| INFLUENCE OF TI ON STRUCTURE AND PROPERTLES OF HIGH Al-Zn ALLOYS |
| LIU Jinshui;SHU Zhen;LI Chuanping Hunan University; Changsha |
|
Cite this article:
LIU Jinshui;SHU Zhen;LI Chuanping Hunan University; Changsha. INFLUENCE OF TI ON STRUCTURE AND PROPERTLES OF HIGH Al-Zn ALLOYS. Acta Metall Sin, 1993, 29(11): 9-13.
|
|
|
Abstract The plasticity and toughness of as-cast high Al-Zn alloy may be obviouslyimproved by Ti modification. In the modified alloy, the heterogeneous nuclei, causing the re-finement of α'-phase, were observed to be ternary compound of single cubic Al_5Ti_2Zn withlattice parameter a=0.3959±0.0003 nm, not flaky or brocky Al_3Ti as generally expected.
|
|
Received: 18 November 1993
|
1 Hadbiby F, Mcnallan M J. Trans Am Foundrymen's Soc, 1984; 92: 263 2 舒震,刘金水.湖南大学学报,1988;2:42 3 骆灼旋,陈华信.铸造,1992;4:28 4 Shu Zhen, Liu Jinshui. Proceedings of Shenyang International Symposium on Casting. 1988; 445 5 Apellian D, Paliwal M. J Met, 1981; 11: 12 6 Pearson W B. A Handbook of Lattice Spacing and Structures of Metals and Alloys. Oxford: Pergamon, 1958: 363e |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|