst Jpn, 1990; 76: 1613
4 Hornbogen E. Int Mater Rev, 1989; 34: 277
5 董连科.分形理论及其应用.沈阳:辽宁科学技术出版社,1991:124
6 李如生.非平衡态热力学和耗散结构.北京:清华大学出版社,1986:143
7 Flemings M C. Solidification Processing. New York: McGraw--Hill, 1974: 112
8 董连科.分形理论及其应用.沈阳:辽宁科学技术出版社,1991:28
[1] LI Jiarong, DONG Jianmin, HAN Mei, LIU Shizhong. Effects of Sand Blasting on Surface Integrity and High Cycle Fatigue Properties of DD6 Single Crystal Superalloy[J]. 金属学报, 2023, 59(9): 1201-1208.
[2] MA Dexin, ZHAO Yunxing, XU Weitai, WANG Fu. Effect of Gravity on Directionally Solidified Structure of Superalloys[J]. 金属学报, 2023, 59(9): 1279-1290.
[3] CHEN Jia, GUO Min, YANG Min, LIU Lin, ZHANG Jun. Effects of W Concentration on Creep Microstructure and Property of Novel Co-Based Superalloys[J]. 金属学报, 2023, 59(9): 1209-1220.
[4] ZHAO Peng, XIE Guang, DUAN Huichao, ZHANG Jian, DU Kui. Recrystallization During Thermo-Mechanical Fatigue of Two High-Generation Ni-Based Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1221-1229.
[5] BAI Jiaming, LIU Jiantao, JIA Jian, ZHANG Yiwen. Creep Properties and Solute Atomic Segregation of High-W and High-Ta Type Powder Metallurgy Superalloy[J]. 金属学报, 2023, 59(9): 1230-1242.
[6] ZHENG Liang, ZHANG Qiang, LI Zhou, ZHANG Guoqing. Effects of Oxygen Increasing/Decreasing Processes on Surface Characteristics of Superalloy Powders and Properties of Their Bulk Alloy Counterparts: Powders Storage and Degassing[J]. 金属学报, 2023, 59(9): 1265-1278.
[7] BI Zhongnan, QIN Hailong, LIU Pei, SHI Songyi, XIE Jinli, ZHANG Ji. Research Progress Regarding Quantitative Characterization and Control Technology of Residual Stress in Superalloy Forgings[J]. 金属学报, 2023, 59(9): 1144-1158.
[8] WANG Lei, LIU Mengya, LIU Yang, SONG Xiu, MENG Fanqiang. Research Progress on Surface Impact Strengthening Mechanisms and Application of Nickel-Based Superalloys[J]. 金属学报, 2023, 59(9): 1173-1189.
[9] GONG Shengkai, LIU Yuan, GENG Lilun, RU Yi, ZHAO Wenyue, PEI Yanling, LI Shusuo. Advances in the Regulation and Interfacial Behavior of Coatings/Superalloys[J]. 金属学报, 2023, 59(9): 1097-1108.
[10] LU Nannan, GUO Yimo, YANG Shulin, LIANG Jingjing, ZHOU Yizhou, SUN Xiaofeng, LI Jinguo. Formation Mechanisms of Hot Cracks in Laser Additive Repairing Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1243-1252.
[11] JIANG He, NAI Qiliang, XU Chao, ZHAO Xiao, YAO Zhihao, DONG Jianxin. Sensitive Temperature and Reason of Rapid Fatigue Crack Propagation in Nickel-Based Superalloy[J]. 金属学报, 2023, 59(9): 1190-1200.
[12] FENG Qiang, LU Song, LI Wendao, ZHANG Xiaorui, LI Longfei, ZOU Min, ZHUANG Xiaoli. Recent Progress in Alloy Design and Creep Mechanism of γ'-Strengthened Co-Based Superalloys[J]. 金属学报, 2023, 59(9): 1125-1143.
[13] ZHANG Jian, WANG Li, XIE Guang, WANG Dong, SHEN Jian, LU Yuzhang, HUANG Yaqi, LI Yawei. Recent Progress in Research and Development of Nickel-Based Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1109-1124.
[14] LIU Xingjun, WEI Zhenbang, LU Yong, HAN Jiajia, SHI Rongpei, WANG Cuiping. Progress on the Diffusion Kinetics of Novel Co-based and Nb-Si-based Superalloys[J]. 金属学报, 2023, 59(8): 969-985.
[15] MU Yahang, ZHANG Xue, CHEN Ziming, SUN Xiaofeng, LIANG Jingjing, LI Jinguo, ZHOU Yizhou. Modeling of Crack Susceptibility of Ni-Based Superalloy for Additive Manufacturing via Thermodynamic Calculation and Machine Learning[J]. 金属学报, 2023, 59(8): 1075-1086.
No Suggested Reading articles found!